Fabrication of Bioactive Apatite Nuclei Precipitated Titanium by Using Electromagnetic Induction Heating

Takeshi Yabutsuka, M. Hibino, T. Yao, Kojiro Tanaka, M. Takemoto, M. Neo, Takashi Nakamura
{"title":"Fabrication of Bioactive Apatite Nuclei Precipitated Titanium by Using Electromagnetic Induction Heating","authors":"Takeshi Yabutsuka, M. Hibino, T. Yao, Kojiro Tanaka, M. Takemoto, M. Neo, Takashi Nakamura","doi":"10.4303/BDA/D110122","DOIUrl":null,"url":null,"abstract":"Many micro pores were formed on the surface of a titanium (Ti) plate by sulfuric acid treatment, then apatite nuclei were precipitated in the pores of the Ti plate by direct heating of the plate by using electromagnetic induction in a simulated body fluid (SBF). When the Ti plate was soaked in SBF, amorphous calcium phosphate thin film covered the whole surface within 6 h and it grew into hydroxyapatite within 12 h. The hydroxyapatite layer showed high adhesive strength to the Ti plate due to a mechanical interlocking effect between hydroxyapatite grown in the micro pores and the Ti plate.","PeriodicalId":127691,"journal":{"name":"Bioceramics Development and Applications","volume":"27 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2010-12-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"10","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Bioceramics Development and Applications","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4303/BDA/D110122","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 10

Abstract

Many micro pores were formed on the surface of a titanium (Ti) plate by sulfuric acid treatment, then apatite nuclei were precipitated in the pores of the Ti plate by direct heating of the plate by using electromagnetic induction in a simulated body fluid (SBF). When the Ti plate was soaked in SBF, amorphous calcium phosphate thin film covered the whole surface within 6 h and it grew into hydroxyapatite within 12 h. The hydroxyapatite layer showed high adhesive strength to the Ti plate due to a mechanical interlocking effect between hydroxyapatite grown in the micro pores and the Ti plate.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
电磁感应加热制备生物活性磷灰石核沉淀钛
硫酸处理后的钛(Ti)板表面形成许多微孔,然后在模拟体液(SBF)中利用电磁感应直接加热钛(Ti)板,在钛(Ti)板的孔中沉淀磷灰石核。将钛板浸泡在SBF中,6 h内无定形磷酸钙薄膜覆盖整个表面,12 h内生长为羟基磷灰石。微孔中生长的羟基磷灰石与钛板之间存在机械互锁作用,羟基磷灰石层与钛板具有较高的粘附强度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Modal Analysis of FGM Plates (Sus304/Al2O3) Using FEM Intentional Replantation with 180° Rotation of a Crown-Root Fracture as a Last Expedient: A Case Report Mechanism of Bonding in Seashell Powder Based Ceramic Composites Used for Binder-Jet 3D Printing Effect of βTricalcium Phosphate Nanoparticles Additions on the Properties of Gelatin-Chitosan Scaffolds Hydroxyapatite Scaffolds for Bone Tissue Engineering
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1