{"title":"Thermoelectric properties and phase stability of La/sub 10/S/sub 14/O","authors":"M. Ohta, S. Hirai, H. Kato, H. Asahi","doi":"10.1109/ICT.2005.1519917","DOIUrl":null,"url":null,"abstract":"The electrical resistivity, thermopower, thermal conductivity measurements have been made on tetragonal La/sub 10/S/sub 14/O. The electrical resistivity was measured during heating and successive cooling through 300 and 1000 K to investigate the high-temperature phase stability. The measurements were carried out in the vacuum chamber pumped down to 1.0 Pa. The electrical properties of La/sub 10/S/sub 14/O are changed dramatically through heat treatment. As annealing time increases, the electrical resistivity increases abruptly and then decreases gradually. However, it seems that this phase can be stabilized by a small addition of Ti. In the electrical resistivity of La/sub 10/S/sub 14/O with Ti, the cooling curve agrees with heating curve. Moreover, the ZT value increases abruptly with increasing temperature, reaching a value of 0.18 at 1000 K. The improvement with respect to the thermoelectric properties of the La/sub 10/S/sub 14/O is realized by a small addition of Ti.","PeriodicalId":422400,"journal":{"name":"ICT 2005. 24th International Conference on Thermoelectrics, 2005.","volume":"6 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2005-06-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"ICT 2005. 24th International Conference on Thermoelectrics, 2005.","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ICT.2005.1519917","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The electrical resistivity, thermopower, thermal conductivity measurements have been made on tetragonal La/sub 10/S/sub 14/O. The electrical resistivity was measured during heating and successive cooling through 300 and 1000 K to investigate the high-temperature phase stability. The measurements were carried out in the vacuum chamber pumped down to 1.0 Pa. The electrical properties of La/sub 10/S/sub 14/O are changed dramatically through heat treatment. As annealing time increases, the electrical resistivity increases abruptly and then decreases gradually. However, it seems that this phase can be stabilized by a small addition of Ti. In the electrical resistivity of La/sub 10/S/sub 14/O with Ti, the cooling curve agrees with heating curve. Moreover, the ZT value increases abruptly with increasing temperature, reaching a value of 0.18 at 1000 K. The improvement with respect to the thermoelectric properties of the La/sub 10/S/sub 14/O is realized by a small addition of Ti.