{"title":"Consolidation of Rapidly Solidifying Al-6Si-0.3Cu Alloy by Spark Plasma Sintering and Cold Compaction Methods","authors":"F. Yasar, F. Yılmaz","doi":"10.36287/ijmsit.6.2.198","DOIUrl":null,"url":null,"abstract":"– In this study, Al-6Si-0.3Cu ribbon alloys produced by melt-spinning method were consolidated by two different methods, which are spark plasma sintering and cryogenic ball milling + cold compaction. From X-ray diffraction analysis, it was found that the solubility of Si in Al matrix in melt-spun alloys increased, but Si precipitated in SPS and ball milled+cold compacted alloys. Optical and scanning electron microscope observation revealed that while melt spun alloys have a very fine and homogenous microstructure, Si phase has become coarser in SPS and cold compacted alloys due to the sintering. The results showed that the spark plasma sintering method is a very effective method for compaction of melt-spun Al-6Si-0.3Cu alloy.","PeriodicalId":166049,"journal":{"name":"International Journal of Multidisciplinary Studies and Innovative Technologies","volume":"88 5 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Multidisciplinary Studies and Innovative Technologies","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36287/ijmsit.6.2.198","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
– In this study, Al-6Si-0.3Cu ribbon alloys produced by melt-spinning method were consolidated by two different methods, which are spark plasma sintering and cryogenic ball milling + cold compaction. From X-ray diffraction analysis, it was found that the solubility of Si in Al matrix in melt-spun alloys increased, but Si precipitated in SPS and ball milled+cold compacted alloys. Optical and scanning electron microscope observation revealed that while melt spun alloys have a very fine and homogenous microstructure, Si phase has become coarser in SPS and cold compacted alloys due to the sintering. The results showed that the spark plasma sintering method is a very effective method for compaction of melt-spun Al-6Si-0.3Cu alloy.