Tsuyoshi Takahashi, Son Thanh Nguyen, Masaaki Kimura
{"title":"Microstructure and Mechanical Characteristics of Friction Welded Joint between Alumina and Aluminum Casting Alloy","authors":"Tsuyoshi Takahashi, Son Thanh Nguyen, Masaaki Kimura","doi":"10.4028/p-9esrhc","DOIUrl":null,"url":null,"abstract":"In this study, the Al2O3 round bar and Al-Si12CuNi (AC8A) round bar were joined by friction welding. AC8A is a typical piston material treated by the heat treatment T6. The parameters of the joining condition are friction time and upset pressure. SEM observed the microstructure at the interface region of joined materials. 1) Judging from these photographs, the damages to the microstructures at the interface region of joined materials by upset pressure are more significant than those caused by friction time. 2) The relationship between the joint conditions and mechanical characteristics from three points of bending test results for the joint material specimens. 3) The residual stresses around the interface were measured by the Raman spectroscopy method. There is a possibility that the friction welding conditions are correlated to the residual stresses.","PeriodicalId":18262,"journal":{"name":"Materials Science Forum","volume":"38 21","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-05-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science Forum","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4028/p-9esrhc","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
In this study, the Al2O3 round bar and Al-Si12CuNi (AC8A) round bar were joined by friction welding. AC8A is a typical piston material treated by the heat treatment T6. The parameters of the joining condition are friction time and upset pressure. SEM observed the microstructure at the interface region of joined materials. 1) Judging from these photographs, the damages to the microstructures at the interface region of joined materials by upset pressure are more significant than those caused by friction time. 2) The relationship between the joint conditions and mechanical characteristics from three points of bending test results for the joint material specimens. 3) The residual stresses around the interface were measured by the Raman spectroscopy method. There is a possibility that the friction welding conditions are correlated to the residual stresses.