Phosphate/Silicate Ratio Allows for Fine-Tuning of Bioactive Glass Crystallisation and Glass-Ceramic Microstructure

A. C. Contreras Jaimes, Gloria Kirste, Christian Patzig, J. Martins de Souza e Silva, J. Massera, N. Karpukhina, Robert G. Hill, A. de Pablos-Martín, D. Brauer
{"title":"Phosphate/Silicate Ratio Allows for Fine-Tuning of Bioactive Glass Crystallisation and Glass-Ceramic Microstructure","authors":"A. C. Contreras Jaimes, Gloria Kirste, Christian Patzig, J. Martins de Souza e Silva, J. Massera, N. Karpukhina, Robert G. Hill, A. de Pablos-Martín, D. Brauer","doi":"10.52825/glass-europe.v2i.1187","DOIUrl":null,"url":null,"abstract":"A combination of XRD, solid-state NMR and state-of-the-art imaging techniques were used to investigate how the calcium orthophosphate/calcium silicate ratio affects the crystallisation of bioactive glasses in the system SiO2-P2O5-CaO-CaF2. In the phosphate-free glass, xonotlite, wollastonite and cuspidine crystallised. From 2.4 mol% P2O5, fluorapatite also formed, while the amount of wollastonite decreased. Crystallisation tendency was low for low phosphate contents, while above 3 mol% P2O5 it increased. The phosphate-free glass showed a volume crystallisation mechanism with constant activation energy. By contrast, the glass with the largest phosphate to silicate ratio showed both volume and surface crystallisation, causing a pronounced decrease in activation energy with crystallisation degree. This work shows that by changing the phosphate/silicate ratio we can determine which crystal phases form, obtaining for example fluorapatite-free or wollastonite-free glass-ceramics, depending on the desired application and properties such as mechanical strength or activity in contact with physiological solutions.","PeriodicalId":130330,"journal":{"name":"Glass Europe","volume":"13 7","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-06-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Glass Europe","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.52825/glass-europe.v2i.1187","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

A combination of XRD, solid-state NMR and state-of-the-art imaging techniques were used to investigate how the calcium orthophosphate/calcium silicate ratio affects the crystallisation of bioactive glasses in the system SiO2-P2O5-CaO-CaF2. In the phosphate-free glass, xonotlite, wollastonite and cuspidine crystallised. From 2.4 mol% P2O5, fluorapatite also formed, while the amount of wollastonite decreased. Crystallisation tendency was low for low phosphate contents, while above 3 mol% P2O5 it increased. The phosphate-free glass showed a volume crystallisation mechanism with constant activation energy. By contrast, the glass with the largest phosphate to silicate ratio showed both volume and surface crystallisation, causing a pronounced decrease in activation energy with crystallisation degree. This work shows that by changing the phosphate/silicate ratio we can determine which crystal phases form, obtaining for example fluorapatite-free or wollastonite-free glass-ceramics, depending on the desired application and properties such as mechanical strength or activity in contact with physiological solutions.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
磷酸盐/硅酸盐比例可微调生物活性玻璃结晶和玻璃陶瓷微观结构
我们结合使用了 XRD、固态 NMR 和最先进的成像技术来研究正磷酸钙/硅酸钙的比例如何影响 SiO2-P2O5-CaO-CaF2 体系中生物活性玻璃的结晶。在无磷酸盐的玻璃中,氙石、硅灰石和乌斯皮定都结晶了。从 2.4 mol% P2O5 开始,氟磷灰石也开始形成,而硅灰石的数量则有所减少。磷酸盐含量较低时,结晶趋势较低,而 P2O5 含量超过 3 摩尔时,结晶趋势增加。无磷酸盐玻璃显示出一种活化能恒定的体积结晶机制。相比之下,磷酸盐与硅酸盐比值最大的玻璃同时表现出体积和表面结晶,导致活化能随着结晶程度的增加而明显下降。这项研究表明,通过改变磷酸盐/硅酸盐的比例,我们可以决定形成哪种晶相,从而获得无磷灰石或无硅灰石玻璃陶瓷,具体取决于所需的应用和特性,如机械强度或与生理溶液接触时的活性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Open Electrode Thermal Poling Setup for Treating Lithium-Aluminosilicate Glass-Ceramics Using Gas Discharge Phosphate/Silicate Ratio Allows for Fine-Tuning of Bioactive Glass Crystallisation and Glass-Ceramic Microstructure Assessment of the Thermal Shock Resistance of Neodymium Doped Alumino-Phosphate Laser Glasses Viscous Sintering of Acid Leached Glass Powders Surface Hardness and Abrasion Threshold of Chemically Strengthened Soda-Lime Silicate Glasses After Steam Processing
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1