[复合材料的不透明度和不透明度变化]。

Deutsche zahnarztliche Zeitschrift Pub Date : 1991-09-01
T Luckenbach, G M Lösche, J F Roulet
{"title":"[复合材料的不透明度和不透明度变化]。","authors":"T Luckenbach,&nbsp;G M Lösche,&nbsp;J F Roulet","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The opacity of 5 self-curing and 11 light-curing composite resins was measured 24 hours after sample/preparation and after 6 months of storage (dry or in water) by means of an UV-visible spectrophotometer. The opacity of the investigated hybrid composite resins was between 47.3 and 62.4%. The opacity of the microfilled composite resins ranged from 48 to 64.4%. The opacity was not influenced by the polymerization time. The spectral opacity decreased with greater wavelengths, particularly in microfilled composite resins. All materials except Durafill, which became more translucent, were more opaque after 180 days of storage in water. Storage in water for 180 days caused greater changes of the opacity than dry storage for the same time. The opacity changes resulting from storage in water can be reduced by increasing the polymerization time.</p>","PeriodicalId":11244,"journal":{"name":"Deutsche zahnarztliche Zeitschrift","volume":"46 9","pages":"621-5"},"PeriodicalIF":0.0000,"publicationDate":"1991-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"[Opacity and opacity changes in composites].\",\"authors\":\"T Luckenbach,&nbsp;G M Lösche,&nbsp;J F Roulet\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>The opacity of 5 self-curing and 11 light-curing composite resins was measured 24 hours after sample/preparation and after 6 months of storage (dry or in water) by means of an UV-visible spectrophotometer. The opacity of the investigated hybrid composite resins was between 47.3 and 62.4%. The opacity of the microfilled composite resins ranged from 48 to 64.4%. The opacity was not influenced by the polymerization time. The spectral opacity decreased with greater wavelengths, particularly in microfilled composite resins. All materials except Durafill, which became more translucent, were more opaque after 180 days of storage in water. Storage in water for 180 days caused greater changes of the opacity than dry storage for the same time. The opacity changes resulting from storage in water can be reduced by increasing the polymerization time.</p>\",\"PeriodicalId\":11244,\"journal\":{\"name\":\"Deutsche zahnarztliche Zeitschrift\",\"volume\":\"46 9\",\"pages\":\"621-5\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1991-09-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Deutsche zahnarztliche Zeitschrift\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Deutsche zahnarztliche Zeitschrift","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

用紫外可见分光光度计测量5种自固化和11种光固化复合树脂在样品制备后24小时和储存(干燥或水中)6个月后的不透明度。混合复合树脂的不透明度在47.3 ~ 62.4%之间。微填充复合树脂的不透明度为48% ~ 64.4%。不透明度不受聚合时间的影响。光谱不透明度随着波长的增加而降低,特别是在微填充复合树脂中。除了Durafill变得更加半透明外,所有材料在水中储存180天后都变得更加不透明。在水中储存180天,其不透明度的变化比在相同时间内干燥储存更大。通过增加聚合时间,可以减少因在水中储存而引起的不透明度变化。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
[Opacity and opacity changes in composites].

The opacity of 5 self-curing and 11 light-curing composite resins was measured 24 hours after sample/preparation and after 6 months of storage (dry or in water) by means of an UV-visible spectrophotometer. The opacity of the investigated hybrid composite resins was between 47.3 and 62.4%. The opacity of the microfilled composite resins ranged from 48 to 64.4%. The opacity was not influenced by the polymerization time. The spectral opacity decreased with greater wavelengths, particularly in microfilled composite resins. All materials except Durafill, which became more translucent, were more opaque after 180 days of storage in water. Storage in water for 180 days caused greater changes of the opacity than dry storage for the same time. The opacity changes resulting from storage in water can be reduced by increasing the polymerization time.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
[Dental alloys and allergy. Case report]. [Medical high-risk patient in the dental practice]. [Long-term results with dental treatment concepts for disabled children]. [Nasal intubation for frontobasal fractures?]. [Fiberoptic intubation as a safe method for the treatment of odontogenic abscesses].
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1