{"title":"【粘接修复瓷面预处理】。","authors":"M Imai","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The effects of pre-treatment of porcelain surfaces, such as etching and treatment with a silane coupling agent, for obtaining firm adhesion between the adhesive resin, Panavia EX, and the porcelain were examined. The effects of heating treatment (100, 150 and 200 degrees C) in applying the silane coupling agents to porcelain surfaces were examined. Infrared spectra and energy dispersive X-ray spectra were obtained for the porcelain surface, on which a silane coupling agent was applied. A stable shearing adhesive strength, such as 450-520 kgf/cm2, was obtained even after a 24-hour immersion in 37 degrees C water, when with the etching the porcelain surface was pretreated with a 30% HF solution (60 sec) or heating treatment (150 degrees C, 10 min) when applying the silane coupling agent (2% gamma-MPTS). Then the adhesive durability was examined by a thermal cycling test (4-60 degrees C, 60 sec). After the thermal cycling test (20,000 times), the adhesive strength to the porcelain surface polished by #600 sand-paper was strong and only when the 2% gamma-MPTS was used did detachment occur. However, the adhesive strength was maintained at about 70-80% of the early strength with the etching treatment by the pre-treatment with 30% HF for 60 sec and the heating treatment (150 degrees C, 10 min) when applying the 2% gamma-MPTS.</p>","PeriodicalId":77622,"journal":{"name":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"1990-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"[Pre-treatment of porcelain surface for adhesive restorations].\",\"authors\":\"M Imai\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>The effects of pre-treatment of porcelain surfaces, such as etching and treatment with a silane coupling agent, for obtaining firm adhesion between the adhesive resin, Panavia EX, and the porcelain were examined. The effects of heating treatment (100, 150 and 200 degrees C) in applying the silane coupling agents to porcelain surfaces were examined. Infrared spectra and energy dispersive X-ray spectra were obtained for the porcelain surface, on which a silane coupling agent was applied. A stable shearing adhesive strength, such as 450-520 kgf/cm2, was obtained even after a 24-hour immersion in 37 degrees C water, when with the etching the porcelain surface was pretreated with a 30% HF solution (60 sec) or heating treatment (150 degrees C, 10 min) when applying the silane coupling agent (2% gamma-MPTS). Then the adhesive durability was examined by a thermal cycling test (4-60 degrees C, 60 sec). After the thermal cycling test (20,000 times), the adhesive strength to the porcelain surface polished by #600 sand-paper was strong and only when the 2% gamma-MPTS was used did detachment occur. However, the adhesive strength was maintained at about 70-80% of the early strength with the etching treatment by the pre-treatment with 30% HF for 60 sec and the heating treatment (150 degrees C, 10 min) when applying the 2% gamma-MPTS.</p>\",\"PeriodicalId\":77622,\"journal\":{\"name\":\"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1990-03-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

考察了陶瓷表面的预处理,如蚀刻和硅烷偶联剂处理,对获得粘接树脂Panavia EX与瓷器之间牢固粘接的影响。考察了热处理(100、150、200℃)对硅烷偶联剂在陶瓷表面的应用效果。用硅烷偶联剂对陶瓷表面进行了红外光谱和能量色散x射线光谱分析。即使在37℃的水中浸泡24小时,在蚀刻时用30% HF溶液预处理(60秒)或用硅烷偶联剂(2% γ - mpts)加热(150℃,10分钟),瓷表面也能获得稳定的剪切粘接强度,如450-520 kgf/cm2。然后通过热循环试验(4-60℃,60秒)检测胶粘剂的耐久性。经过2万次热循环试验,600号砂纸抛光后的陶瓷表面粘接强度较强,只有使用2% γ - mpts时才会发生脱落。然而,采用30% HF预处理60秒和2% γ - mpts加热(150℃,10 min)进行蚀刻处理后,粘接强度保持在早期强度的70-80%左右。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
[Pre-treatment of porcelain surface for adhesive restorations].

The effects of pre-treatment of porcelain surfaces, such as etching and treatment with a silane coupling agent, for obtaining firm adhesion between the adhesive resin, Panavia EX, and the porcelain were examined. The effects of heating treatment (100, 150 and 200 degrees C) in applying the silane coupling agents to porcelain surfaces were examined. Infrared spectra and energy dispersive X-ray spectra were obtained for the porcelain surface, on which a silane coupling agent was applied. A stable shearing adhesive strength, such as 450-520 kgf/cm2, was obtained even after a 24-hour immersion in 37 degrees C water, when with the etching the porcelain surface was pretreated with a 30% HF solution (60 sec) or heating treatment (150 degrees C, 10 min) when applying the silane coupling agent (2% gamma-MPTS). Then the adhesive durability was examined by a thermal cycling test (4-60 degrees C, 60 sec). After the thermal cycling test (20,000 times), the adhesive strength to the porcelain surface polished by #600 sand-paper was strong and only when the 2% gamma-MPTS was used did detachment occur. However, the adhesive strength was maintained at about 70-80% of the early strength with the etching treatment by the pre-treatment with 30% HF for 60 sec and the heating treatment (150 degrees C, 10 min) when applying the 2% gamma-MPTS.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
α-TCP/Te-CPセメントの覆髄剤への応用 Tarnish Resistance of Experimental Ti–Ag Alloys in 0.1% Na2S Solution Influence of surface finish methods on color and gloss of dental porcelains Chitosan/BSA micropatterns on Titanium Surfaces by Functionization and Soft Lithography ビニルエステル/ポリマー系軟性樹脂組成物 (第10報) - VE/PEMA系混和物の理論的硬化時間に及ぼすVEの分子構造の影響 -
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1