燃烧法制备透明MgAl2O4尖晶石陶瓷

IF 1.1 Q3 METALLURGY & METALLURGICAL ENGINEERING Acta Metallurgica Slovaca Pub Date : 2019-09-25 DOI:10.12776/ams.v25i3.1313
Y. Nguyen, Tu Anh Dao, H. M. Le, K. Dang, M. Nanko
{"title":"燃烧法制备透明MgAl2O4尖晶石陶瓷","authors":"Y. Nguyen, Tu Anh Dao, H. M. Le, K. Dang, M. Nanko","doi":"10.12776/ams.v25i3.1313","DOIUrl":null,"url":null,"abstract":"Transparent MgAl2O4 ceramic could be found in a wide range of applications for both military and civil sector due to its high melting point, good mechanical properties, small refractive index (1.71) and its ability to allow light in range from UV to mid-IR to pass through. In the present work, transparent MgAl2O4 were fabricated from metal nitrates via two steps. Firstly, the MgAl2O4 nanopowder was synthesized via solution combustion synthesis from the metal nitrates. Secondly, the powder was then consolidated by Pulsed Electric Current Sintering (PECS) technique to fabricate transparent ceramic. XRD patterns of the obtained powder showed the peaks of only MgAl2O4 phase. Besides, the atomic compositions of magnesium, aluminium and oxygen determined by EDX analysis were approximately corresponded to 1:2:4 of the molecular formula of MgAl2O4. After deagglomerating for 48 hours using soft ball-milling, the powder had the average particle of 27 nm. Transparent MgAl2O4 samples, which were sintered with two-step sintering mode of 1050oC/60 minutes-1400oC/20 minutes, permitted the transmission of visible and infrared light with the transmittance up to 80%, Vickers hardness of 14.2 GPa, and fracture toughness of 1.1 MPa.m1/2. The results are a critical step toward fabrication of high-quality transparent ceramics from metal nitrates.","PeriodicalId":44511,"journal":{"name":"Acta Metallurgica Slovaca","volume":null,"pages":null},"PeriodicalIF":1.1000,"publicationDate":"2019-09-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"FABRICATION OF TRANSPARENT MgAl2O4 SPINEL CERAMICS BY PECS PROCESSING OF COMBUSTION - SYTHESIZED NANOPOWDERS\",\"authors\":\"Y. Nguyen, Tu Anh Dao, H. M. Le, K. Dang, M. Nanko\",\"doi\":\"10.12776/ams.v25i3.1313\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Transparent MgAl2O4 ceramic could be found in a wide range of applications for both military and civil sector due to its high melting point, good mechanical properties, small refractive index (1.71) and its ability to allow light in range from UV to mid-IR to pass through. In the present work, transparent MgAl2O4 were fabricated from metal nitrates via two steps. Firstly, the MgAl2O4 nanopowder was synthesized via solution combustion synthesis from the metal nitrates. Secondly, the powder was then consolidated by Pulsed Electric Current Sintering (PECS) technique to fabricate transparent ceramic. XRD patterns of the obtained powder showed the peaks of only MgAl2O4 phase. Besides, the atomic compositions of magnesium, aluminium and oxygen determined by EDX analysis were approximately corresponded to 1:2:4 of the molecular formula of MgAl2O4. After deagglomerating for 48 hours using soft ball-milling, the powder had the average particle of 27 nm. Transparent MgAl2O4 samples, which were sintered with two-step sintering mode of 1050oC/60 minutes-1400oC/20 minutes, permitted the transmission of visible and infrared light with the transmittance up to 80%, Vickers hardness of 14.2 GPa, and fracture toughness of 1.1 MPa.m1/2. The results are a critical step toward fabrication of high-quality transparent ceramics from metal nitrates.\",\"PeriodicalId\":44511,\"journal\":{\"name\":\"Acta Metallurgica Slovaca\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":1.1000,\"publicationDate\":\"2019-09-25\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Acta Metallurgica Slovaca\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.12776/ams.v25i3.1313\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Acta Metallurgica Slovaca","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.12776/ams.v25i3.1313","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 2

摘要

透明MgAl2O4陶瓷由于其高熔点、良好的机械性能、小折射率(1.71)以及允许从UV到中IR范围内的光通过的能力,可在军事和民用部门的广泛应用中找到。在本工作中,由金属硝酸盐通过两个步骤制备了透明的MgAl2O4。首先,以金属硝酸盐为原料,通过溶液燃烧合成了MgAl2O4纳米粉体。其次,采用脉冲电流烧结(PECS)技术对粉末进行固结,制备出透明陶瓷。所得粉末的XRD图谱显示只有MgAl2O4相的峰。此外,通过EDX分析测定的镁、铝和氧的原子组成大致对应于MgAl2O4分子式的1:2:4。在使用软球磨去除凝聚48小时后,粉末具有27nm的平均颗粒。透明的MgAl2O4样品采用1050℃/60分钟-1400℃/20分钟的两步烧结模式烧结,允许可见光和红外光的透射,透射率高达80%,维氏硬度为14.2GPa,断裂韧性为1.1MPa.m1/2。这一结果是由金属硝酸盐制备高质量透明陶瓷的关键一步。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
FABRICATION OF TRANSPARENT MgAl2O4 SPINEL CERAMICS BY PECS PROCESSING OF COMBUSTION - SYTHESIZED NANOPOWDERS
Transparent MgAl2O4 ceramic could be found in a wide range of applications for both military and civil sector due to its high melting point, good mechanical properties, small refractive index (1.71) and its ability to allow light in range from UV to mid-IR to pass through. In the present work, transparent MgAl2O4 were fabricated from metal nitrates via two steps. Firstly, the MgAl2O4 nanopowder was synthesized via solution combustion synthesis from the metal nitrates. Secondly, the powder was then consolidated by Pulsed Electric Current Sintering (PECS) technique to fabricate transparent ceramic. XRD patterns of the obtained powder showed the peaks of only MgAl2O4 phase. Besides, the atomic compositions of magnesium, aluminium and oxygen determined by EDX analysis were approximately corresponded to 1:2:4 of the molecular formula of MgAl2O4. After deagglomerating for 48 hours using soft ball-milling, the powder had the average particle of 27 nm. Transparent MgAl2O4 samples, which were sintered with two-step sintering mode of 1050oC/60 minutes-1400oC/20 minutes, permitted the transmission of visible and infrared light with the transmittance up to 80%, Vickers hardness of 14.2 GPa, and fracture toughness of 1.1 MPa.m1/2. The results are a critical step toward fabrication of high-quality transparent ceramics from metal nitrates.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Acta Metallurgica Slovaca
Acta Metallurgica Slovaca METALLURGY & METALLURGICAL ENGINEERING-
CiteScore
2.00
自引率
30.00%
发文量
22
审稿时长
12 weeks
期刊最新文献
PHYSICO-MECHANICAL PROPERTIES OF POLYMER MATRIX COMPOSITE MATERIAL REINFORCED WITH CARBONIZED CASSAVA BACK PEEL AND IRON FILLINGS EFFECT OF MIXING METHODS PRIOR THE DECOMPOSITION PROCESS ON THE DECOMPOSED FERRONICKEL SLAG WEAR AND ADHESION PROPERTIES OF MULTILAYER Ti/TiN ,(TiC)/TiCN/TaN THIN FILMS DEPOSITED ON Ti13Nb13Zr ALLOY BY CLOSE FIELD UNBALANCED MAGNETRON SPUTTERING Explicit and Implicit Integration of Constitutive Equations of Chaboche Isotropic-Kinematic Hardening Material Model INFLUENCE OF SINTERING TEMPERATURE ON THE STRUCTURAL OF Mg2Si0.3Sn0.7 ALLOY PREPARED BY POWDER METALLURGY
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1