{"title":"从焚烧固体废物中合成铝硅酸盐提取纯SiO2","authors":"Dinh-Hieu Vu, X. Bui, Hoang-Bac Bui, T. T. D. Ngo","doi":"10.29227/im-2019-02-74","DOIUrl":null,"url":null,"abstract":"In this study, Pure SiO2 solution extraction from inceneratedsolid wastes following after aluminosilicate synthesis. The optimumconditions for obtaining both the pure SiO2 solution and the substantialamounts of unique residue material should be 200○C of reactiontemperature, 1:30 of sample:NaOH, 2M NaOH, and enough reaction timeover 24 hours. The optimization of the pure SiO2 extraction proposes aneffective way for recycling the abundant incinerated solid waste as well asother waste ashes.","PeriodicalId":44414,"journal":{"name":"Inzynieria Mineralna-Journal of the Polish Mineral Engineering Society","volume":null,"pages":null},"PeriodicalIF":0.4000,"publicationDate":"2022-01-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Pure SiO2 extraction through aluminosilicates synthesis from incinerated solid wastes\",\"authors\":\"Dinh-Hieu Vu, X. Bui, Hoang-Bac Bui, T. T. D. Ngo\",\"doi\":\"10.29227/im-2019-02-74\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In this study, Pure SiO2 solution extraction from inceneratedsolid wastes following after aluminosilicate synthesis. The optimumconditions for obtaining both the pure SiO2 solution and the substantialamounts of unique residue material should be 200○C of reactiontemperature, 1:30 of sample:NaOH, 2M NaOH, and enough reaction timeover 24 hours. The optimization of the pure SiO2 extraction proposes aneffective way for recycling the abundant incinerated solid waste as well asother waste ashes.\",\"PeriodicalId\":44414,\"journal\":{\"name\":\"Inzynieria Mineralna-Journal of the Polish Mineral Engineering Society\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.4000,\"publicationDate\":\"2022-01-13\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Inzynieria Mineralna-Journal of the Polish Mineral Engineering Society\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.29227/im-2019-02-74\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"MINING & MINERAL PROCESSING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Inzynieria Mineralna-Journal of the Polish Mineral Engineering Society","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.29227/im-2019-02-74","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MINING & MINERAL PROCESSING","Score":null,"Total":0}
Pure SiO2 extraction through aluminosilicates synthesis from incinerated solid wastes
In this study, Pure SiO2 solution extraction from inceneratedsolid wastes following after aluminosilicate synthesis. The optimumconditions for obtaining both the pure SiO2 solution and the substantialamounts of unique residue material should be 200○C of reactiontemperature, 1:30 of sample:NaOH, 2M NaOH, and enough reaction timeover 24 hours. The optimization of the pure SiO2 extraction proposes aneffective way for recycling the abundant incinerated solid waste as well asother waste ashes.