K. Forkel, C. Köcher, E. Schierhorn, K. Adam, F. G. Wihsmann, P. Bartos
{"title":"金属-类金属玻璃合金(Fe,Cr)80(P,C,Si)20、FeCl3水溶液和空气在“非晶固/液/气”相界面区域的腐蚀过程的形貌和微观分析研究","authors":"K. Forkel, C. Köcher, E. Schierhorn, K. Adam, F. G. Wihsmann, P. Bartos","doi":"10.1007/S002160050389","DOIUrl":null,"url":null,"abstract":"","PeriodicalId":12375,"journal":{"name":"Fresenius' Journal of Analytical Chemistry","volume":"28 1","pages":"219-224"},"PeriodicalIF":0.0000,"publicationDate":"1997-05-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Topographical and microanalytical investigation of corrosion processes on the solid material in the system metal-metalloid glassy alloy (Fe,Cr)80(P,C,Si)20, aqueous FeCl3 solution, and air in the region of the “amorphous solid/liquid/air” phase interface\",\"authors\":\"K. Forkel, C. Köcher, E. Schierhorn, K. Adam, F. G. Wihsmann, P. Bartos\",\"doi\":\"10.1007/S002160050389\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\",\"PeriodicalId\":12375,\"journal\":{\"name\":\"Fresenius' Journal of Analytical Chemistry\",\"volume\":\"28 1\",\"pages\":\"219-224\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1997-05-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Fresenius' Journal of Analytical Chemistry\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1007/S002160050389\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Fresenius' Journal of Analytical Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1007/S002160050389","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Topographical and microanalytical investigation of corrosion processes on the solid material in the system metal-metalloid glassy alloy (Fe,Cr)80(P,C,Si)20, aqueous FeCl3 solution, and air in the region of the “amorphous solid/liquid/air” phase interface