{"title":"319.2汽车铝合金的热处理。第2部分:老化行为","authors":"J. Gauthier, P. Louchez, F. Samuel","doi":"10.1080/09534962.1995.11819198","DOIUrl":null,"url":null,"abstract":"In this part of a two-part study of the heat treatment of 319.2 aluminium alloy, the hardening behaviour upon artificial ageing in the temperature range 155‐220 °C for periods of up to 24 h has bee...","PeriodicalId":9691,"journal":{"name":"Cast Metals","volume":"20 5-6 1","pages":"107-114"},"PeriodicalIF":0.0000,"publicationDate":"1995-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"23","resultStr":"{\"title\":\"Heat treatment of 319.2 aluminium automotive alloy Part 2, Ageing behaviour\",\"authors\":\"J. Gauthier, P. Louchez, F. Samuel\",\"doi\":\"10.1080/09534962.1995.11819198\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In this part of a two-part study of the heat treatment of 319.2 aluminium alloy, the hardening behaviour upon artificial ageing in the temperature range 155‐220 °C for periods of up to 24 h has bee...\",\"PeriodicalId\":9691,\"journal\":{\"name\":\"Cast Metals\",\"volume\":\"20 5-6 1\",\"pages\":\"107-114\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1995-07-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"23\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Cast Metals\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1080/09534962.1995.11819198\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cast Metals","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/09534962.1995.11819198","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Heat treatment of 319.2 aluminium automotive alloy Part 2, Ageing behaviour
In this part of a two-part study of the heat treatment of 319.2 aluminium alloy, the hardening behaviour upon artificial ageing in the temperature range 155‐220 °C for periods of up to 24 h has bee...