{"title":"库克尔赛特页岩半焦化气催化合成噻吩的研究","authors":"D.Yu. Zhogin , A.M. Myasoyedov , G.Ye. Voropanov , M.A. Ryashentseva","doi":"10.1016/0031-6458(90)90044-G","DOIUrl":null,"url":null,"abstract":"<div><p>Liquid catalyzate containing thiophene has been obtained from the gas formed in semicoking of kukersite shale by means of heterocyclization over an alumina-chromium-lanthanum lanthanum oxide catalyst. The thiophene concentration in the catalyzate is 1.5–2 times higher than in industrial byproduct coking thiophene concentrate. At the same a reduction in the hydrogen sulphide content of the semicoking gas from 9–12% to 0·5 vol.% or less has been obtained.</p></div>","PeriodicalId":19738,"journal":{"name":"Petroleum Chemistry U.s.s.r.","volume":"30 4","pages":"Pages 262-266"},"PeriodicalIF":0.0000,"publicationDate":"1990-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1016/0031-6458(90)90044-G","citationCount":"0","resultStr":"{\"title\":\"Catalytic synthesis of thiophene from the gas formed in the semicoking of kukersite shale\",\"authors\":\"D.Yu. Zhogin , A.M. Myasoyedov , G.Ye. Voropanov , M.A. Ryashentseva\",\"doi\":\"10.1016/0031-6458(90)90044-G\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>Liquid catalyzate containing thiophene has been obtained from the gas formed in semicoking of kukersite shale by means of heterocyclization over an alumina-chromium-lanthanum lanthanum oxide catalyst. The thiophene concentration in the catalyzate is 1.5–2 times higher than in industrial byproduct coking thiophene concentrate. At the same a reduction in the hydrogen sulphide content of the semicoking gas from 9–12% to 0·5 vol.% or less has been obtained.</p></div>\",\"PeriodicalId\":19738,\"journal\":{\"name\":\"Petroleum Chemistry U.s.s.r.\",\"volume\":\"30 4\",\"pages\":\"Pages 262-266\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1990-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://sci-hub-pdf.com/10.1016/0031-6458(90)90044-G\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Petroleum Chemistry U.s.s.r.\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/003164589090044G\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Petroleum Chemistry U.s.s.r.","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/003164589090044G","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Catalytic synthesis of thiophene from the gas formed in the semicoking of kukersite shale
Liquid catalyzate containing thiophene has been obtained from the gas formed in semicoking of kukersite shale by means of heterocyclization over an alumina-chromium-lanthanum lanthanum oxide catalyst. The thiophene concentration in the catalyzate is 1.5–2 times higher than in industrial byproduct coking thiophene concentrate. At the same a reduction in the hydrogen sulphide content of the semicoking gas from 9–12% to 0·5 vol.% or less has been obtained.