{"title":"中间包堰组织对中频钢洁净度及汽车钢板深拉深缺陷消除的影响","authors":"Xiaoxuan Deng, Guoliang Liu, Qiangqiang Wang, Baisong Liu, C. Ji, Haibo Li, Xiao-jing Shao, Guo-sen Zhu","doi":"10.1051/metal/2020061","DOIUrl":null,"url":null,"abstract":"The flow control devices (FCDs) in the tundish play an important role in steel cleanliness and removal of macro-inclusions. To eliminate the spot-like defects during deep-drawing process, the liquid steel samples were taken from tundish in three industrial IF steel heats, and the effect of weir structure in the tundish on the steel cleanliness were evaluated and compared with the aid of ASPEX with the total detection area of over 54 000 mm2 . The results showed that non-metallic inclusions over 5 µm observed in the liquid tundish samples were categorized into two types: type 1: alumina based inclusions and type 2: calcium aluminates. Compared to the tundish without weir, the number density of macro-inclusions reduces by half when furnished with weir. In addition, several large sized calcium aluminates were occasionally found without weir whereas no calcium aluminates were detected with the weir. The mechanism of the inclusion distributions with the weir was proposed based on the experimental results, which shows that the weir act as a baffle that block the large sized inclusions from moving toward the mould. After using the weir in the actual casting practice, the occurrence ratio of spot-like defects was decreased by about 25%.","PeriodicalId":21337,"journal":{"name":"Revue De Metallurgie-cahiers D Informations Techniques","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":"{\"title\":\"Effect of the weir structure in the tundish on the cleanliness of IF steels and elimination of spot-like defects in deep drawing automobile steel sheets\",\"authors\":\"Xiaoxuan Deng, Guoliang Liu, Qiangqiang Wang, Baisong Liu, C. Ji, Haibo Li, Xiao-jing Shao, Guo-sen Zhu\",\"doi\":\"10.1051/metal/2020061\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The flow control devices (FCDs) in the tundish play an important role in steel cleanliness and removal of macro-inclusions. To eliminate the spot-like defects during deep-drawing process, the liquid steel samples were taken from tundish in three industrial IF steel heats, and the effect of weir structure in the tundish on the steel cleanliness were evaluated and compared with the aid of ASPEX with the total detection area of over 54 000 mm2 . The results showed that non-metallic inclusions over 5 µm observed in the liquid tundish samples were categorized into two types: type 1: alumina based inclusions and type 2: calcium aluminates. Compared to the tundish without weir, the number density of macro-inclusions reduces by half when furnished with weir. In addition, several large sized calcium aluminates were occasionally found without weir whereas no calcium aluminates were detected with the weir. The mechanism of the inclusion distributions with the weir was proposed based on the experimental results, which shows that the weir act as a baffle that block the large sized inclusions from moving toward the mould. After using the weir in the actual casting practice, the occurrence ratio of spot-like defects was decreased by about 25%.\",\"PeriodicalId\":21337,\"journal\":{\"name\":\"Revue De Metallurgie-cahiers D Informations Techniques\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"3\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Revue De Metallurgie-cahiers D Informations Techniques\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1051/metal/2020061\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revue De Metallurgie-cahiers D Informations Techniques","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1051/metal/2020061","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

摘要

中间包内的流动控制装置(FCDs)对钢的清洁度和宏观夹杂物的去除起着重要的作用。为了消除拉深过程中出现的点状缺陷,在三次中碳钢工业加热中提取了中间包的钢液样品,并借助于ASPEX对中间包的围护结构对钢材清洁度的影响进行了评价和比较,总检测面积超过54000 mm2。结果表明,中间包液样品中大于5µm的非金属夹杂物可分为两类:一类为氧化铝基夹杂物,二类为铝酸钙夹杂物。与未加堰的中间包相比,有堰的中间包中宏观夹杂物的数量密度降低了一半。此外,偶尔发现一些大尺寸的铝酸钙没有堰,而没有堰检测到铝酸钙。根据实验结果,提出了夹杂物随堰的分布机理,表明堰起到了阻挡大尺寸夹杂物向模具移动的挡板作用。在实际铸造中使用后,点状缺陷的发生率降低了25%左右。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Effect of the weir structure in the tundish on the cleanliness of IF steels and elimination of spot-like defects in deep drawing automobile steel sheets
The flow control devices (FCDs) in the tundish play an important role in steel cleanliness and removal of macro-inclusions. To eliminate the spot-like defects during deep-drawing process, the liquid steel samples were taken from tundish in three industrial IF steel heats, and the effect of weir structure in the tundish on the steel cleanliness were evaluated and compared with the aid of ASPEX with the total detection area of over 54 000 mm2 . The results showed that non-metallic inclusions over 5 µm observed in the liquid tundish samples were categorized into two types: type 1: alumina based inclusions and type 2: calcium aluminates. Compared to the tundish without weir, the number density of macro-inclusions reduces by half when furnished with weir. In addition, several large sized calcium aluminates were occasionally found without weir whereas no calcium aluminates were detected with the weir. The mechanism of the inclusion distributions with the weir was proposed based on the experimental results, which shows that the weir act as a baffle that block the large sized inclusions from moving toward the mould. After using the weir in the actual casting practice, the occurrence ratio of spot-like defects was decreased by about 25%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
审稿时长
24 months
期刊最新文献
Preparation and performance analysis of gas-quenched steel slag beads Abnormal toughness characteristics and fracture model in simulated welding HAZ of 5%Ni Steel Measurement of the steady state tearing in thin sheets using the contactless system Evaluation of carbothermic processing for mixed discarded lithium-ion batteries Influence of Nb2O5 and basicity on the viscosity and structure of CaO-SiO2-Nb2O5-CeO2-CaF2 slag system
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1