Fracture resistance of pressed ZLS crowns versus pressed LD crowns under thermo-mechanical cycling.

Q2 Medicine Brazilian dental journal Pub Date : 2022-11-01 DOI:10.1590/0103-6440202204993
Basma Osama Salem, Dina Magdy Elshehawi, Gihan Abdelhady Elnaggar
{"title":"Fracture resistance of pressed ZLS crowns versus pressed LD crowns under thermo-mechanical cycling.","authors":"Basma Osama Salem,&nbsp;Dina Magdy Elshehawi,&nbsp;Gihan Abdelhady Elnaggar","doi":"10.1590/0103-6440202204993","DOIUrl":null,"url":null,"abstract":"<p><p>The aim of this study was conducted to assess the fracture resistance of zirconia reinforced lithium silicate all ceramic material \"Celtra Press\" compared to lithium disilicate one \"IPS e-max Press\" under simulated oral conditions. Fourteen ceramic crowns were fabricated on epoxy dies which were duplicated from stainless steel master die and divided into two equal groups (n=7) according to the material of construction; Group A: Crowns fabricated with IPS e-max Press material and Group B: Crowns fabricated with Celtra Press material. The crowns were then cemented onto their corresponding dies with a self-adhesive resin cement and subjected to thermocycling and cyclic loading. Then they were loaded to fractur in a universal testing machine. The results were tabulated and statistically analyzed using Kolmogorov-Smirnov and Shapiro-Wilk tests. Student t-test used to compare mean values. The significance level was set at P ≤ 0.05 and 95% Confidence interval. Statistical analysis was performed using Graph Pad Instat (Graph Pad, Inc.) software for windows. The mean ± SD values of fracture resistance were recorded for lithium Disilicate group (1706.01 ±154.32 N) meanwhile the mean ± SD value recorded with celtra group were (1550.67±196.71 N). Zirconia reinforced lithium silicate ceramic crowns produced comparable fracture resistance values to lithium disilicate ceramic crowns and both tested materials are within the clinically acceptable values in the posterior area.</p>","PeriodicalId":9211,"journal":{"name":"Brazilian dental journal","volume":"33 6","pages":"103-109"},"PeriodicalIF":0.0000,"publicationDate":"2022-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9733374/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Brazilian dental journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1590/0103-6440202204993","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Medicine","Score":null,"Total":0}
引用次数: 0

Abstract

The aim of this study was conducted to assess the fracture resistance of zirconia reinforced lithium silicate all ceramic material "Celtra Press" compared to lithium disilicate one "IPS e-max Press" under simulated oral conditions. Fourteen ceramic crowns were fabricated on epoxy dies which were duplicated from stainless steel master die and divided into two equal groups (n=7) according to the material of construction; Group A: Crowns fabricated with IPS e-max Press material and Group B: Crowns fabricated with Celtra Press material. The crowns were then cemented onto their corresponding dies with a self-adhesive resin cement and subjected to thermocycling and cyclic loading. Then they were loaded to fractur in a universal testing machine. The results were tabulated and statistically analyzed using Kolmogorov-Smirnov and Shapiro-Wilk tests. Student t-test used to compare mean values. The significance level was set at P ≤ 0.05 and 95% Confidence interval. Statistical analysis was performed using Graph Pad Instat (Graph Pad, Inc.) software for windows. The mean ± SD values of fracture resistance were recorded for lithium Disilicate group (1706.01 ±154.32 N) meanwhile the mean ± SD value recorded with celtra group were (1550.67±196.71 N). Zirconia reinforced lithium silicate ceramic crowns produced comparable fracture resistance values to lithium disilicate ceramic crowns and both tested materials are within the clinically acceptable values in the posterior area.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
加压ZLS冠与加压LD冠在热机械循环下的抗断裂性能。
本研究旨在评估氧化锆增强硅酸锂全陶瓷材料“Celtra Press”与二硅酸锂“IPS e-max Press”在模拟口腔条件下的抗断裂性能。在不锈钢母模复制的环氧树脂模具上制作14个陶瓷冠,按材质分为两组(n=7);A组:用IPS e-max压片材料制作的冠;B组:用Celtra压片材料制作的冠。然后用自粘树脂水泥将冠粘接到相应的模具上,并进行热循环和循环加载。然后将它们装入万能试验机中进行断裂。使用Kolmogorov-Smirnov和Shapiro-Wilk检验将结果制成表格并进行统计分析。学生t检验用于比较平均值。显著性水平为P≤0.05,置信区间为95%。使用Graph Pad Instat (Graph Pad, Inc.) windows软件进行统计分析。二硅酸锂组和celtra组的抗裂性平均值±SD值分别为(1706.01±154.32 N)和(1550.67±196.71 N)。氧化锆增强硅酸锂陶瓷冠与二硅酸锂陶瓷冠的抗裂性值相当,且均在临床可接受的后区范围内。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Brazilian dental journal
Brazilian dental journal Dentistry-Dentistry (all)
CiteScore
2.20
自引率
0.00%
发文量
69
审稿时长
12 weeks
期刊介绍: Brazilian Dental Journal, publishes Full-Length Papers, Short Communications and Case Reports, dealing with dentistry or related disciplines and edited six times a year.
期刊最新文献
Can a dentin bonding agent prevent color change in regenerative endodontic procedures? An in vitro evaluation Antibacterial ability of different activated irrigation after root canal preparation: intratubular analyses Inhibition of incipient caries lesion progression by different fluoridated varnishes A new hydroxyapatite-alginate-gelatin biocomposite favor bone regeneration in a critical-sized calvarial defect model Prevalence of lectures about dental esthetics and female speakers in three Brazilian conferences.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1