E. Armah, F. Ampong, M. Egblewogbe, Hubert Azoda Koffi, F. Boakye, J. Amuzu, R. K. Nkum
{"title":"Solubility of Mn in ZnO Nanocrystallites using Wet Chemical Synthesis","authors":"E. Armah, F. Ampong, M. Egblewogbe, Hubert Azoda Koffi, F. Boakye, J. Amuzu, R. K. Nkum","doi":"10.21467/anr.2.1.53-61","DOIUrl":null,"url":null,"abstract":"There is a substantial amount of literature dealing with many aspects of synthesis and characterization of pure and doped binary compounds including Mn-doped ZnO which has been widely studied due to its superb properties as a dilute magnetic semiconductor (DMS). Aspects concerning doping limits for these compounds is an important stage in the search for new materials. Samples of Zn1-xMnxO nanocrystal were synthesized at temperatures of 180 °C and 200 °C using wet or liquid phase synthesis method. Dopant concentrations x=0.5, 1, 1.5, 2, 2.5, 5, 10, 20, 30, 40 and 50 per cent were studied. Powder x-ray diffraction (PXRD) patterns of the samples were analyzed with a view to determining the onset of secondary phases and hence the solubility limit of the dopant. The solubility limit for Mn in ZnO samples synthesized at temperature of 200 °C is realized at x <20%. For samples synthesized at temperature of 180 °C, the solubility limit is x <0.5%.","PeriodicalId":185865,"journal":{"name":"Advanced Nano Research","volume":"15 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2019-11-05","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advanced Nano Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21467/anr.2.1.53-61","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2
Abstract
There is a substantial amount of literature dealing with many aspects of synthesis and characterization of pure and doped binary compounds including Mn-doped ZnO which has been widely studied due to its superb properties as a dilute magnetic semiconductor (DMS). Aspects concerning doping limits for these compounds is an important stage in the search for new materials. Samples of Zn1-xMnxO nanocrystal were synthesized at temperatures of 180 °C and 200 °C using wet or liquid phase synthesis method. Dopant concentrations x=0.5, 1, 1.5, 2, 2.5, 5, 10, 20, 30, 40 and 50 per cent were studied. Powder x-ray diffraction (PXRD) patterns of the samples were analyzed with a view to determining the onset of secondary phases and hence the solubility limit of the dopant. The solubility limit for Mn in ZnO samples synthesized at temperature of 200 °C is realized at x <20%. For samples synthesized at temperature of 180 °C, the solubility limit is x <0.5%.