{"title":"Sintesis Magnesium Oksida (MgO) dari Dolomit Bangkalan dengan Metode Leaching","authors":"D. Saputri, L. Rohmawati","doi":"10.23960/JTAF.V9I2.2808","DOIUrl":null,"url":null,"abstract":"Magnesium oxide (MgO) is a ceramic material that has potential in the medical and industrial fields, where MgO can be obtained from natural dolomite which has a composition of 21.9% MgO and 54.3% CaCO3. However, MgO from dolomite has not been studied much so that this study was conducted with the aim of analyzing the effect of the holding time of calcination on the synthesized MgO phase. The MgO synthesis method uses the Leaching method, which is dissolving dolomite with HCl and stirring it at 75 ° C for 45 minutes. After that, it is filtered where the results of the filtrate are added with ammonia until the solution reaches pH 12 and a precipitate is formed. Furthermore, the precipitate was filtered and dried at 90 ° C for 6 hours, and calcined at a temperature of 800 ° C with a variation of the holding time of 4, 8, 12, 16, and 20 hours. The calcined powder was characterized by XRD and FTIR. The results showed that the optimum MgO periclase main phase was formed at a holding time of 8 hours at a calcination temperature of 800 ° C and had a nanocrystalline size of 20.12 nm. FTIR results show that the MgO synthesized with a holding time of 8 hours has functional groups Mg-O, Mg-O-Mg, C = O, alkene groups, and H-O-H in the wave number range of 4000 cm-1 - 500 cm-1.","PeriodicalId":314761,"journal":{"name":"Jurnal Teori dan Aplikasi Fisika","volume":"240 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2021-07-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Teori dan Aplikasi Fisika","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.23960/JTAF.V9I2.2808","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

Magnesium oxide (MgO) is a ceramic material that has potential in the medical and industrial fields, where MgO can be obtained from natural dolomite which has a composition of 21.9% MgO and 54.3% CaCO3. However, MgO from dolomite has not been studied much so that this study was conducted with the aim of analyzing the effect of the holding time of calcination on the synthesized MgO phase. The MgO synthesis method uses the Leaching method, which is dissolving dolomite with HCl and stirring it at 75 ° C for 45 minutes. After that, it is filtered where the results of the filtrate are added with ammonia until the solution reaches pH 12 and a precipitate is formed. Furthermore, the precipitate was filtered and dried at 90 ° C for 6 hours, and calcined at a temperature of 800 ° C with a variation of the holding time of 4, 8, 12, 16, and 20 hours. The calcined powder was characterized by XRD and FTIR. The results showed that the optimum MgO periclase main phase was formed at a holding time of 8 hours at a calcination temperature of 800 ° C and had a nanocrystalline size of 20.12 nm. FTIR results show that the MgO synthesized with a holding time of 8 hours has functional groups Mg-O, Mg-O-Mg, C = O, alkene groups, and H-O-H in the wave number range of 4000 cm-1 - 500 cm-1.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
用Leaching方法合成班基的氧化镁(MgO)
氧化镁(MgO)是一种在医疗和工业领域具有潜力的陶瓷材料,其中MgO可以从天然白云石中获得,其中MgO的成分为21.9% MgO和54.3% CaCO3。然而,白云石中MgO的研究并不多,因此本研究旨在分析煅烧保温时间对合成MgO相的影响。MgO的合成方法采用浸出法,即用HCl溶解白云石,在75℃下搅拌45分钟。之后,过滤,滤液的结果加入氨,直到溶液达到pH值12,形成沉淀。此外,沉淀物在90°C下过滤干燥6小时,在800°C下煅烧,保温时间分别为4、8、12、16和20小时。用XRD和FTIR对煅烧后的粉末进行了表征。结果表明:在800℃的煅烧温度下,保温8 h形成MgO方长石主相,纳米晶尺寸为20.12 nm;FTIR结果表明,保温8 h合成的MgO在4000 cm-1 ~ 500 cm-1波数范围内具有Mg-O、Mg-O- mg、C = O、烯烃基团和H-O-H等官能团。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Rancang Bangun Alat Ukur Tingkat Manis Buah Jeruk Menggunakan Sensor Kapasitor Semi Silinder Berbasis Arduino Analisis Pengaruh Ukuran Lantai Muatan Timbangan Terhadap Nilai Error Pada Pengujian Eksentrisitas Timbangan Elektronik Sesuai OIML R76 Dynamic Viscosity Measurement Method Based on the Stokes Drag of Prolate Ellipsoidal Mass Analisis Kuantum pada Rangkaian LC dengan Pendekatan Fungsi Gelombang Radial Persamaan Schrȍdinger Potensial Osilator Harmonik Electric Field Controlled Anisotropic Rashba Splitting in Janus Chromium Dichalcogenide Monolayers : A Computational Study based on Density Functional Theory
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1