M. Yahyaoui, K. Limame, B. Jaber, A. Elghazouali, S. Sayouri
{"title":"Synthesis and Structural Studies of Sol Gel Processed Nanopowders of Lead Doped Y2Ti2O7 Pyrochlores","authors":"M. Yahyaoui, K. Limame, B. Jaber, A. Elghazouali, S. Sayouri","doi":"10.15866/IREPHY.V7I6.4457","DOIUrl":null,"url":null,"abstract":"Pyrochlore-type lead doped yttrium titanate (Y2Ti2O7) nanoparticules were successfully synthesized by a sol gel method through the destabilization of colloidal solution (DCS) at a relatively low temperature. The as-preparation samples were characterized using X-ray diffraction (XRD), Fourier-transform-Infrared spectroscopy (FT-IR) and Raman spectroscopy. The results show that doping with 10% of Pb2+ does not bring any structural change, however further Pb-doping ( 20% ≤ x ≤40% ) leads to formation of Y2Ti2O7 phase along with PbTiO3 phase, which indicates that the limit of solubility of Pb2+ in Y2Ti2O7 is under 20%. The evaluated experimental value of this limit agrees with that calculated from the limiting radii ratio stabilization of the pyrochlore structure A2B2O7.","PeriodicalId":448231,"journal":{"name":"International Review of Physics","volume":"27 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2013-12-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Review of Physics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15866/IREPHY.V7I6.4457","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
Pyrochlore-type lead doped yttrium titanate (Y2Ti2O7) nanoparticules were successfully synthesized by a sol gel method through the destabilization of colloidal solution (DCS) at a relatively low temperature. The as-preparation samples were characterized using X-ray diffraction (XRD), Fourier-transform-Infrared spectroscopy (FT-IR) and Raman spectroscopy. The results show that doping with 10% of Pb2+ does not bring any structural change, however further Pb-doping ( 20% ≤ x ≤40% ) leads to formation of Y2Ti2O7 phase along with PbTiO3 phase, which indicates that the limit of solubility of Pb2+ in Y2Ti2O7 is under 20%. The evaluated experimental value of this limit agrees with that calculated from the limiting radii ratio stabilization of the pyrochlore structure A2B2O7.