{"title":"Influence of sintering conditions on the structure formation of tungsten-based composite materials","authors":"А. V. Minitskyi, M. M. Yamshinskij, Ye. H. Byba, N. V. Minitska, K. V. Polishchuk, I. V. Lukianenko, B. V. Kyvhylo","doi":"10.15407/steelcast2023.02.062","DOIUrl":null,"url":null,"abstract":"The use of heavy tungsten alloys is essential for many industries, as these alloys are ideal for a variety of products due to their high density. The main problem in creating such alloys is the need to use high sintering temperatures, which significantly complicates the technology of producing tungsten alloys. To reduce the sintering temperatures of tungsten alloys, alloying elements are added to their composition to activate sintering processes at lower temperatures (nickel, iron and copper). The main task in forming the structure and properties of tungsten-based alloys is to ensure sintering conditions in the presence of the liquid phase, which contributes to the formation of a strong framework in the material structure and high density of the composite. Various methods of producing tungsten-based alloys have been investigated and the influence of the chemical composition of alloying additives on the sintering process conditions has been studied. The effect of pressing and post-pressing pressure on the porosity of tungsten-based molds was determined. It is shown that in the pressure range of 200-700 MPa, the maximum compaction of tungsten powder occurs at pressures of 500-550 MPa, which provides porosity at the level of 35-37 %. The difference between the sintering mechanisms of W-Ni and W-Fe systems at a temperature of 1350 ºC, which is sufficient for liquid-phase sintering with a nickel bond, and low for an iron bond, is shown. The process of infiltration of a porous tungsten alloy framework with copper melt obtained from metal-working waste was studied. The conditions that ensure complete impregnation of the tungsten framework with copper at a temperature of 1200 ºC and allow to obtain a porous material are determined. The results of the work can be used to create tungsten-based products with high specific gravity and density, including from metalworking waste, which significantly reduces the cost of such materials.","PeriodicalId":33778,"journal":{"name":"Metall i lit''e Ukrainy","volume":"30 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metall i lit''e Ukrainy","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15407/steelcast2023.02.062","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The use of heavy tungsten alloys is essential for many industries, as these alloys are ideal for a variety of products due to their high density. The main problem in creating such alloys is the need to use high sintering temperatures, which significantly complicates the technology of producing tungsten alloys. To reduce the sintering temperatures of tungsten alloys, alloying elements are added to their composition to activate sintering processes at lower temperatures (nickel, iron and copper). The main task in forming the structure and properties of tungsten-based alloys is to ensure sintering conditions in the presence of the liquid phase, which contributes to the formation of a strong framework in the material structure and high density of the composite. Various methods of producing tungsten-based alloys have been investigated and the influence of the chemical composition of alloying additives on the sintering process conditions has been studied. The effect of pressing and post-pressing pressure on the porosity of tungsten-based molds was determined. It is shown that in the pressure range of 200-700 MPa, the maximum compaction of tungsten powder occurs at pressures of 500-550 MPa, which provides porosity at the level of 35-37 %. The difference between the sintering mechanisms of W-Ni and W-Fe systems at a temperature of 1350 ºC, which is sufficient for liquid-phase sintering with a nickel bond, and low for an iron bond, is shown. The process of infiltration of a porous tungsten alloy framework with copper melt obtained from metal-working waste was studied. The conditions that ensure complete impregnation of the tungsten framework with copper at a temperature of 1200 ºC and allow to obtain a porous material are determined. The results of the work can be used to create tungsten-based products with high specific gravity and density, including from metalworking waste, which significantly reduces the cost of such materials.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
烧结条件对钨基复合材料结构形成的影响
重钨合金的使用对于许多工业来说是必不可少的,因为这些合金由于其高密度而非常适合各种产品。制造这种合金的主要问题是需要使用高烧结温度,这大大复杂化了生产钨合金的技术。为了降低钨合金的烧结温度,在其成分中加入合金元素以激活较低温度下的烧结过程(镍,铁和铜)。形成钨基合金结构和性能的主要任务是确保液相存在下的烧结条件,这有助于在材料结构中形成坚固的框架和高密度的复合材料。研究了钨基合金的各种制备方法,并研究了合金添加剂的化学成分对烧结工艺条件的影响。确定了压制压力和压制后压力对钨基模具孔隙率的影响。结果表明:在200 ~ 700 MPa压力范围内,500 ~ 550 MPa压力下钨粉的压实度最大,孔隙率为35 ~ 37%;在1350℃下,W-Ni和W-Fe体系的烧结机制存在差异,在1350℃下,W-Ni和W-Fe体系的烧结机制足以进行液相烧结,而在1350℃下,W-Ni和W-Fe体系的烧结机制较低。研究了金属加工废铜熔体对多孔钨合金骨架的渗透过程。确定了在1200℃的温度下确保钨骨架与铜完全浸渍并允许获得多孔材料的条件。这项工作的结果可用于制造具有高比重和高密度的钨基产品,包括金属加工废料,这大大降低了此类材料的成本。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
24
审稿时长
8 weeks
期刊最新文献
Computer modeling of the process of siphon casting of a large metal cylindrical ingot Influence of heat treatment on the structure and wear resistance at abrasive wearing of high-carbon chromonickel steel of 150H15N5VM type Tasks of foundry enterprises in restoring the infrastructure of Ukraine Prerequisites for the use of electromagnetic forces in technologies for refining aluminum alloys from nonmetallic inclusions Improvement of functional and technological solutions for modernization of steel heating in the tundish of continuous casting machine
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1