Incorporating Environmental Impact Analysis into Louisiana’s Balanced Asphalt Mixture Design

Ibrahim Elnaml, H. Dylla, Jun Liu, L. Mohammad, S. Cooper, S. Cooper
{"title":"Incorporating Environmental Impact Analysis into Louisiana’s Balanced Asphalt Mixture Design","authors":"Ibrahim Elnaml, H. Dylla, Jun Liu, L. Mohammad, S. Cooper, S. Cooper","doi":"10.1177/03611981231214231","DOIUrl":null,"url":null,"abstract":"To meet the asphalt pavement industry’s net zero carbon emission goals, increasing reclaimed asphalt pavement (RAP) levels to greater than 25% is considered a critical tactic. However, many state departments of transportation are cautious in adopting high RAP content into their designs because of durability issues resulting from aged RAP binders. This paper assesses the effectiveness of using the Lewis acid catalyst, FeCl3, in improving the cracking resistance of high-RAP asphalt mixtures to meet Louisiana’s balanced mixture design (BMD) criteria, and lower embodied carbon of asphalt mixtures. Four asphalt mixtures were designed and tested against permanent deformation, intermediate- and low-temperature cracking, and durability. Mixture 1 is conventional, which contains performance grade (PG) 76-22 polymer-modified asphalt binder with no RAP. Mixture 2 is unmodified PG 67-22 and 30% RAP without catalyst. Mixtures 3 and 4 incorporated an unmodified asphalt binder PG 67-22, a catalyst, and 30% and 50% RAP, respectively. A life cycle assessment (LCA) analysis was conducted on asphalt mixtures that complied with Louisiana’s BMD specifications to quantify global warming potential improvements. Because the performance of both mixtures is expected to be similar, the scope of the LCA analysis was limited to only those life cycle stages that are expected to be different, modules A1–A3 (i.e., cradle-to-gate stages). Results showed that the use of FeCl3 can improve asphalt mixtures’ cracking resistance containing high RAP contents, whilst it did not have a negative impact on permanent deformation resistance. Further, the addition of FeCl3 to asphalt mixtures with 30% and 50% RAP levels showed a reduction in greenhouse gas emissions by 28% and 43.4%, respectively.","PeriodicalId":309251,"journal":{"name":"Transportation Research Record: Journal of the Transportation Research Board","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-12-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Transportation Research Record: Journal of the Transportation Research Board","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/03611981231214231","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

To meet the asphalt pavement industry’s net zero carbon emission goals, increasing reclaimed asphalt pavement (RAP) levels to greater than 25% is considered a critical tactic. However, many state departments of transportation are cautious in adopting high RAP content into their designs because of durability issues resulting from aged RAP binders. This paper assesses the effectiveness of using the Lewis acid catalyst, FeCl3, in improving the cracking resistance of high-RAP asphalt mixtures to meet Louisiana’s balanced mixture design (BMD) criteria, and lower embodied carbon of asphalt mixtures. Four asphalt mixtures were designed and tested against permanent deformation, intermediate- and low-temperature cracking, and durability. Mixture 1 is conventional, which contains performance grade (PG) 76-22 polymer-modified asphalt binder with no RAP. Mixture 2 is unmodified PG 67-22 and 30% RAP without catalyst. Mixtures 3 and 4 incorporated an unmodified asphalt binder PG 67-22, a catalyst, and 30% and 50% RAP, respectively. A life cycle assessment (LCA) analysis was conducted on asphalt mixtures that complied with Louisiana’s BMD specifications to quantify global warming potential improvements. Because the performance of both mixtures is expected to be similar, the scope of the LCA analysis was limited to only those life cycle stages that are expected to be different, modules A1–A3 (i.e., cradle-to-gate stages). Results showed that the use of FeCl3 can improve asphalt mixtures’ cracking resistance containing high RAP contents, whilst it did not have a negative impact on permanent deformation resistance. Further, the addition of FeCl3 to asphalt mixtures with 30% and 50% RAP levels showed a reduction in greenhouse gas emissions by 28% and 43.4%, respectively.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
将环境影响分析纳入路易斯安那州的平衡沥青混合料设计中
为实现沥青路面行业的净零碳排放目标,将再生沥青路面(RAP)含量提高到 25% 以上被认为是一项关键措施。然而,由于老化的 RAP 粘合剂会导致耐久性问题,许多州交通部门在设计中采用高 RAP 含量时都很谨慎。本文评估了使用路易斯酸催化剂 FeCl3 提高高 RAP 沥青混合料抗裂性的效果,以满足路易斯安那州的平衡混合料设计 (BMD) 标准,并降低沥青混合料的含碳量。设计并测试了四种沥青混合料的永久变形、中温和低温开裂以及耐久性。混合料 1 为常规混合料,含有性能等级 (PG) 76-22 的聚合物改性沥青胶结料,不含 RAP。混合料 2 是未经改性的 PG 67-22 和 30% 的 RAP,不含催化剂。混合物 3 和 4 包括未改性沥青粘结剂 PG 67-22、催化剂以及 30% 和 50% 的 RAP。对符合路易斯安那州 BMD 规范的沥青混合料进行了生命周期评估(LCA)分析,以量化全球升温潜能值的改善情况。由于两种混合物的性能预计相似,因此生命周期评估分析的范围仅限于预计不同的生命周期阶段,即模块 A1-A3(即从摇篮到大门的阶段)。结果表明,使用三氯化铁可以提高高 RAP 含量沥青混合料的抗裂性,同时对永久变形抗性没有负面影响。此外,在 RAP 含量分别为 30% 和 50% 的沥青混合料中添加三氯化铁后,温室气体排放量分别减少了 28% 和 43.4%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Automatic Traffic Safety Analysis using Unmanned Aerial Vehicle Technology at Unsignalized Intersections in Heterogeneous Traffic Role of Bystanders on Women’s Perception of Personal Security When Using Public Transport Comprehensive Investigation of Pedestrian Hit-and-Run Crashes: Applying XGBoost and Binary Logistic Regression Model Insights for Sustainable Urban Transport via Private Charging Pile Sharing in the Electric Vehicle Sector Correlates of Modal Substitution and Induced Travel of Ridehailing in California
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1