{"title":"Study on the Optimization of the Tensile Properties of an Al-Li Alloy Friction Stir-Welding T-Joint","authors":"Yu Qiu, Yuansong Zeng, Qiang Meng, Wei Guan, Jihong Dong, Huaxia Zhao, Lei Cui, Xuepiao Bai, Mingtao Wang","doi":"10.3390/met14091040","DOIUrl":null,"url":null,"abstract":"The softening of aluminum–lithium alloy welded joints generally leads to a reduction in mechanical properties. In this study, a piece of 2A97-T3 aluminum–lithium alloy with a thickness of 2.8 mm was selected as the test material, and the tool and process used for wire-filled stationary shoulder friction stir welding (SSFSW) were developed. By increasing the bearing area of the softening zone, an equal-strength T-joint was manufactured. Good weld formation was obtained when the rotation speed was set to 2000 rpm and the welding speed ranged from 100 to 120 mm/min. The thickness of the softening zone was controlled by adjusting the reserved gap between the shoulder and the workpiece. The softening mechanism of the weld joint was revealed. The softening was attributed to the coarsening of the main precipitated phases (T1 and θ′ phases) in the heat-affected zone (HAZ) and the dissolution of precipitated phases in the thermo-mechanically affected zone (TMAZ). Grain refinement in the nugget zone (NZ) led to a certain fine-grained strengthening effect, although the precipitated phase was almost completely dissolved. Due to the thermal effect of second-pass welding, the hardness value of the NZ and HAZ in the center of the skin further decreased, and the minimum hardness was approximately 70% that of the base material. Tensile testing results indicated that the softening effect was largely offset by the increased bearing area of the softening zone, resulting in the successful welding of high-strength Al-Li alloy T-joints with equal strength. The strength coefficient was found to be 0.977.","PeriodicalId":18461,"journal":{"name":"Metals","volume":"35 1","pages":""},"PeriodicalIF":2.6000,"publicationDate":"2024-09-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metals","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.3390/met14091040","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

The softening of aluminum–lithium alloy welded joints generally leads to a reduction in mechanical properties. In this study, a piece of 2A97-T3 aluminum–lithium alloy with a thickness of 2.8 mm was selected as the test material, and the tool and process used for wire-filled stationary shoulder friction stir welding (SSFSW) were developed. By increasing the bearing area of the softening zone, an equal-strength T-joint was manufactured. Good weld formation was obtained when the rotation speed was set to 2000 rpm and the welding speed ranged from 100 to 120 mm/min. The thickness of the softening zone was controlled by adjusting the reserved gap between the shoulder and the workpiece. The softening mechanism of the weld joint was revealed. The softening was attributed to the coarsening of the main precipitated phases (T1 and θ′ phases) in the heat-affected zone (HAZ) and the dissolution of precipitated phases in the thermo-mechanically affected zone (TMAZ). Grain refinement in the nugget zone (NZ) led to a certain fine-grained strengthening effect, although the precipitated phase was almost completely dissolved. Due to the thermal effect of second-pass welding, the hardness value of the NZ and HAZ in the center of the skin further decreased, and the minimum hardness was approximately 70% that of the base material. Tensile testing results indicated that the softening effect was largely offset by the increased bearing area of the softening zone, resulting in the successful welding of high-strength Al-Li alloy T-joints with equal strength. The strength coefficient was found to be 0.977.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
铝锂合金摩擦搅拌焊接 T 型接头拉伸性能优化研究
铝锂合金焊接接头的软化通常会导致机械性能下降。本研究选择了一块厚度为 2.8 毫米的 2A97-T3 铝锂合金作为试验材料,并开发了用于填丝固定肩搅拌摩擦焊(SSFSW)的工具和工艺。通过增加软化区的承载面积,制造出了等强度的 T 形接头。当转速设定为 2000 rpm,焊接速度为 100 至 120 mm/min 时,焊缝成形良好。软化区的厚度可通过调整肩部与工件之间的预留间隙来控制。结果揭示了焊点的软化机理。软化归因于热影响区(HAZ)中主要析出相(T1 和 θ′相)的粗化和热机械影响区(TMAZ)中析出相的溶解。虽然析出相几乎完全溶解,但金块区(NZ)的晶粒细化产生了一定的细粒强化效应。由于二次焊接的热效应,NZ 和蒙皮中心 HAZ 的硬度值进一步降低,最低硬度约为母材的 70%。拉伸测试结果表明,软化效应在很大程度上被软化区增大的承载面积所抵消,从而成功焊接出了具有同等强度的高强度铝锂合金 T 型接头。强度系数为 0.977。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Metals
Metals MATERIALS SCIENCE, MULTIDISCIPLINARY-METALLURGY & METALLURGICAL ENGINEERING
CiteScore
4.90
自引率
13.80%
发文量
1832
审稿时长
1.5 months
期刊介绍: Metals (ISSN 2075-4701) is an open access journal of related scientific research and technology development. It publishes reviews, regular research papers (articles) and short communications. Our aim is to encourage scientists to publish their experimental and theoretical results in as much detail as possible. Therefore, there is no restriction on the length of the papers. The full experimental details must be provided so that the results can be reproduced. Metals provides a forum for publishing papers which advance the in-depth understanding of the relationship between the structure, the properties or the functions of all kinds of metals.
期刊最新文献
Improvement of High Temperature Wear Resistance of Laser-Cladding High-Entropy Alloy Coatings: A Review New Method to Recover Activation Energy: Application to Copper Oxidation Alternatives to Reduce Hot Cracking Susceptibility of IN718 Casting Alloy Laser Beam Welds with a Mushroom Shape A Method of Images to Study Plate-Impact-Induced Cavitation in Aluminum through Molecular Dynamics Simulation Morphological Characteristics of W/Cu Composite Nanoparticles with Complex Phase Structure Synthesized via Reactive Radio Frequency (RF) Thermal Plasma
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1