Characterization of stiff porous TiC fabricated by in-situ reaction of Ti with carbon derived from phenolic resin containing template

IF 5.8 2区 材料科学 Q1 MATERIALS SCIENCE, CERAMICS Journal of The European Ceramic Society Pub Date : 2025-01-27 DOI:10.1016/j.jeurceramsoc.2025.117241
Diqiang Liu , Hongqiang Zhang , Weiqi Zhao , Guangkun Chen , Aihong Cui , Shujun Zang , Jiangang Jia , Tieming Guo
{"title":"Characterization of stiff porous TiC fabricated by in-situ reaction of Ti with carbon derived from phenolic resin containing template","authors":"Diqiang Liu ,&nbsp;Hongqiang Zhang ,&nbsp;Weiqi Zhao ,&nbsp;Guangkun Chen ,&nbsp;Aihong Cui ,&nbsp;Shujun Zang ,&nbsp;Jiangang Jia ,&nbsp;Tieming Guo","doi":"10.1016/j.jeurceramsoc.2025.117241","DOIUrl":null,"url":null,"abstract":"<div><div>Porous TiC is a representative of porous ceramic showing poor mechanical properties owing to high fabricate temperature. It has attracted increasing attention to fabricate porous TiC with high mechanical strength and 3D porous structure. Here, we introduce an effective way for fabricating porous TiC via template method in which phenolic resin derived carbon reacts with Ti powders to form TiC. Since the porosity and pore structure play important roles in mechanical performance, in this work the porosity of TiC was controlled by template content of NaCl. For investing the formation process of TiC, green body of phenolic resin-Ti was carried out on TG-DSC and DRIFTS. It was revealed that the formation of TiC occurred in two stages, each governed by phenolic resin carbonization, and TiC was formed above 700 ℃. The as-prepared porous TiC possessed unique 3D porous structure and excellent mechanical performance. With the increase of NaCl content, the porosity of TiC increased, but the pore size distribution became narrower. By taking advantage of pore structure, porous TiC showed high compressive strength. Compressive strength together with bulk density gradually decreased with the porosity increase. When the porosity increased from 30.1 % to 55.1 %, the compressive strength decreased from 177.2 MPa to 58.7 MPa. Moreover, the 3D architecture render TiC excellent thermal insulation performance, as the porosity was decreased, the thermal conductivity of porous TiC decreases from 3.5 W/m.K to 1.9 W/m.K.</div></div>","PeriodicalId":17408,"journal":{"name":"Journal of The European Ceramic Society","volume":"45 7","pages":"Article 117241"},"PeriodicalIF":5.8000,"publicationDate":"2025-01-27","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of The European Ceramic Society","FirstCategoryId":"88","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0955221925000615","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0

Abstract

Porous TiC is a representative of porous ceramic showing poor mechanical properties owing to high fabricate temperature. It has attracted increasing attention to fabricate porous TiC with high mechanical strength and 3D porous structure. Here, we introduce an effective way for fabricating porous TiC via template method in which phenolic resin derived carbon reacts with Ti powders to form TiC. Since the porosity and pore structure play important roles in mechanical performance, in this work the porosity of TiC was controlled by template content of NaCl. For investing the formation process of TiC, green body of phenolic resin-Ti was carried out on TG-DSC and DRIFTS. It was revealed that the formation of TiC occurred in two stages, each governed by phenolic resin carbonization, and TiC was formed above 700 ℃. The as-prepared porous TiC possessed unique 3D porous structure and excellent mechanical performance. With the increase of NaCl content, the porosity of TiC increased, but the pore size distribution became narrower. By taking advantage of pore structure, porous TiC showed high compressive strength. Compressive strength together with bulk density gradually decreased with the porosity increase. When the porosity increased from 30.1 % to 55.1 %, the compressive strength decreased from 177.2 MPa to 58.7 MPa. Moreover, the 3D architecture render TiC excellent thermal insulation performance, as the porosity was decreased, the thermal conductivity of porous TiC decreases from 3.5 W/m.K to 1.9 W/m.K.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
求助全文
约1分钟内获得全文 去求助
来源期刊
Journal of The European Ceramic Society
Journal of The European Ceramic Society 工程技术-材料科学:硅酸盐
CiteScore
10.70
自引率
12.30%
发文量
863
审稿时长
35 days
期刊介绍: The Journal of the European Ceramic Society publishes the results of original research and reviews relating to ceramic materials. Papers of either an experimental or theoretical character will be welcomed on a fully international basis. The emphasis is on novel generic science concerning the relationships between processing, microstructure and properties of polycrystalline ceramics consolidated at high temperature. Papers may relate to any of the conventional categories of ceramic: structural, functional, traditional or composite. The central objective is to sustain a high standard of research quality by means of appropriate reviewing procedures.
期刊最新文献
Multi-mechanism cooperative optimization of electromagnetic shielding and mechanical properties in Cf/PyC/SiC-SiCN(Fe) ceramic-based composites Oxidation resistance and protective mechanism of ZrB2-SiC coating modified by Y2O3 at 1700 ℃ Controllable morphology genetic composites of porous SiC/Ti3SiC2 synthesized via template assembly strategy for tunable microwave absorption performance Enhancement of thermoelectric properties of electropositive and electronegative element double-filled CoSb3 via high-pressure regulating Piezoelectric performances of <001> -textured (Ag,K)NbO3 ceramics
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1