The removal of three kinds of occlusal veneers by Er: Yag laser.

Jianyu Zhu, Feifei Hong, Lianghang He, Wei Wen, Xianlin Lei, Zhisheng Zhang, Lu Yin
{"title":"The removal of three kinds of occlusal veneers by Er: Yag laser.","authors":"Jianyu Zhu,&nbsp;Feifei Hong,&nbsp;Lianghang He,&nbsp;Wei Wen,&nbsp;Xianlin Lei,&nbsp;Zhisheng Zhang,&nbsp;Lu Yin","doi":"10.7518/hxkq.2023.2023038","DOIUrl":null,"url":null,"abstract":"<p><strong>Objectives: </strong>This study aimed to remove occlusal veneers of varied thicknesses and compositions by Er:Yag laser <i>in vitro</i> and analyze the interfacial microstructure between veneers and tooth that irradiated by laser, by which experimental evidence could be provided to support the non-invasive removal of occlusal veneerby laser.</p><p><strong>Methods: </strong>Fresh mandibular premolars extracted for orthodontic requirements were collected for tooth preparation. Three kinds of ceramic materials (Vita Suprinity, Vita Mark Ⅱ, and Upcera Hyramic) were selected to fabricate occlusal veneer with different thicknesses (1.0, 1.5, and 2.0 mm). One week later, Er:Yag laser (2.5 W and 3.5 W) was used to irradiate and remove the occlusal veneer and recorded the timespan. After the removal operation, the micro-morphologies of samples were examined by scanning electron microscope.</p><p><strong>Results: </strong>Upcera Hyramic veneer failed to be removed (>20 min); the operation span at 2.5 W, Vita Suprinity (96.0 s±16.0 s) was longer than Vita MarkⅡ(84.5 s±19.5 s) in the 1.0 mm group (<i>P</i><0.05), and Vita Suprinity (246.5 s±13.5 s) was longer than Vita MarkⅡ(170.0 s±14.0 s) in the 1.5 mm group (<i>P</i><0.05). At 3.5 W, Vita Suprinity (381.0 s±24.0 s) was longer than Vita MarkⅡ(341.5 s±26.5 s) in the 2.0 mm group.</p><p><strong>Conclusions: </strong>Increasing laser power could shorten the operation span and facilitate the removal of occlusal veneers with the same thickness and composition. The occlusal veneer was sustained when insufficient laser power was applied. With the same laser power and ceramic thickness, laser penetration could interfere with the integral of the ceramic structure when the laser interacted with the bonding layer. With the same ceramic composition and laser power, the operation span and laser power increased with the thickness of the occlusal veneer. However, the laser was incapable of removing occlusal resin veneer directly.</p>","PeriodicalId":94028,"journal":{"name":"Hua xi kou qiang yi xue za zhi = Huaxi kouqiang yixue zazhi = West China journal of stomatology","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10580231/pdf/wcjs-41-05-568.pdf","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Hua xi kou qiang yi xue za zhi = Huaxi kouqiang yixue zazhi = West China journal of stomatology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.7518/hxkq.2023.2023038","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Objectives: This study aimed to remove occlusal veneers of varied thicknesses and compositions by Er:Yag laser in vitro and analyze the interfacial microstructure between veneers and tooth that irradiated by laser, by which experimental evidence could be provided to support the non-invasive removal of occlusal veneerby laser.

Methods: Fresh mandibular premolars extracted for orthodontic requirements were collected for tooth preparation. Three kinds of ceramic materials (Vita Suprinity, Vita Mark Ⅱ, and Upcera Hyramic) were selected to fabricate occlusal veneer with different thicknesses (1.0, 1.5, and 2.0 mm). One week later, Er:Yag laser (2.5 W and 3.5 W) was used to irradiate and remove the occlusal veneer and recorded the timespan. After the removal operation, the micro-morphologies of samples were examined by scanning electron microscope.

Results: Upcera Hyramic veneer failed to be removed (>20 min); the operation span at 2.5 W, Vita Suprinity (96.0 s±16.0 s) was longer than Vita MarkⅡ(84.5 s±19.5 s) in the 1.0 mm group (P<0.05), and Vita Suprinity (246.5 s±13.5 s) was longer than Vita MarkⅡ(170.0 s±14.0 s) in the 1.5 mm group (P<0.05). At 3.5 W, Vita Suprinity (381.0 s±24.0 s) was longer than Vita MarkⅡ(341.5 s±26.5 s) in the 2.0 mm group.

Conclusions: Increasing laser power could shorten the operation span and facilitate the removal of occlusal veneers with the same thickness and composition. The occlusal veneer was sustained when insufficient laser power was applied. With the same laser power and ceramic thickness, laser penetration could interfere with the integral of the ceramic structure when the laser interacted with the bonding layer. With the same ceramic composition and laser power, the operation span and laser power increased with the thickness of the occlusal veneer. However, the laser was incapable of removing occlusal resin veneer directly.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Er:Yag激光对三种牙合贴面的去除。
目的:本研究旨在用Er:Yag激光在体外去除不同厚度和成分的咬合单板,并分析激光照射下单板与牙齿之间的界面微观结构,为激光无创去除咬合单板提供实验依据。方法:收集新鲜的下颌前磨牙进行正畸预备。选择三种陶瓷材料(Vita Suprinity、Vita MarkⅡ和Upcera Hyramic)制作不同厚度(1.0、1.5和2.0mm)的咬合贴面。一周后,使用Er:Yag激光(2.5W和3.5W)照射并去除咬合贴面,并记录时间跨度。去除操作后,通过扫描电子显微镜检查样品的微观形貌。结果:上角Hyramic单板切除失败(>20min);2.5W的操作跨度,1.0 mm组的Vita Suprinity(96.0 s±16.0 s)比Vita MarkⅡ(84.5 s±19.5 s)长(PPC结论:增加激光功率可以缩短手术时间,有利于相同厚度和成分的咬合单板的去除。当激光功率不足时,咬合单板是持续的。在相同激光功率和陶瓷厚度的情况下,当激光与陶瓷相互作用时,激光穿透会干扰陶瓷结构的整体性。)粘结层。在相同陶瓷成分和激光功率的情况下,手术时间和激光功率随着咬合单板厚度的增加而增加。然而,激光无法直接去除咬合树脂贴面。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Advantages of remimazolam for sedation in impacted tooth extraction. Anti-inflammatory effects and related mechanisms of naringenin in human periodontal ligament stem cells under lipopolysaccharide stimulation based on RNA sequencing. Application of digital impression and model in removable partial dentures for Kennedy classⅠandⅡdentition defects. Brass wire ligation for treatment of the ectopic eruption of the mandibular second molar: a case report. Current status and influencing factors of fear of surgery in patients with oral and maxillofacial tumors.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1