M. Mališová, M. Horňáček, J. Mikulec, P. Hudec, V. Jorík
{"title":"FTIR study of hydrotalcite","authors":"M. Mališová, M. Horňáček, J. Mikulec, P. Hudec, V. Jorík","doi":"10.2478/acs-2018-0021","DOIUrl":null,"url":null,"abstract":"Abstract The aim of the research was the study of aluminium-magnesium hydrotalcite by FTIR analysis and detection of differences in structure due to calcination. Three types of samples were analysed. In the first two samples, cobalt was added into the structure and the third sample contained nickel and zinc. Hydrotalcite was prepared by one of the most common methods of hydrotalcite preparation, co-precipitation. After preparation, the samples were calcined at temperatures from 150 °C to 750 °C. Samples were compared in terms of calcination temperature; but in case of samples containing cobalt, two samples to each other. The most significant changes were noticed in the 500–700 cm−1 region, where a spinel structure was formed at higher calcination temperatures.","PeriodicalId":7088,"journal":{"name":"Acta Chimica Slovaca","volume":"11 1","pages":"147 - 156"},"PeriodicalIF":0.9000,"publicationDate":"2018-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"12","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Acta Chimica Slovaca","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2478/acs-2018-0021","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"CHEMISTRY, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 12
Abstract
Abstract The aim of the research was the study of aluminium-magnesium hydrotalcite by FTIR analysis and detection of differences in structure due to calcination. Three types of samples were analysed. In the first two samples, cobalt was added into the structure and the third sample contained nickel and zinc. Hydrotalcite was prepared by one of the most common methods of hydrotalcite preparation, co-precipitation. After preparation, the samples were calcined at temperatures from 150 °C to 750 °C. Samples were compared in terms of calcination temperature; but in case of samples containing cobalt, two samples to each other. The most significant changes were noticed in the 500–700 cm−1 region, where a spinel structure was formed at higher calcination temperatures.