Estimation of Fatigue Strength of Reinforced Complete Upper Denture Using a Newly Designed Testing Machine: A Laboratory Research Project

A. Prombonas, N. Poulis, E. Prombonas
{"title":"Estimation of Fatigue Strength of Reinforced Complete Upper Denture Using a Newly Designed Testing Machine: A Laboratory Research Project","authors":"A. Prombonas, N. Poulis, E. Prombonas","doi":"10.4236/JBISE.2021.142006","DOIUrl":null,"url":null,"abstract":"In the present study, an aero pneumatic fatigue testing machine for complete dentures was designed, fabricated, and tested for the evaluation of the fatigue life of reinforced complete upper denture (CUD). On completion and testing, it was observed that the machine has the potential of generating reliable number of cyclic data. The machine’s performance was evaluated using test specimens of identical CUDs that were machined in conformity with standard procedures. The fatigue machine compressed the lower dental arch over the upper denture-specimen in centric occlusion, in the same way that the two masticatory muscles pull the lower jaw over the upper jaw during chewing. The incorporation of glass fibres into the CUD using a sandwich technique quadruples the lifespan of the denture (P = 0.004). The low standard deviation, along with the low coefficient of variation (CV) of the group of unreinforced dentures shows the repeatability of the results and the reliability of the machine. The high standard deviation and coefficient of variation of reinforced dentures was expected, since a high variation of results is usually recorded in fibre reinforcement cases. This research confirmed the view that the crack during denture fracture initiates in the anterior palatal area and propagates to the posterior.","PeriodicalId":64231,"journal":{"name":"生物医学工程(英文)","volume":"14 1","pages":"48-63"},"PeriodicalIF":0.0000,"publicationDate":"2021-02-07","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"生物医学工程(英文)","FirstCategoryId":"1087","ListUrlMain":"https://doi.org/10.4236/JBISE.2021.142006","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

In the present study, an aero pneumatic fatigue testing machine for complete dentures was designed, fabricated, and tested for the evaluation of the fatigue life of reinforced complete upper denture (CUD). On completion and testing, it was observed that the machine has the potential of generating reliable number of cyclic data. The machine’s performance was evaluated using test specimens of identical CUDs that were machined in conformity with standard procedures. The fatigue machine compressed the lower dental arch over the upper denture-specimen in centric occlusion, in the same way that the two masticatory muscles pull the lower jaw over the upper jaw during chewing. The incorporation of glass fibres into the CUD using a sandwich technique quadruples the lifespan of the denture (P = 0.004). The low standard deviation, along with the low coefficient of variation (CV) of the group of unreinforced dentures shows the repeatability of the results and the reliability of the machine. The high standard deviation and coefficient of variation of reinforced dentures was expected, since a high variation of results is usually recorded in fibre reinforcement cases. This research confirmed the view that the crack during denture fracture initiates in the anterior palatal area and propagates to the posterior.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
基于新设计的全口义齿疲劳强度试验机的试验研究
本研究设计、制造并测试了一台用于全口义齿的气动疲劳试验机,用于评估增强型全口义齿(CUD)的疲劳寿命。在完成和测试后,观察到该机器具有生成可靠数量的循环数据的潜力。使用按照标准程序加工的相同CUD的试样来评估机器的性能。疲劳机在中心咬合的情况下将下牙弓压在上义齿样本上,就像咀嚼时两块咀嚼肌将下颌拉到上颌上一样。使用夹层技术将玻璃纤维掺入CUD可使义齿的寿命延长四倍(P=0.004)。低标准偏差以及无增强义齿组的低变异系数(CV)表明了结果的可重复性和机器的可靠性。强化义齿的标准偏差和变异系数较高,这是意料之中的事,因为在纤维强化病例中通常会记录到较高的结果变异。这项研究证实了义齿断裂过程中的裂纹从腭前部开始并向后部扩展的观点。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
900
期刊最新文献
Tectona grandis (Teak Tree) Young Leaf Extract as a Histological Stain An Alternative Method for Incorporating Fiber Meshes in Complete Upper Dentures Research on the Chemical Hazard Risk of Toys Exported to EU from China Based on the Analysis of the EU “Safety Gate” Alerts Cases Impact of Association between Functional Training and Respiratory Muscle Training in Elderly: A Randomized Controlled Trial Morphogenesis of Floating Bone Segments: A Legacy of Serial Tensile Cross-Strut Microdamage in Trabecular Disconnection “Crumple Zones”?
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1