Effects of Pd layer thickness on mechanical properties and microstructures of Sn-3.0 Ag-0.5 Cu solder joints

Yong–Il Kim, Jaehyun Yoon, Seung-Boo Jung
{"title":"Effects of Pd layer thickness on mechanical properties and microstructures of Sn-3.0 Ag-0.5 Cu solder joints","authors":"Yong–Il Kim, Jaehyun Yoon, Seung-Boo Jung","doi":"10.1504/IJMSI.2014.064775","DOIUrl":null,"url":null,"abstract":"In order to investigate effects of Pd layer thickness on the mechanical properties and microstructures of Sn-3.0 Ag-0.5 Cu solder joints, three different Pd layers, i.e., 0.05, 0.1, 0.15 µm, were employed on the electroless nickel immersion gold [ENIG, Ni-P(5 µm )/Au(0.08 µm)] surface finished flame retardant type 4 (FR4) printed circuit board (PCB) substrates. Our studies showed that the addition of Pd layer in ENIG treatment, i.e., ENEPIG, enhanced the bonding strength of solder joints by reducing the formation of intermetallic compounds (IMCs), (Cu, Ni)6Sn5 and (Ni, Cu)3Sn4. The different failure modes were also observed – the crack propagation occurred along the interface between P-rich Ni layer and Cu layer in 0.05 µm Pd specimens while specimens with 0.1 µm and 0.15 µm Pd layers showed the crack propagation proceeded mostly inside solders. In this study the effects of Pd layer thickness in ENEPIG surface finish on the bonding strength of solder joints were investigated by means of drop test and ball shear test, followed by observation of microstructures and interfaces using a scanning electron microscope (SEM) and an energy dispersive spectrometer (EDS).","PeriodicalId":39035,"journal":{"name":"International Journal of Materials and Structural Integrity","volume":"112 1","pages":"76"},"PeriodicalIF":0.0000,"publicationDate":"2014-09-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1504/IJMSI.2014.064775","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Materials and Structural Integrity","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1504/IJMSI.2014.064775","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Engineering","Score":null,"Total":0}
引用次数: 1

Abstract

In order to investigate effects of Pd layer thickness on the mechanical properties and microstructures of Sn-3.0 Ag-0.5 Cu solder joints, three different Pd layers, i.e., 0.05, 0.1, 0.15 µm, were employed on the electroless nickel immersion gold [ENIG, Ni-P(5 µm )/Au(0.08 µm)] surface finished flame retardant type 4 (FR4) printed circuit board (PCB) substrates. Our studies showed that the addition of Pd layer in ENIG treatment, i.e., ENEPIG, enhanced the bonding strength of solder joints by reducing the formation of intermetallic compounds (IMCs), (Cu, Ni)6Sn5 and (Ni, Cu)3Sn4. The different failure modes were also observed – the crack propagation occurred along the interface between P-rich Ni layer and Cu layer in 0.05 µm Pd specimens while specimens with 0.1 µm and 0.15 µm Pd layers showed the crack propagation proceeded mostly inside solders. In this study the effects of Pd layer thickness in ENEPIG surface finish on the bonding strength of solder joints were investigated by means of drop test and ball shear test, followed by observation of microstructures and interfaces using a scanning electron microscope (SEM) and an energy dispersive spectrometer (EDS).
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Pd层厚度对Sn-3.0 Ag-0.5 Cu焊点力学性能和组织的影响
为了研究Pd层厚度对Sn-3.0 Ag-0.5 Cu焊点力学性能和显微组织的影响,在化学镀镍浸金[ENIG, Ni-P(5µm) /Au(0.08µm)]表面加工阻燃型4 (FR4)印刷电路板(PCB)衬底上采用了3种不同的Pd层,即0.05、0.1和0.15µm。我们的研究表明,在ENIG处理中加入Pd层,即ENEPIG,通过减少金属间化合物(IMCs), (Cu, Ni)6Sn5和(Ni, Cu)3Sn4的形成,提高了焊点的结合强度。在0.05µm Pd试样中,裂纹沿富p - Ni层与Cu层的界面扩展,而在0.1µm和0.15µm Pd试样中,裂纹主要在钎料内部扩展。通过跌落试验和球剪试验,利用扫描电镜(SEM)和能谱仪(EDS)观察了ENEPIG表面处理中Pd层厚度对焊点结合强度的影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
0.40
自引率
0.00%
发文量
0
期刊最新文献
Compressive strength enhancement of concrete using fly ash as a partial replacement of fine aggregate and model development Flexural fatigue analysis of fibre reinforced polymer concrete composites under non-reversed loading A new simple formulation for instantaneous coil diameter of a SMA helical spring Effects of two-step heat treatment on the structure of cotton-derived activated carbon fibres Mechanics of contact interaction and deformation of main pipelines in the conditions of extreme external actions
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1