M. Sellami, K. Zouaoui, B. Talbi, C. Mekki-Douadji, M. Berahal, F. Merabet, K. Ezziane
{"title":"Synthesis and physical properties of pyrochlore cobalt oxides Bi1.56-xCaxSb1.48Co0.96O7-δ","authors":"M. Sellami, K. Zouaoui, B. Talbi, C. Mekki-Douadji, M. Berahal, F. Merabet, K. Ezziane","doi":"10.1590/0366-69132023693903404","DOIUrl":null,"url":null,"abstract":"We report here the influence of the partial substitution of bismuth by calcium on the electric and magnetic properties of the Bi 1.56-x Ca x Sb 1.48 Co 0.96 O 7-δ solid solution. We used the ceramic method at 1000 °C in air. The difference in charge of the substitution cations causes an oxygen deficit to appear in the (Bi 1.56-x Ca x Co 0.44 )(Sb 1.48 Co 0.52 )O 7-δ pyrochlore formula. The starting compound Bi 1.56 Sb 1.48 Co 0.96 O 7 [17] has been used in photocatalysis for the degradation of rhodamine B [18]. The obtained results prompted us to synthesize this solid solution and see the influence of oxygen deficit on the degradation of rhodamine B. The photocatalysis applications are in progress and will be the subject of a future publication.","PeriodicalId":9824,"journal":{"name":"Cerâmica","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cerâmica","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1590/0366-69132023693903404","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"Materials Science","Score":null,"Total":0}
引用次数: 0
Abstract
We report here the influence of the partial substitution of bismuth by calcium on the electric and magnetic properties of the Bi 1.56-x Ca x Sb 1.48 Co 0.96 O 7-δ solid solution. We used the ceramic method at 1000 °C in air. The difference in charge of the substitution cations causes an oxygen deficit to appear in the (Bi 1.56-x Ca x Co 0.44 )(Sb 1.48 Co 0.52 )O 7-δ pyrochlore formula. The starting compound Bi 1.56 Sb 1.48 Co 0.96 O 7 [17] has been used in photocatalysis for the degradation of rhodamine B [18]. The obtained results prompted us to synthesize this solid solution and see the influence of oxygen deficit on the degradation of rhodamine B. The photocatalysis applications are in progress and will be the subject of a future publication.
期刊介绍:
A Revista Cerâmica, órgão oficial da Associação Brasileira de Cerâmica (ABCERAM) publica contribuições originais de interesse na área de cerâmica, compreendendo arte cerâmica, abrasivos, biocerâmicas, cerâmicas avançadas, cerâmica branca, cerâmica de mesa, cerâmica eletroeletrônica, cerâmica estrutural, cerâmica magnética, cerâmica nuclear, cerâmica óptica, cerâmica química, cerâmica termomecânica, cerâmica vermelha, cimento, compósitos de matriz cerâmica, materiais refratários, materiais de revestimento, matérias-primas, vidrados, vidros e vitrocerâmicas, análise microestrutural, ciência básica, instrumentação, processos de fabricação, síntese de pós, técnicas de caracterização etc.