{"title":"Influence of Er3+ doping on the mechanical and thermophysical properties of (ErxY1-x)3Al5O12 ceramics","authors":"Xuanli Wang, Jinxing Xing, Min Xie, R. Mu, Xi-wen Song","doi":"10.2298/pac2301023w","DOIUrl":null,"url":null,"abstract":"In this work, Er3+ was selected to replace Y3+ in the yttrium aluminium garnet (YAG) in order to improve its mechanical and thermophysical properties. A series of (ErxY1-x)3Al5O12 (x = 0, 0.1, 0.3, 0.5, 0.7, 0.9 and 1.0) ceramics were prepared by solid-state synthesis method at 1000 ?C and finally sintered at 1600 ?C for 5 h. The microstructure and morphology of the prepared ceramics were investigated. The results showed that all Er3+ doped Y3Al5O12 ceramics exhibited single garnet-type YAG phase and good compactness. With the increase of Er3+ doping concentration, the thermal conductivity of the (ErxY1-x)3Al5O12 ceramics decreased slowly and then increased subsequently. Among the investigated specimens, the (Er0.7Y0.3)3Al5O12 had the lowest thermal conductivity (1.51W/m?K, at 1000 ?C), which was about 28% lower than that of the pure YAG (2.1W/m?K, at 1000 ?C). As the Er3+ doping concentration increased, the thermal expansion coefficient of the (ErxY1-x)3Al5O12 ceramics hardly changed, remaining around 9.08 ? 10?6 K?1 at 1200 ?C. Moreover, when the Er3+ doping concentration exceeded 0.5, the mechanical properties of the (ErxY1-x)3Al5O12 ceramics increased suddenly. Specifically, the hardness increased from 14.28 to 16.53GPa and the bending strength increased from 231.74 to 324.49MPa.","PeriodicalId":20596,"journal":{"name":"Processing and Application of Ceramics","volume":"1 1","pages":""},"PeriodicalIF":0.9000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Processing and Application of Ceramics","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.2298/pac2301023w","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0

Abstract

In this work, Er3+ was selected to replace Y3+ in the yttrium aluminium garnet (YAG) in order to improve its mechanical and thermophysical properties. A series of (ErxY1-x)3Al5O12 (x = 0, 0.1, 0.3, 0.5, 0.7, 0.9 and 1.0) ceramics were prepared by solid-state synthesis method at 1000 ?C and finally sintered at 1600 ?C for 5 h. The microstructure and morphology of the prepared ceramics were investigated. The results showed that all Er3+ doped Y3Al5O12 ceramics exhibited single garnet-type YAG phase and good compactness. With the increase of Er3+ doping concentration, the thermal conductivity of the (ErxY1-x)3Al5O12 ceramics decreased slowly and then increased subsequently. Among the investigated specimens, the (Er0.7Y0.3)3Al5O12 had the lowest thermal conductivity (1.51W/m?K, at 1000 ?C), which was about 28% lower than that of the pure YAG (2.1W/m?K, at 1000 ?C). As the Er3+ doping concentration increased, the thermal expansion coefficient of the (ErxY1-x)3Al5O12 ceramics hardly changed, remaining around 9.08 ? 10?6 K?1 at 1200 ?C. Moreover, when the Er3+ doping concentration exceeded 0.5, the mechanical properties of the (ErxY1-x)3Al5O12 ceramics increased suddenly. Specifically, the hardness increased from 14.28 to 16.53GPa and the bending strength increased from 231.74 to 324.49MPa.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Er3+掺杂对(ErxY1-x)3Al5O12陶瓷力学和热物理性能的影响
本文选择Er3+取代钇铝石榴石(YAG)中的Y3+,以改善其机械和热物理性能。采用固态合成法在1000℃下制备了一系列(ErxY1-x) 3al5012 (x = 0、0.1、0.3、0.5、0.7、0.9和1.0)陶瓷,最后在1600℃下烧结5 h,研究了所制备陶瓷的微观结构和形貌。结果表明,所有掺Er3+的Y3Al5O12陶瓷均表现出单一的石榴石型YAG相和良好的致密性。随着Er3+掺杂浓度的增加,(ErxY1-x)3Al5O12陶瓷的导热系数先降低后升高。在所研究的试样中,(Er0.7Y0.3)3Al5O12的导热系数最低,为1.51W/m?K,在1000℃时),比纯YAG (2.1W/m?K,在1000℃时)。随着Er3+掺杂浓度的增加,(ErxY1-x)3Al5O12陶瓷的热膨胀系数几乎没有变化,保持在9.08 ?10?6 K ?1200c。此外,当Er3+掺杂浓度超过0.5时,(ErxY1-x)3Al5O12陶瓷的力学性能突然提高。硬度从14.28 gpa提高到16.53GPa,抗弯强度从231.74 mpa提高到324.49MPa。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Processing and Application of Ceramics
Processing and Application of Ceramics MATERIALS SCIENCE, CERAMICS-
CiteScore
1.90
自引率
9.10%
发文量
14
审稿时长
10 weeks
期刊介绍: Information not localized
期刊最新文献
Viscosity optimisation of photosensitive al2o3 slurry for stereolithography based additive manufacturing Comments on the paper “Structure, electric and dielectric properties of PbFe1/3Ti1/3W1/3O3 single perovskite compound” by P.G.R. Achary, R.N.P. Choudhary, S.K. Parida, published in Processing and Application of Ceramics 14 (2020) 146-153 Theoretical prediction by DFT on properties of β′-SrTa2O6 crystal Production of tib2 coatings on graphite substrates by electrophoretic deposition in NaF-AlF3 melt Use of cobalt ferrite and activated carbon in supercapacitors
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1