{"title":"Specific Surface Free Energy of As-Grown and Polished Faces of Synthetic Quartz","authors":"Takaomi Suzuki, Keiko Takahashi, M. Kawasaki, T. Kagami","doi":"10.4236/JCPT.2014.44022","DOIUrl":null,"url":null,"abstract":"Contact angles of water droplet on as-grown Z, +X, –X, and m faces of synthetic quartz crystals with growth term of 20 and 48 days, and polished Z, +X, –X, Y, and 45° cut faces of synthetic quartz crystal were observed. The average of the contact angles on as-grown Z, +X, and –X faces increased with the growth term, and they were larger than that on polished Z, +X, and –X faces. On the other hand, the average of the contact angles of water on m face decreased with the growth term, and they were smaller than that on polished Y cut face. Growth rate of the faces of synthetic crystals was measured and the order of growth rate was, m < –X < +X < Z. Specific surface free energy (SSFE) was calculated using Neumann’s equation. The SSFE of polished face was in the order of, m < –X < +X < Z, which corresponds to the order of the growth rate. The SSFE was larger for the face with larger growth rate.","PeriodicalId":64440,"journal":{"name":"结晶过程及技术期刊(英文)","volume":"04 1","pages":"177-184"},"PeriodicalIF":0.0000,"publicationDate":"2014-10-06","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"结晶过程及技术期刊(英文)","FirstCategoryId":"1087","ListUrlMain":"https://doi.org/10.4236/JCPT.2014.44022","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 4
Abstract
Contact angles of water droplet on as-grown Z, +X, –X, and m faces of synthetic quartz crystals with growth term of 20 and 48 days, and polished Z, +X, –X, Y, and 45° cut faces of synthetic quartz crystal were observed. The average of the contact angles on as-grown Z, +X, and –X faces increased with the growth term, and they were larger than that on polished Z, +X, and –X faces. On the other hand, the average of the contact angles of water on m face decreased with the growth term, and they were smaller than that on polished Y cut face. Growth rate of the faces of synthetic crystals was measured and the order of growth rate was, m < –X < +X < Z. Specific surface free energy (SSFE) was calculated using Neumann’s equation. The SSFE of polished face was in the order of, m < –X < +X < Z, which corresponds to the order of the growth rate. The SSFE was larger for the face with larger growth rate.