{"title":"Effect of artificial aging on mechanical and physical properties of CAD-CAM PMMA resins for occlusal splints.","authors":"Júlia Correa Raffaini, Eduardo Jose Soares, Rebeca Franco de Lima Oliveira, Rocio Geng Vivanco, Ayodele Alves Amorim, Ana Lucia Caetano Pereira, Fernanda Carvalho Panzeri Pires-de-Souza","doi":"10.4047/jap.2023.15.5.227","DOIUrl":null,"url":null,"abstract":"<p><strong>Purpose: </strong>This study aimed to assess and compare the color stability, flexural strength (FS), and surface roughness of occlusal splints fabricated from heat-cured acrylic resin, milled polymethyl methacrylate (PMMA)-based resin, and 3D-printed (PMMA) based-resin.</p><p><strong>Materials and methods: </strong>Samples of each type of resin were obtained, and baseline measurements of color and surface roughness were recorded. The specimens were divided into three groups (n = 10) and subjected to distinct aging protocols: thermomechanical cycling (TMC), simulated brushing (SB), and control (without aging). Final assessments of color and surface roughness and three-point bending test (ODM100; Odeme) were conducted, and data were statistically analyzed (2-way ANOVA, Tukey, <i>P</i> <.05).</p><p><strong>Results: </strong>Across all resin types, the most significant increase in surface roughness (Ra) was observed after TMC (<i>P</i> < .05), with the 3D-printed resin exhibiting the lowest Ra (<i>P</i> < .05). After brushing, milled resin displayed the highest Ra (<i>P</i> < .05) and greater color alteration (ΔE<sub>00</sub>) compared to 3D-printed resin. The most substantial ΔE<sub>00</sub> was recorded after brushing for all resins, except for heat-cured resin subjected to TMC. Regardless of aging, milled resin exhibited the highest FS (<i>P</i> < .05), except when compared to 3D-printed resin subjected to TMC. Heat-cured resin exposed to TMC demonstrated the lowest FS, different (<i>P</i> < .05) from the control. Under control conditions, milled resin exhibited the highest FS, different (<i>P</i> < .05) from the brushed group. 3D-printed resin subjected to TMC displayed the highest FS (<i>P</i> < .05).</p><p><strong>Conclusion: </strong>Among the tested resins, 3D-printed resin demonstrated superior longevity, characterized by minimal surface roughness and color alterations. Aging had a negligible impact on its mechanical properties.</p>","PeriodicalId":51291,"journal":{"name":"Journal of Advanced Prosthodontics","volume":"15 5","pages":"227-237"},"PeriodicalIF":2.7000,"publicationDate":"2023-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10625884/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Advanced Prosthodontics","FirstCategoryId":"3","ListUrlMain":"https://doi.org/10.4047/jap.2023.15.5.227","RegionNum":3,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2023/10/26 0:00:00","PubModel":"Epub","JCR":"Q1","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0
Abstract
Purpose: This study aimed to assess and compare the color stability, flexural strength (FS), and surface roughness of occlusal splints fabricated from heat-cured acrylic resin, milled polymethyl methacrylate (PMMA)-based resin, and 3D-printed (PMMA) based-resin.
Materials and methods: Samples of each type of resin were obtained, and baseline measurements of color and surface roughness were recorded. The specimens were divided into three groups (n = 10) and subjected to distinct aging protocols: thermomechanical cycling (TMC), simulated brushing (SB), and control (without aging). Final assessments of color and surface roughness and three-point bending test (ODM100; Odeme) were conducted, and data were statistically analyzed (2-way ANOVA, Tukey, P <.05).
Results: Across all resin types, the most significant increase in surface roughness (Ra) was observed after TMC (P < .05), with the 3D-printed resin exhibiting the lowest Ra (P < .05). After brushing, milled resin displayed the highest Ra (P < .05) and greater color alteration (ΔE00) compared to 3D-printed resin. The most substantial ΔE00 was recorded after brushing for all resins, except for heat-cured resin subjected to TMC. Regardless of aging, milled resin exhibited the highest FS (P < .05), except when compared to 3D-printed resin subjected to TMC. Heat-cured resin exposed to TMC demonstrated the lowest FS, different (P < .05) from the control. Under control conditions, milled resin exhibited the highest FS, different (P < .05) from the brushed group. 3D-printed resin subjected to TMC displayed the highest FS (P < .05).
Conclusion: Among the tested resins, 3D-printed resin demonstrated superior longevity, characterized by minimal surface roughness and color alterations. Aging had a negligible impact on its mechanical properties.
期刊介绍:
This journal aims to convey scientific and clinical progress in the field of prosthodontics and its related areas to many dental communities concerned with esthetic and functional restorations, occlusion, implants, prostheses, and biomaterials related to prosthodontics.
This journal publishes
• Original research data of high scientific merit in the field of diagnosis, function, esthetics and stomatognathic physiology related to prosthodontic rehabilitation, physiology and mechanics of occlusion, mechanical and biologic aspects of prosthodontic materials including dental implants.
• Review articles by experts on controversies and new developments in prosthodontics.
• Case reports if they provide or document new fundamental knowledge.