{"title":"Production of the Al–B master alloy by KBF4and B 2O3aluminothermic reduction in molten salt flux medium","authors":"A. Kataev, O. Tkacheva, N. Molchanova, Y. Zaikov","doi":"10.17073/0021-3438-2019-3-20-29","DOIUrl":null,"url":null,"abstract":"The study covers the process of obtaining the Al–B master alloy by the KBF4and B2O3aluminothermic reduction using KF–AlF3and KF–NaF–AlF3fluoride fluxes at 983 and 1123 К, respectively, and KCl–NaCl–KF chloride-fluoride fluxes at Т= 1173÷1223 К. All experiments were carried out under the same conditions: molten mixture stirring rate was 400 rpm, synthesis duration was 30min. The maximum amount of boron (1,5 %) in the Al–B alloy was obtained when using KBF4(3 % per B) as a boron-containing raw material in the KF–AlF3medium with a molar (cryolite) ratio (CR) of KF/AlF3equal to 1,3, atТ= 983 К, while boron recovery ratio did not exceed 75 %. Comparable results were obtained in experiments with KF–NaF–AlF3f lux (CR = 1,5) at Т= 1123 К. However, with the increased concentration of fed boron its recovery ratio decreased substantially. It is connected with the higher decomposition temperature of not only KBF4, but also less thermally stable NaBF4 formed as a result of exchange reaction in the melt. Therefore it is not recommended to use sodium salts as a f lux component. The Al–B master alloys obtained by KBF4reduction in fluoride fluxes were solid solutions of B in Al containing the AlB2intermetallic compound. The lowest amount of boron in aluminum with the minimum degree of extraction was obtained in experiments with the B2O3in molten KF–AlF3with CR = 1,5. Nevertheless, the results of scanning electron microscopy indicate a uniform distribution of B over the Al matrix and the absence of intermetallic compounds, while a large amount of Al2O3was found, which is the product of B2O3reactions with both liquid Al and KF–AlF3flux.","PeriodicalId":14523,"journal":{"name":"Izvestiya Vuzov Tsvetnaya Metallurgiya (Proceedings of Higher Schools Nonferrous Metallurgy","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2019-06-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Izvestiya Vuzov Tsvetnaya Metallurgiya (Proceedings of Higher Schools Nonferrous Metallurgy","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17073/0021-3438-2019-3-20-29","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The study covers the process of obtaining the Al–B master alloy by the KBF4and B2O3aluminothermic reduction using KF–AlF3and KF–NaF–AlF3fluoride fluxes at 983 and 1123 К, respectively, and KCl–NaCl–KF chloride-fluoride fluxes at Т= 1173÷1223 К. All experiments were carried out under the same conditions: molten mixture stirring rate was 400 rpm, synthesis duration was 30min. The maximum amount of boron (1,5 %) in the Al–B alloy was obtained when using KBF4(3 % per B) as a boron-containing raw material in the KF–AlF3medium with a molar (cryolite) ratio (CR) of KF/AlF3equal to 1,3, atТ= 983 К, while boron recovery ratio did not exceed 75 %. Comparable results were obtained in experiments with KF–NaF–AlF3f lux (CR = 1,5) at Т= 1123 К. However, with the increased concentration of fed boron its recovery ratio decreased substantially. It is connected with the higher decomposition temperature of not only KBF4, but also less thermally stable NaBF4 formed as a result of exchange reaction in the melt. Therefore it is not recommended to use sodium salts as a f lux component. The Al–B master alloys obtained by KBF4reduction in fluoride fluxes were solid solutions of B in Al containing the AlB2intermetallic compound. The lowest amount of boron in aluminum with the minimum degree of extraction was obtained in experiments with the B2O3in molten KF–AlF3with CR = 1,5. Nevertheless, the results of scanning electron microscopy indicate a uniform distribution of B over the Al matrix and the absence of intermetallic compounds, while a large amount of Al2O3was found, which is the product of B2O3reactions with both liquid Al and KF–AlF3flux.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
用kbf4和b2o3铝在熔盐助熔剂介质中热还原法制备Al-B中间合金
采用kf - alf3和kf - naf - alf3氟化剂分别为983和1123 К, KCl-NaCl-KF氯化物氟化剂为Т= 1173÷1223 К,采用kbf4和b2o3铝热还原法制备Al-B中间合金。所有实验均在相同条件下进行:熔融混合物搅拌速度为400 rpm,合成时间为30min。在KF - alf3介质中,当KF/ alf3的摩尔(冰晶石)比(CR) = 1,3, atТ= 983 К时,以KBF4(3% / B)为含硼原料,可获得Al-B合金中硼的最大含量(1.5%),而硼的回收率不超过75%。在Т= 1123 К时,KF-NaF-AlF3f通量(CR = 1,5)的实验也得到了类似的结果。但随着投料硼浓度的增加,其回收率明显下降。这不仅与KBF4的分解温度较高有关,而且与熔体中交换反应形成的热稳定性较差的NaBF4有关。因此不建议使用钠盐作为助流剂。在氟化物助熔剂中kbf4还原制得的Al - B中间合金是含alb2金属间化合物的B在Al中的固溶体。在CR = 1,5的kf - alf3熔体中加入b2o_3时,铝中硼含量最低,萃取度最小。然而,扫描电子显微镜的结果表明,B在Al基体上分布均匀,没有金属间化合物,而发现了大量的al2o3,这是b2o3与液体Al和kf - alf3通量反应的产物。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
ML5 alloy structure and properties at different modification methods Structure and properties of coarse-grained WC-Со hard metals with extra homogeneous microstructure Production of silumins using silicon production waste Al-Ca-M-La-Fe in-situ aluminum-matrix eutectic composites High-temperature ion nitriding of T15K6 indexable carbide inserts
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1