{"title":"Electrolytic Ni-Pb-P alloys","authors":"J. Bieliński,&nbsp;A. Bielińska","doi":"10.1016/0376-4583(85)90072-X","DOIUrl":null,"url":null,"abstract":"<div><p>The conditions required for obtaining electrolytic Ni-Pb-P alloy layers were investigated. Alkaline citrate-ammonia solutions typical of those used in electroless nickel plating containing less than 10 mM lead(II) were used. The electrolysis of these solutions at temperatures of 25–85 °C and current densities of 25–400 A m<sup>-2</sup> produced smooth Ni-Pb-P films containing 4–50 wt.% Pb and 2–8 wt.% P. The films containing 5–8 wt.% and 2–4 wt.% P were very bright and exhibited good corrosion resistance.</p><p>Investigations of the effect of changes in the concentration of the solution components and in other Ni-Pb-P deposition parameters showed that lead was deposited preferentially. Under these conditions the cathodic deposition of lead was diffusion controlled. The lead(II) inhibited the partial deposition of nickel and phosphorus. The efficiency of the current depended strongly on the deposition temperature and varied from 30% to 50% at 25 °C and from 100% to 150% at 75 °C. These results proved that the contribution of electroless nickel and phosphorus deposition increased with increasing temperature. Electroless nickel and phosphorus deposition at the cathode in the presence of such strong inhibitors as lead(II) salts proved that a continuous renewal of the catalyst surface, <em>i.e.</em> metallic nickel, was the most important factor in simultaneous electroless processes.</p></div>","PeriodicalId":22037,"journal":{"name":"Surface Technology","volume":"24 3","pages":"Pages 219-231"},"PeriodicalIF":0.0000,"publicationDate":"1985-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1016/0376-4583(85)90072-X","citationCount":"6","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Surface Technology","FirstCategoryId":"1087","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/037645838590072X","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 6

Abstract

The conditions required for obtaining electrolytic Ni-Pb-P alloy layers were investigated. Alkaline citrate-ammonia solutions typical of those used in electroless nickel plating containing less than 10 mM lead(II) were used. The electrolysis of these solutions at temperatures of 25–85 °C and current densities of 25–400 A m-2 produced smooth Ni-Pb-P films containing 4–50 wt.% Pb and 2–8 wt.% P. The films containing 5–8 wt.% and 2–4 wt.% P were very bright and exhibited good corrosion resistance.

Investigations of the effect of changes in the concentration of the solution components and in other Ni-Pb-P deposition parameters showed that lead was deposited preferentially. Under these conditions the cathodic deposition of lead was diffusion controlled. The lead(II) inhibited the partial deposition of nickel and phosphorus. The efficiency of the current depended strongly on the deposition temperature and varied from 30% to 50% at 25 °C and from 100% to 150% at 75 °C. These results proved that the contribution of electroless nickel and phosphorus deposition increased with increasing temperature. Electroless nickel and phosphorus deposition at the cathode in the presence of such strong inhibitors as lead(II) salts proved that a continuous renewal of the catalyst surface, i.e. metallic nickel, was the most important factor in simultaneous electroless processes.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
电解Ni-Pb-P合金
研究了电解Ni-Pb-P合金层的制备条件。碱性柠檬酸盐-氨溶液是化学镀镍中典型的含有小于10毫米铅(II)的溶液。在25 ~ 85℃的温度和25 ~ 400 A m-2的电流密度下电解这些溶液,得到光滑的Ni-Pb-P薄膜,其中Pb含量为4 ~ 50 wt.%, P含量为2 ~ 8 wt.%, P含量为5 ~ 8 wt.%, P含量为2 ~ 4 wt.%,薄膜非常光亮,具有良好的耐腐蚀性。对溶液组分浓度和其他Ni-Pb-P沉积参数的影响研究表明,铅优先沉积。在此条件下,铅的阴极沉积受到扩散控制。铅(II)抑制镍和磷的部分沉积。电流的效率很大程度上取决于沉积温度,在25°C时为30% ~ 50%,在75°C时为100% ~ 150%。结果表明,随着温度的升高,化学镀镍和化学镀磷的贡献增大。在铅(II)盐等强抑制剂存在的情况下,阴极上的化学镍和磷沉积证明,催化剂表面(即金属镍)的不断更新是同时化学过程中最重要的因素。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Subject index Author index Electrochemical aspects of steel corrosion in sea water The impedance of the porous cadmium electrode in alkali Sorption-desorption studies on alumina pretreated with acids: I. The anionic dye orange II
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1