Vapour-phase conversion of methyl lactate into lactide over TiO2/SiO2 catalyst at the lowered pressure

А.М. Vаrvarin, S. Levytska, А.М. Mylin, V. Brei
{"title":"Vapour-phase conversion of methyl lactate into lactide over TiO2/SiO2 catalyst at the lowered pressure","authors":"А.М. Vаrvarin, S. Levytska, А.М. Mylin, V. Brei","doi":"10.15407/kataliz2020.30.038","DOIUrl":null,"url":null,"abstract":"Now polylactide (PLA) widely use as biodestructive packing material. Usually monomeric lactide produce from lactic acid. Also, methyl (ethyl) lactate could be used for lactide obtaining via its vapour-phase condensation on TiO2/SiO2 catalyst at 2600C in N2 carrier-gas flow. However, at that it is necessary to heat carrier-gas to the reaction temperature. In this communication the results on methyl lactate vapour condensation into lactide with the lowered pressure of 100-150 mbar, without carrier-gas, are presented. Supported TiO2/SiO2 catalyst with 5 wt.% titania content has been prepared by impregnation of silica with Ti(OC4H9)4. After calcination at 5000C prepared catalyst has amorphous mesoporous structure with 335 m2/g surface area and 0.83 сm3/g pore volume. The catalytic experiments were performed in such way. Liquid methyl lactate was dosed into the evaporator (2500C) and further in the flowing reactor (2600C) under pressure of 100 mbar that produced by vacuum pump. Load on a catalyst was varied from 25 to 55 mmol ML/(gcath). Cooled product was analyzed on Agilent 7820A chromatograph and NMR Bruker Avance-400 spectrometer. It was shown that TiO2/SiO2 catalyst provide 74% selectivity towards lactide at 50-53% methyl lactate conversion with lactide productivity of 7.8 mmol L/(gcath) at 2600C/100 mbar. The catalyst stable work is more 80 h. Main impurities are methyl lactoillactate, 1-methoxyethanol and 1,1-dimethoxyethane.","PeriodicalId":9649,"journal":{"name":"Catalysis and Petrochemistry","volume":"13 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Catalysis and Petrochemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15407/kataliz2020.30.038","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

Now polylactide (PLA) widely use as biodestructive packing material. Usually monomeric lactide produce from lactic acid. Also, methyl (ethyl) lactate could be used for lactide obtaining via its vapour-phase condensation on TiO2/SiO2 catalyst at 2600C in N2 carrier-gas flow. However, at that it is necessary to heat carrier-gas to the reaction temperature. In this communication the results on methyl lactate vapour condensation into lactide with the lowered pressure of 100-150 mbar, without carrier-gas, are presented. Supported TiO2/SiO2 catalyst with 5 wt.% titania content has been prepared by impregnation of silica with Ti(OC4H9)4. After calcination at 5000C prepared catalyst has amorphous mesoporous structure with 335 m2/g surface area and 0.83 сm3/g pore volume. The catalytic experiments were performed in such way. Liquid methyl lactate was dosed into the evaporator (2500C) and further in the flowing reactor (2600C) under pressure of 100 mbar that produced by vacuum pump. Load on a catalyst was varied from 25 to 55 mmol ML/(gcath). Cooled product was analyzed on Agilent 7820A chromatograph and NMR Bruker Avance-400 spectrometer. It was shown that TiO2/SiO2 catalyst provide 74% selectivity towards lactide at 50-53% methyl lactate conversion with lactide productivity of 7.8 mmol L/(gcath) at 2600C/100 mbar. The catalyst stable work is more 80 h. Main impurities are methyl lactoillactate, 1-methoxyethanol and 1,1-dimethoxyethane.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
在TiO2/SiO2催化下乳酸甲酯气相转化为丙交酯
聚乳酸(PLA)作为生物破坏性包装材料得到了广泛的应用。通常由乳酸产生单体丙交酯。乳酸甲酯(乙基)在TiO2/SiO2催化剂上气相冷凝,温度为2600C,载气为N2,可制备丙交酯。然而,此时必须将载气加热到反应温度。本文介绍了在无载气条件下,在100-150毫巴的低压条件下,乳酸甲酯蒸汽缩合成丙交酯的结果。用Ti(OC4H9)4浸渍二氧化硅制备了钛含量为5 wt.%的负载型TiO2/SiO2催化剂。经5000C煅烧制备的催化剂具有无定形介孔结构,比表面积为335 m2/g,孔体积为0.83 m3/g。用这种方法进行了催化实验。将乳酸甲酯液体加入蒸发器(2500C)中,并在真空泵产生的100mbar压力下进入流动反应器(2600C)。催化剂负载在25 ~ 55 mmol ML/(gcath)之间变化。冷却后的产物在Agilent 7820A色谱仪和Bruker Avance-400核磁共振光谱仪上进行分析。结果表明,在50-53%的乳酸甲酯转化率下,TiO2/SiO2催化剂对丙交酯的选择性为74%,在2600C/100 mbar条件下,丙交酯的产率为7.8 mmol L/(gcath)。催化剂稳定工作80 h以上,主要杂质为乳乳酸甲酯、1-甲氧基乙醇和1,1-二甲氧基乙烷。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
The kinetic model of the combined heterogeneously catalyzed condensation and esterification of propionic acid and methyl propionate with formaldehyde and methanol Development of catalysts for the synthesis of higher hydrocarbons from carbon dioxide The pathways of the phthalic anhydride selectivity and yield increase at C4-C5-hydrocarbons oxidation Acid transesterification of oils with ethanol on carbon catalysts To the question of oxidation on the surface of oxides: temperature- programmed oxidation of cyclohexanol
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1