{"title":"A Comparison between the Effect of Heat Treatment and Plasma on the Wear Activities and Corrosion Resistance of Ni-B Electroless Coating with AISI 4340 Steel","authors":"Abdul Raheem K. Abid Ali, A. M. Wais","doi":"10.53523/ijoirvol9i2id167","DOIUrl":null,"url":null,"abstract":"The study the hardness, wear corrosion resistance of as-coating, heat treatment and plasma-nitriding of Ni- B electroless coatings was deposit on 4340 steel. After the procees of coating, samples were plasma-nitriding in percentage hydrogen/nitrogen ratio (50%), in the temperature 400°C, at 4 hours were compared with heat treatment. characterization by of FESEM, XRD, microhardness, Corrosion Resistance and surface roughness measurements. Microhardness was show highest hardness of 1050 HV was obtained for Ni-B plasma-nitriding formula whereas the greatest hardness of 800 HV was become for sample of Ni-B heat treated. Ni-B coating is used in the enhancement of properties of the corrosion of AISI 4340 steel is due to the thickness of electroless deposition, which is uniform, and the cold of Ni-B coating to act as an active barrier between corrosion media and metal, it should be noted that the value of Ecorr is less negative and the rate of corrosion and Icorr is lower on the plated sample than on the uncoated sample. The rate of the wear for samples is decrement by plasma-nitriding with deposition time at (4h) and the temperature 400°C. Rate of wear for the materials depends not just into condition of wear test, but also with several properties of material and features as topography, hardness and friction coefficient.","PeriodicalId":14665,"journal":{"name":"Iraqi Journal of Industrial Research","volume":"20 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-10-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Iraqi Journal of Industrial Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.53523/ijoirvol9i2id167","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The study the hardness, wear corrosion resistance of as-coating, heat treatment and plasma-nitriding of Ni- B electroless coatings was deposit on 4340 steel. After the procees of coating, samples were plasma-nitriding in percentage hydrogen/nitrogen ratio (50%), in the temperature 400°C, at 4 hours were compared with heat treatment. characterization by of FESEM, XRD, microhardness, Corrosion Resistance and surface roughness measurements. Microhardness was show highest hardness of 1050 HV was obtained for Ni-B plasma-nitriding formula whereas the greatest hardness of 800 HV was become for sample of Ni-B heat treated. Ni-B coating is used in the enhancement of properties of the corrosion of AISI 4340 steel is due to the thickness of electroless deposition, which is uniform, and the cold of Ni-B coating to act as an active barrier between corrosion media and metal, it should be noted that the value of Ecorr is less negative and the rate of corrosion and Icorr is lower on the plated sample than on the uncoated sample. The rate of the wear for samples is decrement by plasma-nitriding with deposition time at (4h) and the temperature 400°C. Rate of wear for the materials depends not just into condition of wear test, but also with several properties of material and features as topography, hardness and friction coefficient.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
热处理和等离子体对AISI 4340钢Ni-B化学涂层磨损性能和耐蚀性影响的比较
研究了4340钢表面Ni- B化学镀层的硬度、耐磨性、热处理和等离子渗氮性能。涂层工艺完成后,样品以氢氮比(50%)等离子体渗氮,在温度400℃下,4小时后与热处理进行比较。通过FESEM, XRD,显微硬度,耐蚀性和表面粗糙度测试进行表征。显微硬度表明,Ni-B等离子体渗氮配方硬度最高,为1050 HV, Ni-B热处理样品硬度最高,为800 HV。Ni-B涂层用于提高AISI 4340钢的腐蚀性能是由于化学沉积的厚度均匀,并且Ni-B涂层的冷态在腐蚀介质与金属之间起到了活性屏障的作用,应该注意的是,镀后样品的Ecorr值小于负,腐蚀速率和Icorr低于未涂覆样品。随着沉积时间(4h)和温度(400℃)的增加,样品的磨损率逐渐降低。材料的磨损率不仅取决于磨损试验条件,还与材料的形貌、硬度和摩擦系数等性能和特征有关。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Impact of Different Organic Extracts on Growth and Yield of Chili Pepper (Capsicum frutescens L.) VLSI Synthesis for Low-Power Clocking in Synchronous Designs Ferritin Levels as Indicators of Severity and Mortality in COVID-19 Patients from Tripoli, Libya Recycling Discharged Treated Wastewater from Dairy Factories for Industrial and Irrigation Purposes Efficient Ammonium Ion Removal from the State Company of Fertilizers Wastewater through Nano Zeolite Treatment
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1