{"title":"INFLUENCE OF ELECTROLYTE COMPOSITION AND OVERHEATING ON THE SIDELEDGE IN THE ALUMINUM CELL","authors":"V. Stakhanov, A. Redkin, Y. Zaikov, A. Galashev","doi":"10.17073/0021-3438-2018-4-24-30","DOIUrl":null,"url":null,"abstract":"The paper presents a theoretical study conducted to investigate the effect that the chemical composition of electrolyte and its overheating have on the size of sideledge formed in an aluminum smelting bath. Three electrolyte compositions were chosen: (1) sodium cryolite with the cryolite ratio CR = 2,7; (2) cryolite CR = 2,7 + 5 wt.% CaF2; (3) cryolite CR = 2,7 + 5 wt.% CaF2 + 5 wt.% Al2О3. The electrolyte liquidus overheating temperatures were 5, 10, 15 and 20 °C. Calculations were performed using the finite element method. A simplified design of an aluminum cell was used with a prebaked anode. The temperature field was calculated using a mathematical model based on the Boussinesq approximation, which contains the Navier–Stokes equation as well as thermal conductivity and incompressibility equations. The key role of electrolyte overheating in sideledge formation was established. The resulting sideledge profile depends on the heat transfer coefficients and thermophysical properties of materials. The smallest sideledge thickness with the same electrolyte overheating was observed in cryolite composition 3, and the profiles of the formed sideledge for samples 1 and 2 were nearly the same. The thickness of the sideledge formed with a 5 degree overheating exceeded 7 cm and the difference in temperature between the sideledge in contact with electrolyte and the side block wall was 20–25 degrees. It was found that the virtually total disappearance of the sideledge occurs at electrolyte liquidus overheating by 20 degrees.","PeriodicalId":14523,"journal":{"name":"Izvestiya Vuzov Tsvetnaya Metallurgiya (Proceedings of Higher Schools Nonferrous Metallurgy","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2018-08-16","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Izvestiya Vuzov Tsvetnaya Metallurgiya (Proceedings of Higher Schools Nonferrous Metallurgy","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17073/0021-3438-2018-4-24-30","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

The paper presents a theoretical study conducted to investigate the effect that the chemical composition of electrolyte and its overheating have on the size of sideledge formed in an aluminum smelting bath. Three electrolyte compositions were chosen: (1) sodium cryolite with the cryolite ratio CR = 2,7; (2) cryolite CR = 2,7 + 5 wt.% CaF2; (3) cryolite CR = 2,7 + 5 wt.% CaF2 + 5 wt.% Al2О3. The electrolyte liquidus overheating temperatures were 5, 10, 15 and 20 °C. Calculations were performed using the finite element method. A simplified design of an aluminum cell was used with a prebaked anode. The temperature field was calculated using a mathematical model based on the Boussinesq approximation, which contains the Navier–Stokes equation as well as thermal conductivity and incompressibility equations. The key role of electrolyte overheating in sideledge formation was established. The resulting sideledge profile depends on the heat transfer coefficients and thermophysical properties of materials. The smallest sideledge thickness with the same electrolyte overheating was observed in cryolite composition 3, and the profiles of the formed sideledge for samples 1 and 2 were nearly the same. The thickness of the sideledge formed with a 5 degree overheating exceeded 7 cm and the difference in temperature between the sideledge in contact with electrolyte and the side block wall was 20–25 degrees. It was found that the virtually total disappearance of the sideledge occurs at electrolyte liquidus overheating by 20 degrees.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
电解液成分和过热对铝电池侧壁的影响
本文从理论上研究了电解液的化学成分及其过热对铝熔炼槽中侧边尺寸的影响。选择三种电解质组成:(1)冰晶石钠,冰晶石比CR = 2,7;(2)冰晶石CR = 2,7 + 5 wt.% CaF2;(3)冰晶石CR = 2,7 + 5 wt.% CaF2 + 5 wt.% Al2О3。电解液过热温度分别为5、10、15和20℃。采用有限元法进行了计算。采用了一种简化的铝电解槽设计和预焙阳极。温度场的计算采用了基于Boussinesq近似的数学模型,该模型包含了Navier-Stokes方程、导热系数方程和不可压缩性方程。确定了电解液过热在侧边形成中的关键作用。得到的侧边轮廓取决于材料的传热系数和热物理性质。在相同的电解质过热条件下,冰晶石组成3的侧边厚度最小,样品1和样品2形成的侧边轮廓几乎相同。过热5度形成的侧边厚度超过7cm,与电解液接触的侧边与侧块壁的温差为20-25度。研究发现,在电解液过热20度时,侧边几乎完全消失。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
ML5 alloy structure and properties at different modification methods Structure and properties of coarse-grained WC-Со hard metals with extra homogeneous microstructure Production of silumins using silicon production waste Al-Ca-M-La-Fe in-situ aluminum-matrix eutectic composites High-temperature ion nitriding of T15K6 indexable carbide inserts
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1