Effect of W addition on compressive strength of Nb-10Mo-10Ti-18Si-base in-situ composites

J. Sha, H. Hirai, T. Tabaru, A. Kitahara, Hidetoshi Ueno, S. Hanada
{"title":"Effect of W addition on compressive strength of Nb-10Mo-10Ti-18Si-base in-situ composites","authors":"J. Sha, H. Hirai, T. Tabaru, A. Kitahara, Hidetoshi Ueno, S. Hanada","doi":"10.2320/MATERTRANS1989.41.1125","DOIUrl":null,"url":null,"abstract":"Niobium solid solution/niobium silicides in-situ composites are expected to have applications in the future as high-temperature structural materials. To improve the high temperature strength further, we tried to add tungsten to Nb-10Mo-10Ti-18Si eutectic alloy by replacing Nb with 0, 5, 10 and 15 mol%W, The samples were prepared by arc casting and some of them were directionally solidified by the floating zone melting technique at a growth rate of 15 mm/h, After annealing at 1870 K for 100h, the microstructure, Vickers hardness and high-temperature compressive strength were examined. The samples without W consisted of eutectic Nb solid solution and (Nb, Mo, Ti) 5 Si 3 silicide, while primary Nb solid solution appeared as a result of substituting W for Nb. The microstructure of directionally solidified samples was coarse and oriented in the direction of growth, but they did not show the typical microstructure often observed in the case of directionally solidified materials. The Vickers hardness increased with increasing W content. The 0.2% yield strength (σ 0.2 ) and the specific 0.2% yield strength (σ 0.25 ) (σ 0.2 divided by the density) at 1670 K increased markedly with increasing W content. The directionally solidified samples showed higher σ 0.2 and σ 0.2S than the arc-cast samples. Even at 1770 K, the directionally solidified sample with 15 mol% W showed σ 0.2 of about 650 MPa.","PeriodicalId":18264,"journal":{"name":"Materials Transactions Jim","volume":"17 1","pages":"1125-1128"},"PeriodicalIF":0.0000,"publicationDate":"2000-09-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"13","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Transactions Jim","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2320/MATERTRANS1989.41.1125","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 13

Abstract

Niobium solid solution/niobium silicides in-situ composites are expected to have applications in the future as high-temperature structural materials. To improve the high temperature strength further, we tried to add tungsten to Nb-10Mo-10Ti-18Si eutectic alloy by replacing Nb with 0, 5, 10 and 15 mol%W, The samples were prepared by arc casting and some of them were directionally solidified by the floating zone melting technique at a growth rate of 15 mm/h, After annealing at 1870 K for 100h, the microstructure, Vickers hardness and high-temperature compressive strength were examined. The samples without W consisted of eutectic Nb solid solution and (Nb, Mo, Ti) 5 Si 3 silicide, while primary Nb solid solution appeared as a result of substituting W for Nb. The microstructure of directionally solidified samples was coarse and oriented in the direction of growth, but they did not show the typical microstructure often observed in the case of directionally solidified materials. The Vickers hardness increased with increasing W content. The 0.2% yield strength (σ 0.2 ) and the specific 0.2% yield strength (σ 0.25 ) (σ 0.2 divided by the density) at 1670 K increased markedly with increasing W content. The directionally solidified samples showed higher σ 0.2 and σ 0.2S than the arc-cast samples. Even at 1770 K, the directionally solidified sample with 15 mol% W showed σ 0.2 of about 650 MPa.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
添加W对nb - 10mo - 10ti - 18si基原位复合材料抗压强度的影响
铌固溶体/硅化铌原位复合材料作为高温结构材料具有广阔的应用前景。为进一步提高Nb- 10mo - 10ti - 18si共晶合金的高温强度,尝试用0、5、10、15 mol%W代替Nb加入钨,采用电弧铸造法制备试样,部分试样采用浮区熔融定向凝固,生长速率为15 mm/h, 1870 K退火100h后,对试样的显微组织、维氏硬度和高温抗压强度进行了检测。不含W的样品由共晶Nb固溶体和(Nb, Mo, Ti) 5si3硅化物组成,以W代替Nb形成初生Nb固溶体。定向凝固试样的显微组织较粗,且在生长方向上有取向,但没有表现出定向凝固材料的典型显微组织。随着W含量的增加,合金的维氏硬度逐渐升高。随着W含量的增加,合金在1670 K时的0.2%屈服强度(σ 0.2)和比0.2%屈服强度(σ 0.25) (σ 0.2除以密度)显著提高。定向凝固试样的σ 0.2和σ 0.2 s均高于弧铸试样。即使在1770 K时,15 mol% W的定向凝固试样在650 MPa左右的σ 0.2。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Solid state diffusion bonding of silicon nitride using vanadium foils : Structural and functional control of materials through solid-solid phase transformations in high magnetic field Characteristics of paramagnetic and diamagnetic anisotropy which induce magnetic alignment of micron-sized non-ferromagnetic particles : Structural and functional control of materials through solid-solid phase transformations in high magnetic field Combination of triboelectrostatic separation and air tabling for sorting plastics from a multi-component plastic mixture : New systems and processes in recycling and high performance waste treatments Impurity removal from carbon saturated liquid iron using lead solvent : New systems and processes in recycling and high performance waste treatments Surface treatment of magnesium alloys by artificial corrosion-oxidization method : Special issue on platform science and technology for advanced magnesium alloys, II
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1