Effect of Illite Clay Additive on Sintering, Phase Composition and Properties of Mullite-ZrO2 Ceramics / Illītu mālu piedevas ietekme uz mullīta-ZrO2 keramikas saķepšanu, fāžu sastāvu un īpašībām.

G. Sedmale, Inga Raubiska, A. Krumina, A. Hmelov
{"title":"Effect of Illite Clay Additive on Sintering, Phase Composition and Properties of Mullite-ZrO2 Ceramics / Illītu mālu piedevas ietekme uz mullīta-ZrO2 keramikas saķepšanu, fāžu sastāvu un īpašībām.","authors":"G. Sedmale, Inga Raubiska, A. Krumina, A. Hmelov","doi":"10.1515/msac-2015-0004","DOIUrl":null,"url":null,"abstract":"Abstract This study focuses on the influence of illite clay on changes of ZrO2 modifications after sintering and consolidation of mullite-ZrO2 ceramics with or without Y2O3 additive. It was found that mullite-ZrO2 ceramics both with 4.5 % Y2O3 additive or without it in presence of illite clay tend to have increased densification and compression strength after sintering. Presence of illite clay also promotes change of ZrO2 monoclinic phase to tetragonal phase and the presence of Y2O3 promotes change to ZrO2 cubic phase. Mullīts ir viena no svarīgākajām augsttemperatūras kristāliskajām fāzēm. Mullīta veidošanās keramikā, tajā skaitā arī keramikā, kas satur ZrO2, nodrošina tai augstas mehāniskās, ķīmiskās un termiskās īpašības, arī pie paaugstinātām temperatūrām. Lai gan mullīta fāze sāk veidoties jau ~ 1000 °C temperatūrā, blīvu mullīta keramikas materiālu parasti iegūst viena cikla saķepināšanas procesā pie paaugstinātas temperatūras (≥ 1400 °C). Lai veicinātu šīs keramikas saķepšanu un saķepšanas temperatūras pazemināšanu, pielieto piedevas vai arī aktīvus pulverus, piemēram, γ-Al2O3 nanopulveri, kvarca smiltis, u.c. Dotajā darbā ir pētīta illīta nanopulvera ietekme uz mullīta-ZrO2 keramikas (ar Y2O3 piedevu un bez tās) sablīvēšanos saķepšanas procesā, iegūtā keramikas materiāla kristālisko fāžu sastāvu un īpašībām. Darbā ir pielietoti divu veidu pulveru maisījumi, kas sastāv no γ-Al2O3, SiO2, ZrO2 (monoklīns), ar Y2O3 piedevu vai bez tās. Katrai maisījumu grupai pievienots illīts 5 %, 10 % vai 15 % (masas daļas). Izejas pulveru morfoloģijas izpētei pielietots elektronmikroskops Hitachi-TM3000 un diferenciāli termiskai analīzes iekārta Setaram, Setsys Evolution 1750. Paraugi formēti disku un cilindru veidā. Saķepināšana veikta divās maksimālajās temperatūrās - 1400 °C vai 1500 °C. Keramikas fāžu sastāvs noteikts pielietojot Rentgena staru difraktometriju (D8 Advance Bruker). Raksturīgās keramikas īpašības (relatīvais blīvums, sarukums) noteiktas izmantojot EN, spiedes izturība noteikta pielietojot iekārtu Toni-Technic. Ir iegūti rezultāti, kas parāda, ka saķepināto keramikas paraugu sablīvēšanās (relatīvais blīvums un sarukums) pakāpe pieaug ar illīta mālu piedevu līdz 10%. Pie lielākas piedevas (15 %) ir vērojama iekšējo poru veidošanās tendece. Savukārt Y2O3 piedeva, it sevišķi illītu mālu klātienē veicina sablīvēšanos saķepināšanas procesā, it seviķi pie 1500 ºC. Ir jāatzīmē arī, ka mālu klātiene veicina ZrO2 monoklīnās modifikācijas transformāciju tetragonālā, bet vienlaicīga mālu un Y2O3 piedevu klātiene savukārt ZrO2 monoklīno modifikāciju tranformē kubiskā modifikācijā.","PeriodicalId":18239,"journal":{"name":"Materials Science and Applied Chemistry","volume":"10 1","pages":"23 - 26"},"PeriodicalIF":0.0000,"publicationDate":"2015-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science and Applied Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1515/msac-2015-0004","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

Abstract This study focuses on the influence of illite clay on changes of ZrO2 modifications after sintering and consolidation of mullite-ZrO2 ceramics with or without Y2O3 additive. It was found that mullite-ZrO2 ceramics both with 4.5 % Y2O3 additive or without it in presence of illite clay tend to have increased densification and compression strength after sintering. Presence of illite clay also promotes change of ZrO2 monoclinic phase to tetragonal phase and the presence of Y2O3 promotes change to ZrO2 cubic phase. Mullīts ir viena no svarīgākajām augsttemperatūras kristāliskajām fāzēm. Mullīta veidošanās keramikā, tajā skaitā arī keramikā, kas satur ZrO2, nodrošina tai augstas mehāniskās, ķīmiskās un termiskās īpašības, arī pie paaugstinātām temperatūrām. Lai gan mullīta fāze sāk veidoties jau ~ 1000 °C temperatūrā, blīvu mullīta keramikas materiālu parasti iegūst viena cikla saķepināšanas procesā pie paaugstinātas temperatūras (≥ 1400 °C). Lai veicinātu šīs keramikas saķepšanu un saķepšanas temperatūras pazemināšanu, pielieto piedevas vai arī aktīvus pulverus, piemēram, γ-Al2O3 nanopulveri, kvarca smiltis, u.c. Dotajā darbā ir pētīta illīta nanopulvera ietekme uz mullīta-ZrO2 keramikas (ar Y2O3 piedevu un bez tās) sablīvēšanos saķepšanas procesā, iegūtā keramikas materiāla kristālisko fāžu sastāvu un īpašībām. Darbā ir pielietoti divu veidu pulveru maisījumi, kas sastāv no γ-Al2O3, SiO2, ZrO2 (monoklīns), ar Y2O3 piedevu vai bez tās. Katrai maisījumu grupai pievienots illīts 5 %, 10 % vai 15 % (masas daļas). Izejas pulveru morfoloģijas izpētei pielietots elektronmikroskops Hitachi-TM3000 un diferenciāli termiskai analīzes iekārta Setaram, Setsys Evolution 1750. Paraugi formēti disku un cilindru veidā. Saķepināšana veikta divās maksimālajās temperatūrās - 1400 °C vai 1500 °C. Keramikas fāžu sastāvs noteikts pielietojot Rentgena staru difraktometriju (D8 Advance Bruker). Raksturīgās keramikas īpašības (relatīvais blīvums, sarukums) noteiktas izmantojot EN, spiedes izturība noteikta pielietojot iekārtu Toni-Technic. Ir iegūti rezultāti, kas parāda, ka saķepināto keramikas paraugu sablīvēšanās (relatīvais blīvums un sarukums) pakāpe pieaug ar illīta mālu piedevu līdz 10%. Pie lielākas piedevas (15 %) ir vērojama iekšējo poru veidošanās tendece. Savukārt Y2O3 piedeva, it sevišķi illītu mālu klātienē veicina sablīvēšanos saķepināšanas procesā, it seviķi pie 1500 ºC. Ir jāatzīmē arī, ka mālu klātiene veicina ZrO2 monoklīnās modifikācijas transformāciju tetragonālā, bet vienlaicīga mālu un Y2O3 piedevu klātiene savukārt ZrO2 monoklīno modifikāciju tranformē kubiskā modifikācijā.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Minerālo izejvielu pielietošanas un stikla šķiedras defektu izpēte Minerālo saistvielu pētījumi Silikātu materiālu institūtā Pašattīroši audumi: kas tie ir un kāpēc tādi nepieciešami? Mūrējumu korozija apkārtējās vides ietekmē Augsti poraina oksīdu keramika
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1