Recovery of hydrogen induced defects and thermal desorption of residual hydrogen in LaNi5 : Special issue on grain boundaries, interfaces, defects and localized quantum structures in ceramics

K. Sakaki, H. Araki, Y. Shirai
{"title":"Recovery of hydrogen induced defects and thermal desorption of residual hydrogen in LaNi5 : Special issue on grain boundaries, interfaces, defects and localized quantum structures in ceramics","authors":"K. Sakaki, H. Araki, Y. Shirai","doi":"10.2320/MATERTRANS.43.1494","DOIUrl":null,"url":null,"abstract":"Lattice defects induced by initial hydriding and their effect on residual hydrogen content in LaNi 5 have been studied by means of positron lifetime spectroscopy and hydrogen thermal desorption measurement. Component analyses of positron lifetime spectra show that surprising amount of vacancies together with dislocations are generated by the initial hydriding. Vacancy migration in LaNi 5 after hydrogen desorption at room temperature is observed around 423-673 K, while dislocations in LaNi 5 are much more stable. Hydrogen thermal desorption measurement shows that the release of residual hydrogen occurs mainly in the temperature range from 450 to 650 K, and it ceases at about 800 K. The release temperature of residual hydrogen closely corresponds with the temperature of vacancy migration and annihilation in LaNi 5 . Residual hydrogen in LaNi 5 is most likely trapped by vacancies and vacancy clusters, which are induced by hydriding.","PeriodicalId":18264,"journal":{"name":"Materials Transactions Jim","volume":"18 1","pages":"1494-1497"},"PeriodicalIF":0.0000,"publicationDate":"2002-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"20","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Transactions Jim","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2320/MATERTRANS.43.1494","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 20

Abstract

Lattice defects induced by initial hydriding and their effect on residual hydrogen content in LaNi 5 have been studied by means of positron lifetime spectroscopy and hydrogen thermal desorption measurement. Component analyses of positron lifetime spectra show that surprising amount of vacancies together with dislocations are generated by the initial hydriding. Vacancy migration in LaNi 5 after hydrogen desorption at room temperature is observed around 423-673 K, while dislocations in LaNi 5 are much more stable. Hydrogen thermal desorption measurement shows that the release of residual hydrogen occurs mainly in the temperature range from 450 to 650 K, and it ceases at about 800 K. The release temperature of residual hydrogen closely corresponds with the temperature of vacancy migration and annihilation in LaNi 5 . Residual hydrogen in LaNi 5 is most likely trapped by vacancies and vacancy clusters, which are induced by hydriding.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
LaNi5中氢致缺陷的恢复和残余氢的热解吸:陶瓷中的晶界、界面、缺陷和局域量子结构专刊
采用正电子寿命谱法和氢热脱附法研究了lani5中初始氢化引起的晶格缺陷及其对残余氢含量的影响。正电子寿命谱的成分分析表明,初始氢化产生了数量惊人的空位和位错。室温下,在423 ~ 673 K范围内,LaNi 5的空位迁移现象较为明显,而LaNi 5的位错更为稳定。氢热解吸测量表明,残余氢的释放主要发生在450 ~ 650 K温度范围内,在800 K左右停止。残余氢的释放温度与lani5中空位迁移和湮灭的温度密切相关。lani5中残留的氢很可能被氢化引起的空位和空位团簇所捕获。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Solid state diffusion bonding of silicon nitride using vanadium foils : Structural and functional control of materials through solid-solid phase transformations in high magnetic field Characteristics of paramagnetic and diamagnetic anisotropy which induce magnetic alignment of micron-sized non-ferromagnetic particles : Structural and functional control of materials through solid-solid phase transformations in high magnetic field Combination of triboelectrostatic separation and air tabling for sorting plastics from a multi-component plastic mixture : New systems and processes in recycling and high performance waste treatments Impurity removal from carbon saturated liquid iron using lead solvent : New systems and processes in recycling and high performance waste treatments Surface treatment of magnesium alloys by artificial corrosion-oxidization method : Special issue on platform science and technology for advanced magnesium alloys, II
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1