Recovery of Nickel and Cobalt from a Low Grade Laterite Ore

B. Altansukh, Kazutoshi Haga, A. Shibayama
{"title":"Recovery of Nickel and Cobalt from a Low Grade Laterite Ore","authors":"B. Altansukh, Kazutoshi Haga, A. Shibayama","doi":"10.4144/RPSJ.61.100","DOIUrl":null,"url":null,"abstract":"This study focused on the development of hydrometallurgical process which allows the nickel (Ni) and cobalt (Co) recovery from a low grade laterite ore. The developed process consists of two main stages: leaching and precipitation. In the first stage, an appropriate leach liquor which contains a relatively high nickel and cobalt concentration is prepared by chemical leaching and pressure leaching followed by separation steps, respectively. The effects of sulfuric acid concentration, leaching temperature and time, internal pressure in an autoclave on the efficient leaching of Ni and Co from a laterite ore were presented. In the next stage, the Ni and Co ions present in the liquor are co-precipitated as sulfides by sulfuration with sodium hydrosulfide (pH 3.8). It was found that talc (Mg 3 Si 4 O 10 (OH) 2 ), goethite (FeOOH) and quartz (SiO 2 ) are main minerals of the laterite ore which contains 48.12% Fe, 1.8% Al, 0.95% Ni, 0.07% Co, 0.29% Cr and 0.15% Mg. The high efficiency of pressure leaching for Ni and Co from the low grade laterite ore was re vealed by comparing the chemical leaching results. The vast majority of Co (>97%) and Ni (55%) from the purified liquor resulting after neutralization with calcium carbonate (CaCO 3 ) was precipitat- ed as mixed-sulfides by adjusting the NaHS/(Co + Ni) ratio to 3 by the addition of sulfuration agent (NaHS) at the solution pH of 3.8. Based on the experimental results, the efficient recovery of cobalt (Co) and nickel (Ni) from the low grade laterite ore can be achieved using the pressure leaching and neutralization treatment followed by sulfuration.","PeriodicalId":20971,"journal":{"name":"Resources Processing","volume":"29 1","pages":"100-109"},"PeriodicalIF":0.0000,"publicationDate":"2014-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Resources Processing","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4144/RPSJ.61.100","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

Abstract

This study focused on the development of hydrometallurgical process which allows the nickel (Ni) and cobalt (Co) recovery from a low grade laterite ore. The developed process consists of two main stages: leaching and precipitation. In the first stage, an appropriate leach liquor which contains a relatively high nickel and cobalt concentration is prepared by chemical leaching and pressure leaching followed by separation steps, respectively. The effects of sulfuric acid concentration, leaching temperature and time, internal pressure in an autoclave on the efficient leaching of Ni and Co from a laterite ore were presented. In the next stage, the Ni and Co ions present in the liquor are co-precipitated as sulfides by sulfuration with sodium hydrosulfide (pH 3.8). It was found that talc (Mg 3 Si 4 O 10 (OH) 2 ), goethite (FeOOH) and quartz (SiO 2 ) are main minerals of the laterite ore which contains 48.12% Fe, 1.8% Al, 0.95% Ni, 0.07% Co, 0.29% Cr and 0.15% Mg. The high efficiency of pressure leaching for Ni and Co from the low grade laterite ore was re vealed by comparing the chemical leaching results. The vast majority of Co (>97%) and Ni (55%) from the purified liquor resulting after neutralization with calcium carbonate (CaCO 3 ) was precipitat- ed as mixed-sulfides by adjusting the NaHS/(Co + Ni) ratio to 3 by the addition of sulfuration agent (NaHS) at the solution pH of 3.8. Based on the experimental results, the efficient recovery of cobalt (Co) and nickel (Ni) from the low grade laterite ore can be achieved using the pressure leaching and neutralization treatment followed by sulfuration.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
某低品位红土矿石中镍钴的回收
研究了一种低品位红土矿石湿法冶金工艺,该工艺主要包括浸出和沉淀两个阶段。在第一阶段,分别通过化学浸出和压力浸出制备含镍和钴浓度较高的合适浸出液,然后进行分离。研究了硫酸浓度、浸出温度和浸出时间、高压釜内压对红土矿石中镍和钴的有效浸出的影响。在下一阶段,存在于液中的Ni和Co离子通过与氢硫化钠(pH 3.8)的硫化作用以硫化物的形式共沉淀。结果表明,该红土矿石含铁48.12%、铝1.8%、镍0.95%、Co 0.07%、Cr 0.29%、Mg 0.15%,主要矿物为滑石(mg3si4o10 (OH) 2)、针铁矿(FeOOH)和石英(sio2)。通过对化学浸出结果的比较,揭示了压力浸出低品位红土中镍、钴的高效。在溶液pH为3.8的条件下,通过添加硫化剂(NaHS)调节NaHS/(Co + Ni)比为3,将碳酸钙(caco3)中和后的纯化液中绝大部分Co(>97%)和Ni(55%)析出为混合硫化物。试验结果表明,采用压力浸出中和后再进行硫化处理,可实现低品位红土矿石中钴(Co)和镍(Ni)的高效回收。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Optimum Design Using Genetic Algorithm and Discrete-element Method: Application to Vibration Feeder Design for E-waste Recycling Automation 画像認識技術による廃電子基板上製錬忌避素子/有価素子の自動検出 Effect of Impurities on Spinel Precipitation Behavior in Molten Fayalite Slag Study on Arsenic Methyltransferase of Cellulomonas sp. K31 Expressed in Recombinant E. coli Development of the Process for Concentrating Valuable Metals and Removing Smelting Repellent Components from Waste PCBs by Combining Roasting, Selective Comminution, and Physical Separation
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1