{"title":"Low loss microstructured polymer optical fibre (mPOF)","authors":"R. Lwin, A. Argyros, S. Leon-Saval, M. Large","doi":"10.1364/OFC.2011.OWS6","DOIUrl":null,"url":null,"abstract":"Using a high tension draw we produced a fibre with a loss of 0.16 dB/m at 650nm, making mPOF competitive for the first time with conventional POF. Annealing increases thermal stability.","PeriodicalId":6373,"journal":{"name":"2011 Optical Fiber Communication Conference and Exposition and the National Fiber Optic Engineers Conference","volume":"30 1","pages":"1-3"},"PeriodicalIF":0.0000,"publicationDate":"2011-03-06","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2011 Optical Fiber Communication Conference and Exposition and the National Fiber Optic Engineers Conference","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1364/OFC.2011.OWS6","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 6
Abstract
Using a high tension draw we produced a fibre with a loss of 0.16 dB/m at 650nm, making mPOF competitive for the first time with conventional POF. Annealing increases thermal stability.