{"title":"Hydrometallurgical Processing of the Wastes of Polymetallic Ore Dressing","authors":"A. Bulaev","doi":"10.18502/kms.v6i1.8067","DOIUrl":null,"url":null,"abstract":"The possibility of hydrometallurgical treatment of old flotation tailings to extract base and noble metals was investigated. Two samples of old flotation tailings samples containing 0.26% and 0.36% of copper, and 0.22% and 0.23% of zinc were the subjects of this study. Agitation and percolator leaching was performed with distilled water and sulfuric acid solutions (of 0.5 to 10% H2SO4). It was shown that under certain conditions (sulfuric acid concentration) it was possible to achieve selective leaching of non-ferrous metals and obtain solutions with relatively low concentrations of iron ions, which is necessary for further effective extraction of non-ferrous metal ions from the solution. The effect of acid leaching on further gold recovery from the first sample containing 0.7 g/t of gold by cyanidation was investigated. The sample of the tailings after leaching with a 1% sulfuric acid solution was leached with 10% sulfuric acid. After that, the tailings sample and the acid leach residues were subjected to sorption cyanidation. Two-stage acid leaching with 1 and 10% sulfuric acid provided the higher gold recovery than one-stage (49 and 65%, respectively). Also it was shown that pregnant solution obtained during leaching of the second sample with 10% sulfuric acid may be used for oxidative leaching of substandard copper-zinc concentrate that allowed to 13 and 48% of copper and zinc from the concentrate during the leaching at 80∘C. \nKeywords: flotation tailings, leaching, substandard sulfide concentrates","PeriodicalId":17908,"journal":{"name":"KnE Materials Science","volume":"44 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-12-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"KnE Materials Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.18502/kms.v6i1.8067","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The possibility of hydrometallurgical treatment of old flotation tailings to extract base and noble metals was investigated. Two samples of old flotation tailings samples containing 0.26% and 0.36% of copper, and 0.22% and 0.23% of zinc were the subjects of this study. Agitation and percolator leaching was performed with distilled water and sulfuric acid solutions (of 0.5 to 10% H2SO4). It was shown that under certain conditions (sulfuric acid concentration) it was possible to achieve selective leaching of non-ferrous metals and obtain solutions with relatively low concentrations of iron ions, which is necessary for further effective extraction of non-ferrous metal ions from the solution. The effect of acid leaching on further gold recovery from the first sample containing 0.7 g/t of gold by cyanidation was investigated. The sample of the tailings after leaching with a 1% sulfuric acid solution was leached with 10% sulfuric acid. After that, the tailings sample and the acid leach residues were subjected to sorption cyanidation. Two-stage acid leaching with 1 and 10% sulfuric acid provided the higher gold recovery than one-stage (49 and 65%, respectively). Also it was shown that pregnant solution obtained during leaching of the second sample with 10% sulfuric acid may be used for oxidative leaching of substandard copper-zinc concentrate that allowed to 13 and 48% of copper and zinc from the concentrate during the leaching at 80∘C.
Keywords: flotation tailings, leaching, substandard sulfide concentrates