{"title":"Fabrication of stabilized ZrO2 by hot petroleum drying method","authors":"Su-il Pyun","doi":"10.1016/0390-5519(79)90030-9","DOIUrl":null,"url":null,"abstract":"<div><p>A series of MgO- and CaO- partially and fully-stabilized ZrO<sub>2</sub> bodies were produced from sulfate and acetate powders using a wet chemical drying method (“ hot petroleum drying method ”). The optimum sintering conditions for powders produced from sulfates and acetates were found: calcining at 1200°C for 2–5 h, followed by sintering for 5 h at 1600°C. This drying process proved to be a very effective method for preparing stabilized ZrO<sub>2</sub> without conventional ceramic process of mixing, milling, and granulating.</p></div>","PeriodicalId":100227,"journal":{"name":"Ceramurgia International","volume":"5 2","pages":"Pages 61-65"},"PeriodicalIF":0.0000,"publicationDate":"1979-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1016/0390-5519(79)90030-9","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Ceramurgia International","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/0390551979900309","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
A series of MgO- and CaO- partially and fully-stabilized ZrO2 bodies were produced from sulfate and acetate powders using a wet chemical drying method (“ hot petroleum drying method ”). The optimum sintering conditions for powders produced from sulfates and acetates were found: calcining at 1200°C for 2–5 h, followed by sintering for 5 h at 1600°C. This drying process proved to be a very effective method for preparing stabilized ZrO2 without conventional ceramic process of mixing, milling, and granulating.