{"title":"抛光基板表面和涂层光学质量的清洁研究*","authors":"A. Tesar, W. Eickelberg, K. Koons, K. Davis","doi":"10.1364/oft.1992.wb11","DOIUrl":null,"url":null,"abstract":"The optical substrate-coating interface is established by (1) the original polished condition of the substrate; (2) the substrate cleaning process; and (3) the environment of the coating process. The substrate-coating interface affects the coating adhesion properties, is where most coating defects and scatter sites are thought to initiate, and in some instances may control the structure of the coating as it is deposited. Often features appear on an optic after coating which could not be observed after cleaning and prior to coating. Because of the wide variety of possible substrate materials, surface problems, and contaminants, cleaning processes are constantly evolving. Our study has clearly shown that the coating appearance is dependent not only on the cleaning method, but especially on the initial character of the substrate surface.","PeriodicalId":142307,"journal":{"name":"Optical Fabrication and Testing Workshop","volume":"40 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1992-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Polished Substrate Surface and Cleaning Study for Coated Optic Quality*\",\"authors\":\"A. Tesar, W. Eickelberg, K. Koons, K. Davis\",\"doi\":\"10.1364/oft.1992.wb11\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The optical substrate-coating interface is established by (1) the original polished condition of the substrate; (2) the substrate cleaning process; and (3) the environment of the coating process. The substrate-coating interface affects the coating adhesion properties, is where most coating defects and scatter sites are thought to initiate, and in some instances may control the structure of the coating as it is deposited. Often features appear on an optic after coating which could not be observed after cleaning and prior to coating. Because of the wide variety of possible substrate materials, surface problems, and contaminants, cleaning processes are constantly evolving. Our study has clearly shown that the coating appearance is dependent not only on the cleaning method, but especially on the initial character of the substrate surface.\",\"PeriodicalId\":142307,\"journal\":{\"name\":\"Optical Fabrication and Testing Workshop\",\"volume\":\"40 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1992-11-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Optical Fabrication and Testing Workshop\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1364/oft.1992.wb11\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Optical Fabrication and Testing Workshop","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1364/oft.1992.wb11","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

摘要

光学基片-镀膜界面由(1)基片的原始抛光状态建立;(2)基材清洗工艺;(3)涂装过程的环境。衬底-涂层界面影响涂层的粘附性能,是大多数涂层缺陷和散射点被认为是开始的地方,在某些情况下可能控制涂层的结构,因为它是沉积的。通常在涂层后的光学器件上出现的特征在清洗后和涂层前是无法观察到的。由于各种各样可能的基材,表面问题和污染物,清洁过程不断发展。我们的研究清楚地表明,涂层的外观不仅取决于清洁方法,而且尤其取决于基材表面的初始特性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Polished Substrate Surface and Cleaning Study for Coated Optic Quality*
The optical substrate-coating interface is established by (1) the original polished condition of the substrate; (2) the substrate cleaning process; and (3) the environment of the coating process. The substrate-coating interface affects the coating adhesion properties, is where most coating defects and scatter sites are thought to initiate, and in some instances may control the structure of the coating as it is deposited. Often features appear on an optic after coating which could not be observed after cleaning and prior to coating. Because of the wide variety of possible substrate materials, surface problems, and contaminants, cleaning processes are constantly evolving. Our study has clearly shown that the coating appearance is dependent not only on the cleaning method, but especially on the initial character of the substrate surface.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Defocus Measurement Using A Liquid Crystal Point Diffraction Interferometer Aberration Measurement Using Axial Intensity Polished Substrate Surface and Cleaning Study for Coated Optic Quality* Zerodur Polishing Process for High Surface Quality and High Efficiency* Surface Evaluation Techniques for the Optics of the Future
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1