桥梁正交异性钢桥面疲劳弹性设计

Wenli Fan, Huaiguang Li
{"title":"桥梁正交异性钢桥面疲劳弹性设计","authors":"Wenli Fan, Huaiguang Li","doi":"10.2749/nanjing.2022.1976","DOIUrl":null,"url":null,"abstract":"It is difficult to precisely predict the fatigue life of orthotropic decks due to random initial defects and high-cycle loading conditions. Two typical fatigue failures occurr in orthotropic steel decks, which hinder both the capacity and the efficient life of modern steel bridges. The Type 1 crack is along the super-long weld joints between the cover plate and U-shaped rib, while Type 2 crack develop within the diaphragm adjacent to the fillet joints. While both cracks originate and develop from weld toes, and the Type 2 crack usually develop along the near-horizontal direction. Among the many factors contributing to the failure, the notch type, notch size, vehicle loads uncertainties related to positions, magnitudes and frequency were uncertain. Thus, it is reasonable to apply different strategies to achieve more resilient orthotropic decks. It is recommended new weld improvement has to be introduced to mitigate initial notch for type Ⅰ details, and structural flexibility has to be selected to improve the fatigue performance for type Ⅱ detail.","PeriodicalId":410450,"journal":{"name":"IABSE Congress, Nanjing 2022: Bridges and Structures: Connection, Integration and Harmonisation","volume":"67 5 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Fatigue Resilient Design of Bridge Orthotropic Steel Deck\",\"authors\":\"Wenli Fan, Huaiguang Li\",\"doi\":\"10.2749/nanjing.2022.1976\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"It is difficult to precisely predict the fatigue life of orthotropic decks due to random initial defects and high-cycle loading conditions. Two typical fatigue failures occurr in orthotropic steel decks, which hinder both the capacity and the efficient life of modern steel bridges. The Type 1 crack is along the super-long weld joints between the cover plate and U-shaped rib, while Type 2 crack develop within the diaphragm adjacent to the fillet joints. While both cracks originate and develop from weld toes, and the Type 2 crack usually develop along the near-horizontal direction. Among the many factors contributing to the failure, the notch type, notch size, vehicle loads uncertainties related to positions, magnitudes and frequency were uncertain. Thus, it is reasonable to apply different strategies to achieve more resilient orthotropic decks. It is recommended new weld improvement has to be introduced to mitigate initial notch for type Ⅰ details, and structural flexibility has to be selected to improve the fatigue performance for type Ⅱ detail.\",\"PeriodicalId\":410450,\"journal\":{\"name\":\"IABSE Congress, Nanjing 2022: Bridges and Structures: Connection, Integration and Harmonisation\",\"volume\":\"67 5 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"IABSE Congress, Nanjing 2022: Bridges and Structures: Connection, Integration and Harmonisation\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.2749/nanjing.2022.1976\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"IABSE Congress, Nanjing 2022: Bridges and Structures: Connection, Integration and Harmonisation","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2749/nanjing.2022.1976","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

正交各向异性甲板由于随机初始缺陷和高周载荷条件,使其疲劳寿命难以准确预测。正交各向异性钢桥面存在两种典型的疲劳破坏,严重影响了现代钢结构桥梁的承载力和有效使用寿命。1型裂纹主要分布在盖板与u型肋之间的超长焊缝处,2型裂纹主要分布在靠近圆角接头的膜片处。两种裂纹均从焊趾处产生和发展,2型裂纹通常沿近水平方向发展。在导致失效的诸多因素中,缺口类型、缺口尺寸、与位置、幅度和频率相关的车辆载荷不确定性是不确定的。因此,采用不同的策略来获得更有弹性的正交各向异性甲板是合理的。建议引入新的焊缝改进以减轻Ⅰ型细部的初始缺口,并选择结构灵活性以改善Ⅱ型细部的疲劳性能。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Fatigue Resilient Design of Bridge Orthotropic Steel Deck
It is difficult to precisely predict the fatigue life of orthotropic decks due to random initial defects and high-cycle loading conditions. Two typical fatigue failures occurr in orthotropic steel decks, which hinder both the capacity and the efficient life of modern steel bridges. The Type 1 crack is along the super-long weld joints between the cover plate and U-shaped rib, while Type 2 crack develop within the diaphragm adjacent to the fillet joints. While both cracks originate and develop from weld toes, and the Type 2 crack usually develop along the near-horizontal direction. Among the many factors contributing to the failure, the notch type, notch size, vehicle loads uncertainties related to positions, magnitudes and frequency were uncertain. Thus, it is reasonable to apply different strategies to achieve more resilient orthotropic decks. It is recommended new weld improvement has to be introduced to mitigate initial notch for type Ⅰ details, and structural flexibility has to be selected to improve the fatigue performance for type Ⅱ detail.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
FE Modeling of the Interfacial Behaviour of Precast Multi-box Girder The Behavior of Long-span Suspended Footbridge Under Wind Load The Durability and SHM System of Hong Kong-Zhuhai-Macao Bridge Study on the Influence of Bridge Expansion Joints on Vehicle-Track- Bridge System Numerical Examination in Bridge Responses due to Fracture of Truss Member in a Steel Truss Bridge under Vehicle Loadings
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1