{"title":"用于评价ILI测量性能的管道制造裂纹","authors":"Jason B. Skow, J. Krynicki, Lujian Peng","doi":"10.1115/IPC2020-9400","DOIUrl":null,"url":null,"abstract":"\n Recently, transmission pipeline operators have started designing pipe spools with manufactured cracks of very precise size and orientation for the purpose of qualifying measurement technologies. The manufactured cracks are very similar to naturally occurring cracks and can be made to have varied profiles and off-planar shapes (like hook cracks). The manufactured spools are installed on a transmission pipeline at either the pipe launcher, the receiver or in-line such that an in-line inpsection (ILI) tool passes through it during a transmission pipeline ILI field run. This produces highly valuable data to evaluate measurement performance because the crack sizes are precisely known, crack morphologies are similar to realistic cracks and the ILI tool is tested in field conditions. This paper describes the effect on the estimated ILI tool measurement performance for various combinations of manufactured cracks in a pipe spool. The cases described vary the number of manufactured cracks in the spool to estimate the value of each additional crack and vary the distribution of cracks sizes to compare the value of large versus small cracks.","PeriodicalId":273758,"journal":{"name":"Volume 1: Pipeline and Facilities Integrity","volume":"31 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2020-09-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Manufactured Cracks in Pipe Used to Evaluate ILI Measurement Performance\",\"authors\":\"Jason B. Skow, J. Krynicki, Lujian Peng\",\"doi\":\"10.1115/IPC2020-9400\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\\n Recently, transmission pipeline operators have started designing pipe spools with manufactured cracks of very precise size and orientation for the purpose of qualifying measurement technologies. The manufactured cracks are very similar to naturally occurring cracks and can be made to have varied profiles and off-planar shapes (like hook cracks). The manufactured spools are installed on a transmission pipeline at either the pipe launcher, the receiver or in-line such that an in-line inpsection (ILI) tool passes through it during a transmission pipeline ILI field run. This produces highly valuable data to evaluate measurement performance because the crack sizes are precisely known, crack morphologies are similar to realistic cracks and the ILI tool is tested in field conditions. This paper describes the effect on the estimated ILI tool measurement performance for various combinations of manufactured cracks in a pipe spool. The cases described vary the number of manufactured cracks in the spool to estimate the value of each additional crack and vary the distribution of cracks sizes to compare the value of large versus small cracks.\",\"PeriodicalId\":273758,\"journal\":{\"name\":\"Volume 1: Pipeline and Facilities Integrity\",\"volume\":\"31 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-09-28\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Volume 1: Pipeline and Facilities Integrity\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1115/IPC2020-9400\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Volume 1: Pipeline and Facilities Integrity","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1115/IPC2020-9400","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

最近,输油管道运营商已经开始设计带有非常精确尺寸和方向的制造裂纹的管轴,以满足测量技术的要求。制造的裂缝与自然产生的裂缝非常相似,可以制造出不同的轮廓和非平面形状(如钩状裂缝)。制造的线轴安装在管道发射器、接收器或直列管道上,以便在传输管道ILI现场运行期间,直列检查(ILI)工具通过它。这为评估测量性能提供了非常有价值的数据,因为裂缝尺寸是精确已知的,裂缝形态与实际裂缝相似,ILI工具在现场条件下进行了测试。本文描述了管道阀芯制造裂纹的各种组合对ILI工具测量性能的影响。所描述的情况改变了线轴中制造裂缝的数量,以估计每个额外裂缝的值,并改变了裂缝尺寸的分布,以比较大裂缝和小裂缝的值。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Manufactured Cracks in Pipe Used to Evaluate ILI Measurement Performance
Recently, transmission pipeline operators have started designing pipe spools with manufactured cracks of very precise size and orientation for the purpose of qualifying measurement technologies. The manufactured cracks are very similar to naturally occurring cracks and can be made to have varied profiles and off-planar shapes (like hook cracks). The manufactured spools are installed on a transmission pipeline at either the pipe launcher, the receiver or in-line such that an in-line inpsection (ILI) tool passes through it during a transmission pipeline ILI field run. This produces highly valuable data to evaluate measurement performance because the crack sizes are precisely known, crack morphologies are similar to realistic cracks and the ILI tool is tested in field conditions. This paper describes the effect on the estimated ILI tool measurement performance for various combinations of manufactured cracks in a pipe spool. The cases described vary the number of manufactured cracks in the spool to estimate the value of each additional crack and vary the distribution of cracks sizes to compare the value of large versus small cracks.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Application of Noise Filtering Techniques for the Quantification of Uncertainty in Dent Strain Calculations The Impact of Pressure Fluctuations on the Early Onset of Stage II Growth of High pH Stress Corrosion Crack A Data Driven Validation of a Defect Assessment Model and its Safe Implementation Microwave Chipless Resonator Strain Sensor for Pipeline Safety Monitoring Full-Scale Fatigue Testing of Crack-in-Dent and Framework Development for Life Prediction
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1