煅烧工艺对工业废渣中富铁酸钙硅酸盐水泥熟料铁酸盐相和硅酸盐相的影响

IF 4.7 3区 工程技术 Q1 CONSTRUCTION & BUILDING TECHNOLOGY Journal of Sustainable Cement-Based Materials Pub Date : 2023-09-15 DOI:10.1080/21650373.2023.2258124
Yifan Gao, Xiaolin Liu, Zhaofeng Li, Jian Zhang
{"title":"煅烧工艺对工业废渣中富铁酸钙硅酸盐水泥熟料铁酸盐相和硅酸盐相的影响","authors":"Yifan Gao, Xiaolin Liu, Zhaofeng Li, Jian Zhang","doi":"10.1080/21650373.2023.2258124","DOIUrl":null,"url":null,"abstract":"AbstractIn this paper, the industrial solid waste with potential cementitious activity was used to prepare ferrite-belite-rich Portland cement clinker. The changes in solid waste composition, raw meal ratio, calcination temperature, and holding time on the type and content of iron aluminate phase and silicate phase in the clinker were studied. The effects of flue gas desulfurization gypsum on the mechanical properties of clinker, mineral composition, and microstructure of hardened slurry were briefly discussed. In addition, the sustainability of the production of ferrite-belite-rich Portland cement clinker was evaluated by using a life cycle assessment. The analysis results show that: (1) The content of the ferrite phase increased first and then decreased with the increase of calcination temperature, and the content of the silicate phase and ferrite phase increased first and then decreased with the extension of holding time. (2) With the change of calcination temperature, the silicate phase is always cobblestone-like and evenly distributed. The ferrite phase changes from granular or flake to branch dendritic, and finally is swallowed by the liquid phase, filled between the gaps of the silicate phase structure, or attached to the surface of the silicate phase. (3) The Si elements in the clinker are always agglomerated in cobblestone shapes with uneven sizes. With the holding time from 30 min to 60 min, the distribution area of Al and Fe elements in the gaps of silicate phases increased gradually. Some Al and Fe elements are distributed in the area where silicate phase minerals are located. When the holding time is extended to 90 min, Fe and Al elements tend to be randomly distributed. (4) Fe will replace part of Al to form Fe-ettringite, Fe-siliceous hydrogarnet, etc. in the hydration process of C4AF. (5) The use of red mud, carbide slag, and silica fume to produce ferrite-belite-rich Portland cement clinker will reduce carbon emissions by 57.50%.Keywords: Ferrite-belite-rich Portland cement clinkercalcination temperatureholding timemineral compositionmicrostructure AcknowledgmentThe authors acknowledge the support of this work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province, the National Key R&D Program of China and the Key Projects of Natural Science Foundation of Shandong Province.Disclosure statementNo potential conflict of interest was reported by the author(s).Additional informationFundingThis work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province [Grants Nos. 2020CXGC011405 and Grants Nos. 2021CXGC010301], the National Key R&D Program of China [Grants Nos. 2022YFB2601900] and the Key Projects of Natural Science Foundation of Shandong Province [No. 2020KE006].","PeriodicalId":48521,"journal":{"name":"Journal of Sustainable Cement-Based Materials","volume":"9 1","pages":"0"},"PeriodicalIF":4.7000,"publicationDate":"2023-09-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Effect of calcination process on ferrite phase and silicate phase of ferrite-belite-rich Portland cement clinker from industrial solid waste\",\"authors\":\"Yifan Gao, Xiaolin Liu, Zhaofeng Li, Jian Zhang\",\"doi\":\"10.1080/21650373.2023.2258124\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"AbstractIn this paper, the industrial solid waste with potential cementitious activity was used to prepare ferrite-belite-rich Portland cement clinker. The changes in solid waste composition, raw meal ratio, calcination temperature, and holding time on the type and content of iron aluminate phase and silicate phase in the clinker were studied. The effects of flue gas desulfurization gypsum on the mechanical properties of clinker, mineral composition, and microstructure of hardened slurry were briefly discussed. In addition, the sustainability of the production of ferrite-belite-rich Portland cement clinker was evaluated by using a life cycle assessment. The analysis results show that: (1) The content of the ferrite phase increased first and then decreased with the increase of calcination temperature, and the content of the silicate phase and ferrite phase increased first and then decreased with the extension of holding time. (2) With the change of calcination temperature, the silicate phase is always cobblestone-like and evenly distributed. The ferrite phase changes from granular or flake to branch dendritic, and finally is swallowed by the liquid phase, filled between the gaps of the silicate phase structure, or attached to the surface of the silicate phase. (3) The Si elements in the clinker are always agglomerated in cobblestone shapes with uneven sizes. With the holding time from 30 min to 60 min, the distribution area of Al and Fe elements in the gaps of silicate phases increased gradually. Some Al and Fe elements are distributed in the area where silicate phase minerals are located. When the holding time is extended to 90 min, Fe and Al elements tend to be randomly distributed. (4) Fe will replace part of Al to form Fe-ettringite, Fe-siliceous hydrogarnet, etc. in the hydration process of C4AF. (5) The use of red mud, carbide slag, and silica fume to produce ferrite-belite-rich Portland cement clinker will reduce carbon emissions by 57.50%.Keywords: Ferrite-belite-rich Portland cement clinkercalcination temperatureholding timemineral compositionmicrostructure AcknowledgmentThe authors acknowledge the support of this work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province, the National Key R&D Program of China and the Key Projects of Natural Science Foundation of Shandong Province.Disclosure statementNo potential conflict of interest was reported by the author(s).Additional informationFundingThis work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province [Grants Nos. 2020CXGC011405 and Grants Nos. 2021CXGC010301], the National Key R&D Program of China [Grants Nos. 2022YFB2601900] and the Key Projects of Natural Science Foundation of Shandong Province [No. 2020KE006].\",\"PeriodicalId\":48521,\"journal\":{\"name\":\"Journal of Sustainable Cement-Based Materials\",\"volume\":\"9 1\",\"pages\":\"0\"},\"PeriodicalIF\":4.7000,\"publicationDate\":\"2023-09-15\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Sustainable Cement-Based Materials\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1080/21650373.2023.2258124\",\"RegionNum\":3,\"RegionCategory\":\"工程技术\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"CONSTRUCTION & BUILDING TECHNOLOGY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Sustainable Cement-Based Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/21650373.2023.2258124","RegionNum":3,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"CONSTRUCTION & BUILDING TECHNOLOGY","Score":null,"Total":0}
引用次数: 0

摘要

摘要利用具有潜在胶凝活性的工业固体废弃物制备富铁酸盐-白石硅酸盐水泥熟料。研究了固废组成、生料比、煅烧温度、保温时间等因素对熟料中铝酸铁相和硅酸盐相类型及含量的影响。简要讨论了烟气脱硫石膏对熟料力学性能、矿物组成和硬化浆料微观结构的影响。此外,采用生命周期评价法对富铁酸钡硅酸盐水泥熟料生产的可持续性进行了评价。分析结果表明:(1)铁素体相含量随煅烧温度的升高先升高后降低,硅酸盐相和铁素体相含量随保温时间的延长先升高后降低。(2)随着煅烧温度的变化,硅酸盐相始终呈鹅卵石状且分布均匀。铁素体相由粒状或片状变为枝状,最后被液相吞噬,填充在硅酸盐相结构的间隙之间,或附着在硅酸盐相的表面。(3)熟料中的Si元素总是聚集成鹅卵石状,大小不均匀。随着保温时间从30 min增加到60 min, Al和Fe元素在硅酸盐相间隙中的分布面积逐渐增大。部分铝、铁元素分布在硅酸盐相矿物所在区域。保温时间延长至90min后,Fe和Al元素趋于随机分布。(4)在C4AF水化过程中,Fe会取代部分Al形成Fe-钙矾石、Fe-硅质水榴石等。(5)利用赤泥、电石渣、硅灰生产富铁氧体-白铁矿硅酸盐水泥熟料,可减少57.50%的碳排放。关键词:富铁酸盐-白石硅酸盐水泥熟料煅烧保温时间矿物成分微观结构致谢本文得到了山东省重大科技创新专项、国家重点研发计划和山东省自然科学基金重点项目的支持。披露声明作者未报告潜在的利益冲突。项目资助:山东省重大科技创新项目[批准号:2020CXGC011405和批准号:2021CXGC010301]、国家重点研发计划[批准号:2022YFB2601900]、山东省自然科学基金重点项目[批准号:2022YFB2601900];2020 ke006]。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Effect of calcination process on ferrite phase and silicate phase of ferrite-belite-rich Portland cement clinker from industrial solid waste
AbstractIn this paper, the industrial solid waste with potential cementitious activity was used to prepare ferrite-belite-rich Portland cement clinker. The changes in solid waste composition, raw meal ratio, calcination temperature, and holding time on the type and content of iron aluminate phase and silicate phase in the clinker were studied. The effects of flue gas desulfurization gypsum on the mechanical properties of clinker, mineral composition, and microstructure of hardened slurry were briefly discussed. In addition, the sustainability of the production of ferrite-belite-rich Portland cement clinker was evaluated by using a life cycle assessment. The analysis results show that: (1) The content of the ferrite phase increased first and then decreased with the increase of calcination temperature, and the content of the silicate phase and ferrite phase increased first and then decreased with the extension of holding time. (2) With the change of calcination temperature, the silicate phase is always cobblestone-like and evenly distributed. The ferrite phase changes from granular or flake to branch dendritic, and finally is swallowed by the liquid phase, filled between the gaps of the silicate phase structure, or attached to the surface of the silicate phase. (3) The Si elements in the clinker are always agglomerated in cobblestone shapes with uneven sizes. With the holding time from 30 min to 60 min, the distribution area of Al and Fe elements in the gaps of silicate phases increased gradually. Some Al and Fe elements are distributed in the area where silicate phase minerals are located. When the holding time is extended to 90 min, Fe and Al elements tend to be randomly distributed. (4) Fe will replace part of Al to form Fe-ettringite, Fe-siliceous hydrogarnet, etc. in the hydration process of C4AF. (5) The use of red mud, carbide slag, and silica fume to produce ferrite-belite-rich Portland cement clinker will reduce carbon emissions by 57.50%.Keywords: Ferrite-belite-rich Portland cement clinkercalcination temperatureholding timemineral compositionmicrostructure AcknowledgmentThe authors acknowledge the support of this work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province, the National Key R&D Program of China and the Key Projects of Natural Science Foundation of Shandong Province.Disclosure statementNo potential conflict of interest was reported by the author(s).Additional informationFundingThis work was supported by the Major Scientific and Technological Innovation Projects in Shandong Province [Grants Nos. 2020CXGC011405 and Grants Nos. 2021CXGC010301], the National Key R&D Program of China [Grants Nos. 2022YFB2601900] and the Key Projects of Natural Science Foundation of Shandong Province [No. 2020KE006].
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
6.60
自引率
15.90%
发文量
71
期刊介绍: The Journal of Sustainable Cement-Based Materials aims to publish theoretical and applied researches on materials, products and structures that incorporate cement. The journal is a forum for discussion of research on manufacture, hydration and performance of cement-based materials; novel experimental techniques; the latest analytical and modelling methods; the examination and the diagnosis of real cement and concrete structures; and the potential for improved cement-based materials. The journal welcomes original research papers, major reviews, rapid communications and selected conference papers. The Journal of Sustainable Cement-Based Materials covers a wide range of topics within its subject category, including but are not limited to: • raw materials and manufacture of cement • mixing, rheology and hydration • admixtures • structural characteristics and performance of cement-based materials • characterisation techniques and modeling • use of fibre in cement based-materials • degradation and repair of cement-based materials • novel testing techniques and applications • waste management
期刊最新文献
Preparation of high flexural strength rankinite cement benefiting from formation of aragonite whisker during carbonation curing Hydration mechanism and mechanical properties of a developed low-carbon and lightweight strain-hardening cementitious composites Development and characterization of volume-stabilized grouts used for borehole heat exchangers Piezoresistive performance of self-sensing cement-based composites filled with multi-layer graphene Mechanical and microstructural properties of structural and non-structural lightweight foamed concrete with coal bottom ash as cement and sand replacement material
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1