{"title":"Pahae天然沸石-煤底灰吸附剂的合成与表征","authors":"Susilawati Susilawati, Nurul Syafina Lubis, Khatarina Meldawati Pasaribu","doi":"10.14710/jksa.26.6.211-216","DOIUrl":null,"url":null,"abstract":"Zeolite is a porous crystalline mineral alumina silica tetrahydrate that has an open three-dimensional framework structure that has channels and cavities filled with metal ions, while Bottom ash is also known to have high porosity and surface area. Thus, both zeolite and bottom ash can be used as adsorbents. This study aims to make an adsorbent based on Pahae natural zeolite with a mixture of bottom ash from coal as an adsorbent for iron (Fe) and manganese (Mn) metals in well water. Adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash with a size of 200 mesh (74 µm) which has been chemically activated with 1 M NaOH solution, was prepared with various compositions of (100:0)%, (95:5)%, (90:10)%, (85:15)%, (80:20)%, (75:25)% respectively, then mold using a hydraulic press with a load of 6 tons of weight for 10 minutes. The mold samples were then physically activated with temperature variations of 600°C, 700°C, and 800°C for 4 hours, respectively. The addition of coal bottom ash filler is known to increase the porosity of the adsorbent with the composition of (75:25)% with an activated temperature of 800°C by 10%. The results of the AAS test showed that the adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash reduced the content of Fe and Mn metals by 92.37% and 53.49% in well water, respectively.","PeriodicalId":17811,"journal":{"name":"Jurnal Kimia Sains dan Aplikasi","volume":"13 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"The Synthesis and Characterization of Pahae Natural Zeolite-Coal Bottom Ash Adsorbent for Fe and Mn Purifier in Well Water\",\"authors\":\"Susilawati Susilawati, Nurul Syafina Lubis, Khatarina Meldawati Pasaribu\",\"doi\":\"10.14710/jksa.26.6.211-216\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Zeolite is a porous crystalline mineral alumina silica tetrahydrate that has an open three-dimensional framework structure that has channels and cavities filled with metal ions, while Bottom ash is also known to have high porosity and surface area. Thus, both zeolite and bottom ash can be used as adsorbents. This study aims to make an adsorbent based on Pahae natural zeolite with a mixture of bottom ash from coal as an adsorbent for iron (Fe) and manganese (Mn) metals in well water. Adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash with a size of 200 mesh (74 µm) which has been chemically activated with 1 M NaOH solution, was prepared with various compositions of (100:0)%, (95:5)%, (90:10)%, (85:15)%, (80:20)%, (75:25)% respectively, then mold using a hydraulic press with a load of 6 tons of weight for 10 minutes. The mold samples were then physically activated with temperature variations of 600°C, 700°C, and 800°C for 4 hours, respectively. The addition of coal bottom ash filler is known to increase the porosity of the adsorbent with the composition of (75:25)% with an activated temperature of 800°C by 10%. The results of the AAS test showed that the adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash reduced the content of Fe and Mn metals by 92.37% and 53.49% in well water, respectively.\",\"PeriodicalId\":17811,\"journal\":{\"name\":\"Jurnal Kimia Sains dan Aplikasi\",\"volume\":\"13 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-08-22\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Jurnal Kimia Sains dan Aplikasi\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.14710/jksa.26.6.211-216\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Kimia Sains dan Aplikasi","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.14710/jksa.26.6.211-216","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

沸石是一种多孔晶体矿物四水氧化铝二氧化硅,具有开放的三维框架结构,具有充满金属离子的通道和空腔,而底灰也具有较高的孔隙率和表面积。因此,沸石和底灰都可以作为吸附剂。本研究旨在以Pahae天然沸石为基材,以煤底灰混合制备吸附剂,作为井水中铁(Fe)和锰(Mn)金属的吸附剂。以200目(74µm)的天然沸石pahae -煤底灰为吸附剂,经1m NaOH溶液化学活化,分别配制成(100:0)%、(95:5)%、(90:10)%、(85:15)%、(80:20)%、(75:25)%等不同配比的吸附剂,在负载6吨重量的液压机上成型10分钟。然后将模具样品分别在600°C、700°C和800°C的温度变化下物理激活4小时。已知添加煤底灰填料可使组分为(75:25)%、活化温度为800℃的吸附剂的孔隙率提高10%。原子吸收光谱(AAS)测试结果表明,天然沸石-煤底灰制备的吸附剂对井水中铁和锰金属的含量分别降低了92.37%和53.49%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
The Synthesis and Characterization of Pahae Natural Zeolite-Coal Bottom Ash Adsorbent for Fe and Mn Purifier in Well Water
Zeolite is a porous crystalline mineral alumina silica tetrahydrate that has an open three-dimensional framework structure that has channels and cavities filled with metal ions, while Bottom ash is also known to have high porosity and surface area. Thus, both zeolite and bottom ash can be used as adsorbents. This study aims to make an adsorbent based on Pahae natural zeolite with a mixture of bottom ash from coal as an adsorbent for iron (Fe) and manganese (Mn) metals in well water. Adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash with a size of 200 mesh (74 µm) which has been chemically activated with 1 M NaOH solution, was prepared with various compositions of (100:0)%, (95:5)%, (90:10)%, (85:15)%, (80:20)%, (75:25)% respectively, then mold using a hydraulic press with a load of 6 tons of weight for 10 minutes. The mold samples were then physically activated with temperature variations of 600°C, 700°C, and 800°C for 4 hours, respectively. The addition of coal bottom ash filler is known to increase the porosity of the adsorbent with the composition of (75:25)% with an activated temperature of 800°C by 10%. The results of the AAS test showed that the adsorbent made from Natural Zeolite Pahae-Coal Bottom Ash reduced the content of Fe and Mn metals by 92.37% and 53.49% in well water, respectively.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
36
审稿时长
17 weeks
期刊最新文献
Production of Biodiesel from Candlenut Seed Oil (Aleurites Moluccana Wild) Using a NaOH/CaO/Ca Catalyst with Microwave Heating Synthesis of Molecularly Imprinted Polymers with Magnetite Cores for Ibuprofen Adsorption Impact of Fermentation on Hyptolide and Phytochemical Composition of Hyptis pectinata (L.) Poit Effects of Temperature, Molecular Weight, and Non-Solvent Variation on the Physical Properties of PVDF Membranes Prepared through Immersion Precipitation Isolation of Phenolic Acids from Land Kale (Ipomoea reptans Poir) and Antioxidant Activity
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1