{"title":"韩国落叶松和日本雪松建筑材料阻燃剂的最佳浸渍量","authors":"Seok-Un Jo, HAK-BYUNG Chae, H. Park, EUN-SUK Jang","doi":"10.37763/wr.1336-4561/69.1.179186","DOIUrl":null,"url":null,"abstract":"In Korea, in accordance with regulations MOLIT notice 2023-24 regarding the flame retardant performance of building finishing materials and fire spread prevention structure, it is mandated that flame-retardant materials have a total heat emission less than 8 MJ/m2. Consequently, our study aimed to determine the quantity of flame-retardant treatment required to meet MOLIT notice 2023-24 for Korean larch and Japanese cedar, as commonly used exterior materials in construction. To this end, we investigated using a cone calorimeter to observe changes in the THR (total heat released) depending on the SCFI (solid content of flame-retardant impregnation). Our simple linear regression analysis indicated that the SCFI needed to satisfy the prescribed flame-retardant standard of 8 MJ/m2 was 93.9 kg/m3 for Korean larch and 144.6 kg/m3 for Japanese cedar. As a result, we established optimal impregnation levels of flame retardant for both species.","PeriodicalId":0,"journal":{"name":"","volume":"6 5","pages":""},"PeriodicalIF":0.0,"publicationDate":"2024-04-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"THE OPTIMAL IMPREGNATION AMOUNTS OF FLAME-RETARDANT FOR KOREAN LARCH AND JAPANESE CEDAR BUILDING MATERIALS\",\"authors\":\"Seok-Un Jo, HAK-BYUNG Chae, H. Park, EUN-SUK Jang\",\"doi\":\"10.37763/wr.1336-4561/69.1.179186\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In Korea, in accordance with regulations MOLIT notice 2023-24 regarding the flame retardant performance of building finishing materials and fire spread prevention structure, it is mandated that flame-retardant materials have a total heat emission less than 8 MJ/m2. Consequently, our study aimed to determine the quantity of flame-retardant treatment required to meet MOLIT notice 2023-24 for Korean larch and Japanese cedar, as commonly used exterior materials in construction. To this end, we investigated using a cone calorimeter to observe changes in the THR (total heat released) depending on the SCFI (solid content of flame-retardant impregnation). Our simple linear regression analysis indicated that the SCFI needed to satisfy the prescribed flame-retardant standard of 8 MJ/m2 was 93.9 kg/m3 for Korean larch and 144.6 kg/m3 for Japanese cedar. As a result, we established optimal impregnation levels of flame retardant for both species.\",\"PeriodicalId\":0,\"journal\":{\"name\":\"\",\"volume\":\"6 5\",\"pages\":\"\"},\"PeriodicalIF\":0.0,\"publicationDate\":\"2024-04-25\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.37763/wr.1336-4561/69.1.179186\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.37763/wr.1336-4561/69.1.179186","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
THE OPTIMAL IMPREGNATION AMOUNTS OF FLAME-RETARDANT FOR KOREAN LARCH AND JAPANESE CEDAR BUILDING MATERIALS
In Korea, in accordance with regulations MOLIT notice 2023-24 regarding the flame retardant performance of building finishing materials and fire spread prevention structure, it is mandated that flame-retardant materials have a total heat emission less than 8 MJ/m2. Consequently, our study aimed to determine the quantity of flame-retardant treatment required to meet MOLIT notice 2023-24 for Korean larch and Japanese cedar, as commonly used exterior materials in construction. To this end, we investigated using a cone calorimeter to observe changes in the THR (total heat released) depending on the SCFI (solid content of flame-retardant impregnation). Our simple linear regression analysis indicated that the SCFI needed to satisfy the prescribed flame-retardant standard of 8 MJ/m2 was 93.9 kg/m3 for Korean larch and 144.6 kg/m3 for Japanese cedar. As a result, we established optimal impregnation levels of flame retardant for both species.