带保护涂层的 Ti-6Al-4V 钛合金在高速腐蚀过程中的磨损和失效分析

IF 1.8 4区 材料科学 Q2 MATERIALS SCIENCE, CHARACTERIZATION & TESTING Physical Mesomechanics Pub Date : 2024-08-23 DOI:10.1134/S1029959924040039
S. A. Atroshenko, R. Z. Valiev, N. F. Morozov, R. R. Valiev, Ya. N. Savina, M. N. Antonova, A. D. Evstifeev
{"title":"带保护涂层的 Ti-6Al-4V 钛合金在高速腐蚀过程中的磨损和失效分析","authors":"S. A. Atroshenko,&nbsp;R. Z. Valiev,&nbsp;N. F. Morozov,&nbsp;R. R. Valiev,&nbsp;Ya. N. Savina,&nbsp;M. N. Antonova,&nbsp;A. D. Evstifeev","doi":"10.1134/S1029959924040039","DOIUrl":null,"url":null,"abstract":"<p>An experimental study is presented on the wear and failure of initial coarse-grained and modified ultrafine-grained Ti-6Al-4V alloy with a TiN protective coating, subjected to high-speed dynamic erosion by solid corundum particles with an average size of 109 μm in an air flow at a speed of 150 m/s and an erosion time of 30, 60, 180, 300 and 600 s. The experimental results are used to determine the erosive wear rate and the shear area percentage, as well as to measure the worn layer depth and erosion-induced changes in microhardness and structure of the alloy near the coated and uncoated surface. It is shown that all alloy samples are prone to wear and failure under the given high-speed erosion conditions, but their behavior is closely related to the erosion time and the structure of the substrate. The protective coating deposited onto the surface of ultrafine-grained Ti-6Al-4V titanium alloy significantly reduces the erosive wear rate compared to a similar coating on as-received coarse-grained alloy.</p>","PeriodicalId":726,"journal":{"name":"Physical Mesomechanics","volume":"27 4","pages":"387 - 397"},"PeriodicalIF":1.8000,"publicationDate":"2024-08-23","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Wear and Failure Analysis of Ti-6Al-4V Titanium Alloy with a Protective Coating during High-Speed Erosion\",\"authors\":\"S. A. Atroshenko,&nbsp;R. Z. Valiev,&nbsp;N. F. Morozov,&nbsp;R. R. Valiev,&nbsp;Ya. N. Savina,&nbsp;M. N. Antonova,&nbsp;A. D. Evstifeev\",\"doi\":\"10.1134/S1029959924040039\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>An experimental study is presented on the wear and failure of initial coarse-grained and modified ultrafine-grained Ti-6Al-4V alloy with a TiN protective coating, subjected to high-speed dynamic erosion by solid corundum particles with an average size of 109 μm in an air flow at a speed of 150 m/s and an erosion time of 30, 60, 180, 300 and 600 s. The experimental results are used to determine the erosive wear rate and the shear area percentage, as well as to measure the worn layer depth and erosion-induced changes in microhardness and structure of the alloy near the coated and uncoated surface. It is shown that all alloy samples are prone to wear and failure under the given high-speed erosion conditions, but their behavior is closely related to the erosion time and the structure of the substrate. The protective coating deposited onto the surface of ultrafine-grained Ti-6Al-4V titanium alloy significantly reduces the erosive wear rate compared to a similar coating on as-received coarse-grained alloy.</p>\",\"PeriodicalId\":726,\"journal\":{\"name\":\"Physical Mesomechanics\",\"volume\":\"27 4\",\"pages\":\"387 - 397\"},\"PeriodicalIF\":1.8000,\"publicationDate\":\"2024-08-23\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Physical Mesomechanics\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://link.springer.com/article/10.1134/S1029959924040039\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"MATERIALS SCIENCE, CHARACTERIZATION & TESTING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Physical Mesomechanics","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1134/S1029959924040039","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, CHARACTERIZATION & TESTING","Score":null,"Total":0}
引用次数: 0

摘要

摘要 本文对带有 TiN 保护涂层的初始粗晶粒和改性超细晶粒 Ti-6Al-4V 合金的磨损和失效情况进行了实验研究。在速度为 150 m/s、侵蚀时间为 30、60、180、300 和 600 s 的气流中,平均粒度为 109 μm 的固体刚玉颗粒对合金进行高速动态侵蚀。实验结果用于确定侵蚀磨损率和剪切面积百分比,以及测量磨损层深度和侵蚀引起的涂层和未涂层表面附近合金微硬度和结构的变化。结果表明,在给定的高速侵蚀条件下,所有合金样品都容易发生磨损和失效,但其行为与侵蚀时间和基体结构密切相关。在超细晶粒 Ti-6Al-4V 钛合金表面沉积的保护涂层与在粗晶粒合金表面沉积的类似涂层相比,可显著降低侵蚀磨损率。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

摘要图片

摘要图片

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Wear and Failure Analysis of Ti-6Al-4V Titanium Alloy with a Protective Coating during High-Speed Erosion

An experimental study is presented on the wear and failure of initial coarse-grained and modified ultrafine-grained Ti-6Al-4V alloy with a TiN protective coating, subjected to high-speed dynamic erosion by solid corundum particles with an average size of 109 μm in an air flow at a speed of 150 m/s and an erosion time of 30, 60, 180, 300 and 600 s. The experimental results are used to determine the erosive wear rate and the shear area percentage, as well as to measure the worn layer depth and erosion-induced changes in microhardness and structure of the alloy near the coated and uncoated surface. It is shown that all alloy samples are prone to wear and failure under the given high-speed erosion conditions, but their behavior is closely related to the erosion time and the structure of the substrate. The protective coating deposited onto the surface of ultrafine-grained Ti-6Al-4V titanium alloy significantly reduces the erosive wear rate compared to a similar coating on as-received coarse-grained alloy.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Physical Mesomechanics
Physical Mesomechanics Materials Science-General Materials Science
CiteScore
3.50
自引率
18.80%
发文量
48
期刊介绍: The journal provides an international medium for the publication of theoretical and experimental studies and reviews related in the physical mesomechanics and also solid-state physics, mechanics, materials science, geodynamics, non-destructive testing and in a large number of other fields where the physical mesomechanics may be used extensively. Papers dealing with the processing, characterization, structure and physical properties and computational aspects of the mesomechanics of heterogeneous media, fracture mesomechanics, physical mesomechanics of materials, mesomechanics applications for geodynamics and tectonics, mesomechanics of smart materials and materials for electronics, non-destructive testing are viewed as suitable for publication.
期刊最新文献
Evaluation of the Effective Mechanical Properties of a Particle-Reinforced Polymer Composite with Low-Modulus Inclusions Absorption of Impact and Shear Energy by Crystal Lattices of Mechanically Activated Inorganic Substances: A Review Multiscale Modeling and Computer-Aided Design of Advanced Materials with Hierarchical Structure Microstructural Deformation and Fracture of Reduced Activation Ferritic-Martensitic Steel EK-181 under Different Heat Treatment Conditions Synthesis of Porous Composites Based on Electroexplosive Ti/Al Nanopowder for Bone Implants
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1