{"title":"加工对 2507 双相不锈钢铸件微观结构、机械性能和断裂行为的影响","authors":"S. K. Ghosh, Muralidhar Yadav","doi":"10.1007/s11041-024-01042-0","DOIUrl":null,"url":null,"abstract":"<p>The effect of processing on the microstructure and mechanical properties of cast duplex stainless steel 2507 is studied. It is established that the structure of hot-rolled steel contains δ-ferrite and austenite (γ) bands that change due to 50% cold rolling to form microstructural constituents of a more refined and fragmented nature of a duplex (γ +δ) phase. Austenite grains are most effectively refined (up to 5 μm) because of the recrystallization occurring during aging treatment. The cold-rolled steel has maximum strength and minimum elongation. The best combination of strength and ductility is achieved after hot deformation + solution treatment at 1040°C with water cooling and after hot deformation + solution treatment at 1300°C with water cooling followed by isothermal aging at 1000°C. Such processing ensures a good formability of the steel.</p>","PeriodicalId":701,"journal":{"name":"Metal Science and Heat Treatment","volume":"66 3-4","pages":"237 - 242"},"PeriodicalIF":0.6000,"publicationDate":"2024-09-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Influence of Processing on Microstructure, Mechanical Properties, and Fracture Behavior of a Cast 2507 Duplex Stainless Steel\",\"authors\":\"S. K. Ghosh, Muralidhar Yadav\",\"doi\":\"10.1007/s11041-024-01042-0\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The effect of processing on the microstructure and mechanical properties of cast duplex stainless steel 2507 is studied. It is established that the structure of hot-rolled steel contains δ-ferrite and austenite (γ) bands that change due to 50% cold rolling to form microstructural constituents of a more refined and fragmented nature of a duplex (γ +δ) phase. Austenite grains are most effectively refined (up to 5 μm) because of the recrystallization occurring during aging treatment. The cold-rolled steel has maximum strength and minimum elongation. The best combination of strength and ductility is achieved after hot deformation + solution treatment at 1040°C with water cooling and after hot deformation + solution treatment at 1300°C with water cooling followed by isothermal aging at 1000°C. Such processing ensures a good formability of the steel.</p>\",\"PeriodicalId\":701,\"journal\":{\"name\":\"Metal Science and Heat Treatment\",\"volume\":\"66 3-4\",\"pages\":\"237 - 242\"},\"PeriodicalIF\":0.6000,\"publicationDate\":\"2024-09-19\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Metal Science and Heat Treatment\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://link.springer.com/article/10.1007/s11041-024-01042-0\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metal Science and Heat Treatment","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s11041-024-01042-0","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
Influence of Processing on Microstructure, Mechanical Properties, and Fracture Behavior of a Cast 2507 Duplex Stainless Steel
The effect of processing on the microstructure and mechanical properties of cast duplex stainless steel 2507 is studied. It is established that the structure of hot-rolled steel contains δ-ferrite and austenite (γ) bands that change due to 50% cold rolling to form microstructural constituents of a more refined and fragmented nature of a duplex (γ +δ) phase. Austenite grains are most effectively refined (up to 5 μm) because of the recrystallization occurring during aging treatment. The cold-rolled steel has maximum strength and minimum elongation. The best combination of strength and ductility is achieved after hot deformation + solution treatment at 1040°C with water cooling and after hot deformation + solution treatment at 1300°C with water cooling followed by isothermal aging at 1000°C. Such processing ensures a good formability of the steel.
期刊介绍:
Metal Science and Heat Treatment presents new fundamental and practical research in physical metallurgy, heat treatment equipment, and surface engineering.
Topics covered include:
New structural, high temperature, tool and precision steels;
Cold-resistant, corrosion-resistant and radiation-resistant steels;
Steels with rapid decline of induced properties;
Alloys with shape memory effect;
Bulk-amorphyzable metal alloys;
Microcrystalline alloys;
Nano materials and foam materials for medical use.