Laura Lourenço Morel, Marcus Vinícius Rocha de Almeida, Karoline Moraes Dos Santos, Maryana Fernandes Praseres, Ana Luíza Gonçalves Girundi, Larissa Dolfini Alexandrino, Wander José da Silva
{"title":"通过添加芳纶纤维增强义齿基底的 3D 打印树脂:对机械、表面和光学特性的影响。","authors":"Laura Lourenço Morel, Marcus Vinícius Rocha de Almeida, Karoline Moraes Dos Santos, Maryana Fernandes Praseres, Ana Luíza Gonçalves Girundi, Larissa Dolfini Alexandrino, Wander José da Silva","doi":"10.1111/jopr.13957","DOIUrl":null,"url":null,"abstract":"<p><strong>Purpose: </strong>The present study evaluated the mechanical, surface, and optical properties of 3D-printed resins for removable prostheses reinforced by the addition of aramid fibers.</p><p><strong>Materials and methods: </strong>According to ISO 20795-1:2013 standards, specimens were printed using a digital light processing 3D printer and divided into two groups (n = 06/group): 3D-printed resin for denture base as the control group, and a group with the same 3D-printed resin in addition of 5% aramid fibers as the experimental group. Red aramid fibers were chosen for aesthetic characterization. The specimens were evaluated for their mechanical properties, such as elastic modulus (GPa), flexural strength (MPa), and superficial properties by their surface microhardness (KHN), surface roughness (μm), and surface free energy (mJ/m<sup>2</sup>). Optical properties were evaluated by the color difference (∆E00) between groups. The statistical test chosen after the exploratory analysis of the data was One-way ANOVA followed by Tukey's HSD (α = 0.05).</p><p><strong>Results: </strong>The results showed statistical differences in elastic modulus (p < 0.0001), flexural strength (p < 0.0001), surface free energy polar variable (p = 0.0322), total surface free energy (p = 0.0344), with higher values for the experimental. Surface hardness and surface roughness showed no statistical difference (p ≥ 0.05). The color difference (∆E00) obtained through the CIEDE2000 calculus was below the perceptibility threshold (≤1.1).</p><p><strong>Conclusion: </strong>Adding aramid fibers to 3D-printed resin for denture bases resulted in better mechanical properties, without major alterations in surface properties. In addition, it is an easy-to-apply choice for mechanical reinforcement and aesthetic characterization, with the expression of small blood vessels in the 3D-printed resin for removable denture bases.</p>","PeriodicalId":49152,"journal":{"name":"Journal of Prosthodontics-Implant Esthetic and Reconstructive Dentistry","volume":null,"pages":null},"PeriodicalIF":3.4000,"publicationDate":"2024-09-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Reinforcement of 3D-printed resins for denture base by adding aramid fibers: Effect on mechanical, surface, and optical properties.\",\"authors\":\"Laura Lourenço Morel, Marcus Vinícius Rocha de Almeida, Karoline Moraes Dos Santos, Maryana Fernandes Praseres, Ana Luíza Gonçalves Girundi, Larissa Dolfini Alexandrino, Wander José da Silva\",\"doi\":\"10.1111/jopr.13957\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><strong>Purpose: </strong>The present study evaluated the mechanical, surface, and optical properties of 3D-printed resins for removable prostheses reinforced by the addition of aramid fibers.</p><p><strong>Materials and methods: </strong>According to ISO 20795-1:2013 standards, specimens were printed using a digital light processing 3D printer and divided into two groups (n = 06/group): 3D-printed resin for denture base as the control group, and a group with the same 3D-printed resin in addition of 5% aramid fibers as the experimental group. Red aramid fibers were chosen for aesthetic characterization. The specimens were evaluated for their mechanical properties, such as elastic modulus (GPa), flexural strength (MPa), and superficial properties by their surface microhardness (KHN), surface roughness (μm), and surface free energy (mJ/m<sup>2</sup>). Optical properties were evaluated by the color difference (∆E00) between groups. The statistical test chosen after the exploratory analysis of the data was One-way ANOVA followed by Tukey's HSD (α = 0.05).</p><p><strong>Results: </strong>The results showed statistical differences in elastic modulus (p < 0.0001), flexural strength (p < 0.0001), surface free energy polar variable (p = 0.0322), total surface free energy (p = 0.0344), with higher values for the experimental. Surface hardness and surface roughness showed no statistical difference (p ≥ 0.05). The color difference (∆E00) obtained through the CIEDE2000 calculus was below the perceptibility threshold (≤1.1).</p><p><strong>Conclusion: </strong>Adding aramid fibers to 3D-printed resin for denture bases resulted in better mechanical properties, without major alterations in surface properties. In addition, it is an easy-to-apply choice for mechanical reinforcement and aesthetic characterization, with the expression of small blood vessels in the 3D-printed resin for removable denture bases.</p>\",\"PeriodicalId\":49152,\"journal\":{\"name\":\"Journal of Prosthodontics-Implant Esthetic and Reconstructive Dentistry\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":3.4000,\"publicationDate\":\"2024-09-24\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Prosthodontics-Implant Esthetic and Reconstructive Dentistry\",\"FirstCategoryId\":\"3\",\"ListUrlMain\":\"https://doi.org/10.1111/jopr.13957\",\"RegionNum\":2,\"RegionCategory\":\"医学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"DENTISTRY, ORAL SURGERY & MEDICINE\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Prosthodontics-Implant Esthetic and Reconstructive Dentistry","FirstCategoryId":"3","ListUrlMain":"https://doi.org/10.1111/jopr.13957","RegionNum":2,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0
摘要
目的:本研究评估了通过添加芳纶纤维增强可摘义齿的三维打印树脂的机械、表面和光学特性:根据 ISO 20795-1:2013 标准,使用数字光处理 3D 打印机打印试样,并将试样分为两组(n = 06/组):对照组为义齿基托用三维打印树脂,实验组为添加 5%芳纶纤维的相同三维打印树脂。为美观起见,选择了红色芳纶纤维。对试样的机械性能(如弹性模量(GPa)、抗弯强度(MPa))和表面性能(如表面微硬度(KHN)、表面粗糙度(μm)和表面自由能(mJ/m2))进行了评估。光学特性通过组间色差(ΔE00)进行评估。数据探索性分析后选择的统计检验是单因素方差分析,然后是 Tukey's HSD(α = 0.05):结果表明,弹性模量存在统计学差异(p在用于义齿基托的三维打印树脂中添加芳纶纤维可获得更好的机械性能,而表面性能不会发生重大变化。此外,在可摘义齿基托的三维打印树脂中添加芳纶纤维还能表现出细小的血管,是一种易于应用的机械强化和美学特性选择。
Reinforcement of 3D-printed resins for denture base by adding aramid fibers: Effect on mechanical, surface, and optical properties.
Purpose: The present study evaluated the mechanical, surface, and optical properties of 3D-printed resins for removable prostheses reinforced by the addition of aramid fibers.
Materials and methods: According to ISO 20795-1:2013 standards, specimens were printed using a digital light processing 3D printer and divided into two groups (n = 06/group): 3D-printed resin for denture base as the control group, and a group with the same 3D-printed resin in addition of 5% aramid fibers as the experimental group. Red aramid fibers were chosen for aesthetic characterization. The specimens were evaluated for their mechanical properties, such as elastic modulus (GPa), flexural strength (MPa), and superficial properties by their surface microhardness (KHN), surface roughness (μm), and surface free energy (mJ/m2). Optical properties were evaluated by the color difference (∆E00) between groups. The statistical test chosen after the exploratory analysis of the data was One-way ANOVA followed by Tukey's HSD (α = 0.05).
Results: The results showed statistical differences in elastic modulus (p < 0.0001), flexural strength (p < 0.0001), surface free energy polar variable (p = 0.0322), total surface free energy (p = 0.0344), with higher values for the experimental. Surface hardness and surface roughness showed no statistical difference (p ≥ 0.05). The color difference (∆E00) obtained through the CIEDE2000 calculus was below the perceptibility threshold (≤1.1).
Conclusion: Adding aramid fibers to 3D-printed resin for denture bases resulted in better mechanical properties, without major alterations in surface properties. In addition, it is an easy-to-apply choice for mechanical reinforcement and aesthetic characterization, with the expression of small blood vessels in the 3D-printed resin for removable denture bases.
期刊介绍:
The Journal of Prosthodontics promotes the advanced study and practice of prosthodontics, implant, esthetic, and reconstructive dentistry. It is the official journal of the American College of Prosthodontists, the American Dental Association-recognized voice of the Specialty of Prosthodontics. The journal publishes evidence-based original scientific articles presenting information that is relevant and useful to prosthodontists. Additionally, it publishes reports of innovative techniques, new instructional methodologies, and instructive clinical reports with an interdisciplinary flair. The journal is particularly focused on promoting the study and use of cutting-edge technology and positioning prosthodontists as the early-adopters of new technology in the dental community.